Skip Nav Destination
Close Modal
Search Results for
chemical industries
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 2051
Search Results for chemical industries
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
REMANIT 4462: Ferritic Austenitic Duplex Stainless Steel
Available to Purchase
Alloy Digest (1993) 42 (12): SS-558.
Published: 01 December 1993
... REMANIT 4462 is a ferritic/austenitic duplex stainless steel with a low carbon content, an addition of nitrogen and a balanced ratio of the alloying elements. This offers a stable structure with good weldability. REMANIT 4462 is well suited for many applications in the chemical industry, in off...
Abstract
View articletitled, REMANIT 4462: Ferritic Austenitic Duplex Stainless Steel
View
PDF
for article titled, REMANIT 4462: Ferritic Austenitic Duplex Stainless Steel
REMANIT 4462 is a ferritic/austenitic duplex stainless steel with a low carbon content, an addition of nitrogen and a balanced ratio of the alloying elements. This offers a stable structure with good weldability. REMANIT 4462 is well suited for many applications in the chemical industry, in off-shore technology and in the gas and oil industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-558. Producer or source: Thyssen Stahl AG.
Journal Articles
UHB STAINLESS 904L: Austenitic Stainless Steel
Available to Purchase
Alloy Digest (1973) 22 (7): SS-287.
Published: 01 July 1973
... UHB Stainless 904L is an extra-low-carbon, non-stabilized austenitic stainless steel with excellent corrosion resistance in severe acids and acidic solutions. It is particularly suitable for structural applications in the chemical industry and other process industries. This datasheet provides...
Abstract
View articletitled, UHB STAINLESS 904L: Austenitic Stainless Steel
View
PDF
for article titled, UHB STAINLESS 904L: Austenitic Stainless Steel
UHB Stainless 904L is an extra-low-carbon, non-stabilized austenitic stainless steel with excellent corrosion resistance in severe acids and acidic solutions. It is particularly suitable for structural applications in the chemical industry and other process industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-287. Producer or source: Uddeholm Aktiebolag.
Journal Articles
ANACONDA ALLOY (A) 5090: Standard and Superfine Grain Duraflex Phosphor Bronze
Available to Purchase
Alloy Digest (1979) 28 (5): Cu-372.
Published: 01 May 1979
... ANACONDA (A) 5090, long a specialty item in the industry, is a wrought intermediate phospor bronze developed to fulfill a need for special end-products such as kettles and other containers. It has found broad applications in the chemical industry. It offers a good combination of strength...
Abstract
View articletitled, ANACONDA ALLOY (A) 5090: Standard and Superfine Grain Duraflex Phosphor Bronze
View
PDF
for article titled, ANACONDA ALLOY (A) 5090: Standard and Superfine Grain Duraflex Phosphor Bronze
ANACONDA (A) 5090, long a specialty item in the industry, is a wrought intermediate phospor bronze developed to fulfill a need for special end-products such as kettles and other containers. It has found broad applications in the chemical industry. It offers a good combination of strength, ductility, resilience, fatigue properties and resistance to both corrosion and erosion. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-372. Producer or source: Anaconda American Brass Company.
Journal Articles
CARLSON C20 PLUS: Acid Resistant Austenitic Stainless
Available to Purchase
Alloy Digest (1992) 41 (10): SS-535.
Published: 01 October 1992
... CARLSON C20 PLUS alloy is an austenitic stainless steel designed for improved resistance to reducing acids, particularly sulfuric acid. It finds wide use in all phases of the chemical industry and has good strength and fabricability for case in making process equipment and piping. This datasheet...
Abstract
View articletitled, CARLSON C20 PLUS: Acid Resistant Austenitic Stainless
View
PDF
for article titled, CARLSON C20 PLUS: Acid Resistant Austenitic Stainless
CARLSON C20 PLUS alloy is an austenitic stainless steel designed for improved resistance to reducing acids, particularly sulfuric acid. It finds wide use in all phases of the chemical industry and has good strength and fabricability for case in making process equipment and piping. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-535. Producer or source: G.O. Carlson Inc..
Journal Articles
MAERKER G-4848: Heat Resistant Alloy
Available to Purchase
Alloy Digest (1995) 44 (10): SS-617.
Published: 01 October 1995
... MAERKER G-4848 is a heat resistant alloy for the petro chemical industry. The alloy has very good creep-rupture strength with low embrittlement. Similar to HK Mod. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes...
