1-20 of 270 Search Results for

chemical plant equipment

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1984) 33 (8): SS-450.
Published: 01 August 1984
... 310S, a few typical uses include annealing boxes, chemical plant equipment, fire box sheets, furnace linings, heat exchangers, oil-refining equipment, kiln linings and tube hangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1986) 35 (2): Al-265.
Published: 01 February 1986
... ALUMINUM 513.0 is an aluminum-magnesium-zinc permanent-mold casting alloy. It cannot be hardened nor strengthened by any thermal treatment and is characterized by moderate strength and ductility. It is recommended for such applications as chemical-plant equipment, food handling and marine hardware...
Journal Articles
Alloy Digest (1969) 18 (12): Al-193.
Published: 01 December 1969
... ALLCAST P400 is an aluminum-magnesium-zinc permanent mold casting alloy. It is recommended for food handling and chemical plant equipment and where good resistance to corrosion and tarnishing are required. It does not respond to an age-hardening heat treatment. This datasheet provides information...
Journal Articles
Alloy Digest (1970) 19 (4): SS-236.
Published: 01 April 1970
... FIRTH VICKERS FI (A1) is a chromium type heat and corrosion resistant alloy steel recommended for oil refining and chemical plant equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1967) 16 (2): SS-191.
Published: 01 February 1967
... Type CK-20 is the 25-20 type corrosion resisting casting alloy. It has high degree of stability against intergranular corrosion. It is recommended for chemical plant equipment, oil refinery components and paper and pulp industry parts. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1968) 17 (1): Al-171.
Published: 01 January 1968
... ALUMINUM A-214 is an aluminum-magnesium-zinc permanent mold and die casting alloy. It is recommended for food handling and chemical plant equipment. It does not respond to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1968) 17 (7): SS-211.
Published: 01 July 1968
... AISI Type 502 is a corrosion and heat resisting 5% chromium alloy steel. It is generally used in the annealed condition only. It is recommended for oil refinery and chemical plant equipment, oil pump impellers, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1987) 36 (8): SS-488.
Published: 01 August 1987
... at elevated temperatures. Type 316 is suitable for a wide range of applications in chemical and petroleum processing, power plants, pollution-control equipment, pulp and paper plants and food and pharmaceutical processing. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1985) 34 (5): Ni-314.
Published: 01 May 1985
... at room and elevated temperatures. Its applications include heat treating furnace equipment, chemical equipment in various industries, and power plant equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1997) 46 (2): Ni-521.
Published: 01 February 1997
... at room temperatures. Its application includes heat-treating furnace equipment, chemical equipment in various industries, and power plant equipment. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (1969) 18 (7): SS-227.
Published: 01 July 1969
... AISI Type 430 is a ductile, non-hardenable type of stainless steel recommended for parts requiring a combination of good formability, weldability and corrosion resistance. It is used for architectural trim, food and dairy handling equipment, chemical and oil refinery plant equipment...
Journal Articles
Alloy Digest (2002) 51 (3): SS-846.
Published: 01 March 2002
... in air-pollution control systems, pulp and paper plants, and chemical and petrochemical processing equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1970) 19 (5): SS-239.
Published: 01 May 1970
... Type CH-20 is a 25-12 type of heat and corrosion resisting cast alloy steel. It is recommended for equipment in the chemical, processing, power plant and paper and pulp industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1960) 9 (11): Al-97.
Published: 01 November 1960
... for marine applications. It is a non-heat treatable alloy and has a high order of resistance to corrosion. Forms Available: Ingots and sand castings. Applications: Architectural work and food handling equip- ment, chemical plant equipment, cooking utensils, fittings, marine hardware. Manufacturer: Bohn...
Journal Articles
Alloy Digest (2000) 49 (10): SS-805.
Published: 01 October 2000
... capability on a polished surface, particularly following deep machining. Product Forms Available: Plate and bars Applications: Applications include chemical plant equipment such as heat ex- changers, agitators, kettles, evaporators, tanks, digesters, valve trim, and special equipment. Producer: Allegheny...
Journal Articles
Alloy Digest (1955) 4 (10): SS-35.
Published: 01 October 1955
... will be greatly reduced. Forms Available: Bars, rods and forgiogs. Applications: Chemical plant equipment, ice making machinery, nitric acid plant equipment, nitrogen fixation apparatus, oil burner parts and heaters, oil refinery equipment, rubber plant machinery, soot blowers, tanks, bolts, low temperature...
Journal Articles
Alloy Digest (1961) 10 (1): Cu-96.
Published: 01 January 1961
... with its good resistance to corrosion and oxidation, this alloy becomes suitable for service in steam plants, internal combustion engines, petroleum refinery and chemical plant equipments. Its high cortosioa-fatigue limit in salt water per- mits higher working stresses, and results in thinner and more...
Journal Articles
Alloy Digest (2010) 59 (5): Ta-13.
Published: 01 May 2010
... level then pure tantalum and better corrosion resistance in HCI and H 2 SO 4 acids. Paddle stirrers and agitators, solid or covered (loose-lined) Distillation columns, boilers and condensers Tantalum clad dip pipes, heaters and chemical plant equipment Repair kits, for tanks, vats and other...
Journal Articles
Alloy Digest (1964) 13 (11): Al-141.
Published: 01 November 1964
.... Forms Available: Ingots and sand castings. Applications: Architectural work, food handling equipment, chemical plant equipment, cooking utensils, fittings, marine hardware. Manufacturer: Aluminum Co. of America, Pittsburgh, Pennsylvania Olin Mathieson, Metals Division, New York, New York Reynolds Metals...
Journal Articles
Alloy Digest (1961) 10 (9): Al-107.
Published: 01 September 1961
... service up to 300OF. It is a non-heat treatable alloy. Forms Available: Ingots Applications: Cooking utensils, marine parts, food handling equipment, chemical plant equipment, fittings and hardware. Manfacturer: Apex Smelting Company Cleveland, Ohio Chicago, Illinois Long Beach, California ...