Alloy Digest (1957) 6 (5): Cu-50.
Published: 01 May 1957
... CHAMET BRONZE is a copper-zinc alloy containing 0.75% of tin, having high strength, toughness and resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on...