Abstract
View articletitled, MAERKER G-4848: Heat Resistant Alloy
View
PDF
for article titled, MAERKER G-4848: Heat Resistant Alloy
MAERKER G-4848 is a heat resistant alloy for the petro chemical industry. The alloy has very good creep-rupture strength with low embrittlement. Similar to HK Mod. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting and joining. Filing Code: SS-617. Producer or source: Schmidt & Clemens Inc.
Journal Articles
CIRCLE L 21: Corrosion Resistant Casting Alloy
Available to Purchase
Alloy Digest (1964) 13 (9): SS-160.
Published: 01 September 1964
... CIRCLE L 21 is a columbium type 18-8 stainless steel casting alloy recommended for welded structures and equipment in the chemical industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Abstract
View articletitled, CIRCLE L 21: Corrosion Resistant Casting Alloy
View
PDF
for article titled, CIRCLE L 21: Corrosion Resistant Casting Alloy
CIRCLE L 21 is a columbium type 18-8 stainless steel casting alloy recommended for welded structures and equipment in the chemical industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-160. Producer or source: Lebanon Steel Foundry.
Journal Articles
Ti-0.15 Pd: High Temperature Titanium Alloy
Available to Purchase
Alloy Digest (1965) 14 (10): Ti-45.
Published: 01 October 1965
... Ti-0.15Pd is an alpha-type titanium alloy recommended for the chemical industry applications where environments are moderately reducing, or fluctuate between oxidizing and reducing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View articletitled, Ti-0.15 Pd: High Temperature Titanium Alloy
View
PDF
for article titled, Ti-0.15 Pd: High Temperature Titanium Alloy
Ti-0.15Pd is an alpha-type titanium alloy recommended for the chemical industry applications where environments are moderately reducing, or fluctuate between oxidizing and reducing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-45. Producer or source: Reactive Metals Corporation.
Journal Articles
SANICRO 71: Heat and Corrosion Resisting Alloy
Available to Purchase
Alloy Digest (1965) 14 (12): Ni-108.
Published: 01 December 1965
... Sanicro 71 is a nickel-base alloy having good resistance to stress-corrosion, oxidation and creep at elevated temperatures. It is recommended for nuclear power reactor heat exchanger tubes, aircraft turbojet engines and for equipment in the textile, plastic, and chemical industries. This datasheet...
Abstract
View articletitled, SANICRO 71: Heat and Corrosion Resisting Alloy
View
PDF
for article titled, SANICRO 71: Heat and Corrosion Resisting Alloy
Sanicro 71 is a nickel-base alloy having good resistance to stress-corrosion, oxidation and creep at elevated temperatures. It is recommended for nuclear power reactor heat exchanger tubes, aircraft turbojet engines and for equipment in the textile, plastic, and chemical industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-108. Producer or source: Sandvik.
Journal Articles
CARPENTER STAINLESS 20Cb-3: Acid Resistant Steel
Available to Purchase
Alloy Digest (1966) 15 (6): SS-182.
Published: 01 June 1966
... Carpenter Stainless 20Cb-3 is an austenitic stainless steel designed for improved resistance to sulfuric acid. It finds wide use in all phases of the chemical industry. It has good mechanical properties and comparative ease of fabrication. Columbium stabilizes the alloy to minimize carbide...
Abstract
View articletitled, CARPENTER STAINLESS 20Cb-3: Acid Resistant Steel
View
PDF
for article titled, CARPENTER STAINLESS 20Cb-3: Acid Resistant Steel
Carpenter Stainless 20Cb-3 is an austenitic stainless steel designed for improved resistance to sulfuric acid. It finds wide use in all phases of the chemical industry. It has good mechanical properties and comparative ease of fabrication. Columbium stabilizes the alloy to minimize carbide precipitation during welding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-182. Producer or source: Carpenter.
Journal Articles
ULBRICH TITANIUM GRADE 1 (UNS R50250): Unalloyed Commercially Pure Titanium
Available to Purchase
Alloy Digest (2020) 69 (4): Ti-165.
Published: 01 April 2020
... Ulbrich Titanium Grade 1 (UNS R50250) is an unalloyed commercially pure titanium. It is one of the softest and the most ductile of the commercially pure grades, and exhibits excellent formability. It has excellent corrosion resistance and is mainly used in marine and chemical industries where...
Abstract
View articletitled, ULBRICH TITANIUM GRADE 1 (UNS R50250): Unalloyed Commercially Pure Titanium
View
PDF
for article titled, ULBRICH TITANIUM GRADE 1 (UNS R50250): Unalloyed Commercially Pure Titanium
Ulbrich Titanium Grade 1 (UNS R50250) is an unalloyed commercially pure titanium. It is one of the softest and the most ductile of the commercially pure grades, and exhibits excellent formability. It has excellent corrosion resistance and is mainly used in marine and chemical industries where the parts are exposed to very harsh environments. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming. Filing Code: Ti-165. Producer or source: Ulbrich Stainless Steels & Special Metals, Inc.
Journal Articles
J&L TYPE 2205: Duplex Stainless Steel
Available to Purchase
Alloy Digest (2000) 49 (1): SS-773.
Published: 01 January 2000
..., tubing, tanks, and heat exchangers for the chemical industries. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-773. Producer or source...
Abstract
View articletitled, J&L TYPE 2205: Duplex Stainless Steel
View
PDF
for article titled, J&L TYPE 2205: Duplex Stainless Steel
J and L 2205 is a ferritic-austenitic duplex stainless steel. It resists stress-corrosion cracking very well and has good pitting and general corrosion resistance. Its high strength and stress-corrosion resisting characteristics are a reflection of its duplex microstructure. Its uses include pipe, tubing, tanks, and heat exchangers for the chemical industries. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-773. Producer or source: J & L Specialty Steel Inc.
Journal Articles
COMMERCIALLY PURE TITANIUM GRADE 12: Commercially Pure Wrought Titanium Modified with Nickel and Molybdenum
Available to Purchase
Alloy Digest (1989) 38 (9): Ti-93.
Published: 01 September 1989
... Commercially pure wrought titanium, Grade 12 is used in the chemical industry where conditions are mildly reducing or varying between oxidizing and reducing. It is immune to formic acid, aerated or non-aerated. This datasheet provides information on composition, physical properties, elasticity...
Abstract
View articletitled, COMMERCIALLY PURE TITANIUM GRADE 12: Commercially Pure Wrought Titanium Modified with Nickel and Molybdenum
View
PDF
for article titled, COMMERCIALLY PURE TITANIUM GRADE 12: Commercially Pure Wrought Titanium Modified with Nickel and Molybdenum
Commercially pure wrought titanium, Grade 12 is used in the chemical industry where conditions are mildly reducing or varying between oxidizing and reducing. It is immune to formic acid, aerated or non-aerated. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-93. Producer or source: Titanium alloy mills. Originally published August 1989, revised September 1989.
Journal Articles
ACI TYPE CF-20: Corrosion Resistant Cast Stainless Steel
Available to Purchase
Alloy Digest (1976) 25 (1): SS-323.
Published: 01 January 1976
... ironchromium AC1 Type CB-30. Its many uses include the architectural, food and chemical industries. *Additional information is available from the source of the material herein: Alloy Casting Institute Division, Steel Founders Society of America, Rocky River, Ohio 44116. Composition: Physical Constants: Carbon...
Abstract
View articletitled, ACI TYPE CF-20: Corrosion Resistant Cast Stainless Steel
View
PDF
for article titled, ACI TYPE CF-20: Corrosion Resistant Cast Stainless Steel
Type CF-20 is an austenitic iron-chromium-nickel alloy that serves satisfactorily in many types of oxidizing corrosion service where its superior ductility and toughness make it more useful that the ferritic iron-chromium ACI Type CB-30. Its many uses include the architectural, food and chemical industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-323. Producer or source: Stainless steel foundries.
Journal Articles
KYNAL P10: Wrought Aluminum
Available to Purchase
Alloy Digest (1957) 6 (10): Al-57.
Published: 01 October 1957
... on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-57. Producer or source: Imperial Chemical Industries Inc.. Producer or Source: Imperial Chemical Industries Inc. Copyright © ASM International® 1996 1996 ASM...
Abstract
View articletitled, KYNAL P10: Wrought Aluminum
View
PDF
for article titled, KYNAL P10: Wrought Aluminum
KYNAL P10 is a grade of commercially pure aluminum having high corrosion resistance and fabricating qualities. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-57. Producer or source: Imperial Chemical Industries Inc..
Journal Articles
KUMANIC: Heat Treatable Copper Alloy
Available to Purchase
Alloy Digest (1959) 8 (8): Cu-79.
Published: 01 August 1959
.... It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-79. Producer or source: Imperial Chemical Industries Ltd. Producer or Source: Imperial Chemical Industries Ltd Copyright © ASM International® 1996 1996 ASM International chemical composition...
Abstract
View articletitled, KUMANIC: Heat Treatable Copper Alloy
View
PDF
for article titled, KUMANIC: Heat Treatable Copper Alloy
KUMANIC is a copper-manganese-nickel alloy that responds to hardening by heat treatment. It has high tensile and fatigue strength along with excellent resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-79. Producer or source: Imperial Chemical Industries Ltd.
Journal Articles
KYNAL C69: Heat Treatable Aluminum Alloy
Available to Purchase
Alloy Digest (1959) 8 (12): Al-87.
Published: 01 December 1959
... treating, and joining. Filing Code: Al-87. Producer or source: Imperial Chemical Industries Inc.. Producer or Source: Imperial Chemical Industries Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity fatigue resistance...
Abstract
View articletitled, KYNAL C69: Heat Treatable Aluminum Alloy
View
PDF
for article titled, KYNAL C69: Heat Treatable Aluminum Alloy
KYNAI C69 is an age-hardenable aluminum alloy recommended for medium and high strength appIications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Al-87. Producer or source: Imperial Chemical Industries Inc..
Journal Articles
FERRALIUM 255-SD50: Ferritic/Austenitic Duplex Stainless Steel
Available to Purchase
Alloy Digest (2013) 62 (1): SS-1133.
Published: 01 January 2013
... impurities giving improved corrosion resistance, and it is used extensively in the offshore and chemical industries. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming and machining...
Abstract
View articletitled, FERRALIUM 255-SD50: Ferritic/Austenitic Duplex Stainless Steel
View
PDF
for article titled, FERRALIUM 255-SD50: Ferritic/Austenitic Duplex Stainless Steel
Ferralium 255-SD50 has much higher strength than other commercially available superduplex alloys. Ferralium 255 is the original superduplex stainless steel, noted for its unique combination of mechanical properties and resistance to corrosion, erosion, and cavitation. It has especially low impurities giving improved corrosion resistance, and it is used extensively in the offshore and chemical industries. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming and machining. Filing Code: SS-1133. Producer or source: Langley Alloys.
Journal Articles
Ti-0.20Pd: High Temperature Titanium Alloy
Available to Purchase
Alloy Digest (1968) 17 (3): Ti-56.
Published: 01 March 1968
... Ti-0.20Pd is an alpha-type titanium alloy recommended for the chemical industry applications where environments are moderately reducing, or fluctuate between oxidizing and reducing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View articletitled, Ti-0.20Pd: High Temperature Titanium Alloy
View
PDF
for article titled, Ti-0.20Pd: High Temperature Titanium Alloy
Ti-0.20Pd is an alpha-type titanium alloy recommended for the chemical industry applications where environments are moderately reducing, or fluctuate between oxidizing and reducing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-56. Producer or source: Reactive Metals Corporation.
Journal Articles
DELORO ALLOY C: Corrosion Resistant Alloy
Available to Purchase
Alloy Digest (1969) 18 (5): Ni-145.
Published: 01 May 1969
... Deloro alloy C is a nickel base alloy designed primarily for high corrosion resistance for the chemical industry. It is used for pumps, valves, and hard facing electrodes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Abstract
View articletitled, DELORO ALLOY C: Corrosion Resistant Alloy
View
PDF
for article titled, DELORO ALLOY C: Corrosion Resistant Alloy
Deloro alloy C is a nickel base alloy designed primarily for high corrosion resistance for the chemical industry. It is used for pumps, valves, and hard facing electrodes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-145. Producer or source: Deloro Stellite Ltd.
Journal Articles
UDDEHOLM STAINLESS 24 and 24L: Austenitic Stainless Steels, Types 316 and 316L
Available to Purchase
Alloy Digest (1978) 27 (5): SS-350.
Published: 01 May 1978
... includes process vessels and containers in the chemical industry, steam superheaters and pickling vats. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low...
Abstract
View articletitled, UDDEHOLM STAINLESS 24 and 24L: Austenitic Stainless Steels, Types 316 and 316L
View
PDF
for article titled, UDDEHOLM STAINLESS 24 and 24L: Austenitic Stainless Steels, Types 316 and 316L
UDDEHOLM Stainless 24 and 24L are essentially similar except for the extra-low carbon content of 24L for use where forming and welding result in relatively long heating within the range 930-1650 F (500-900 C). They are acid-resistant, non-hardenable and nonmagnetic steels. Their wide usage includes process vessels and containers in the chemical industry, steam superheaters and pickling vats. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-350. Producer or source: Uddeholm Aktiebolag.