Journal Articles
Alloy Digest (1997) 46 (9): SS-696.
Published: 01 September 1997
... UCI-270 is a cast, cobalt and tungsten stabilized, nickel-chromium-iron alloy having unequaled performance in high-temperature applications to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace tubes, and refining furnace tubes...
Journal Articles
Alloy Digest (1977) 26 (11): SS-228.
Published: 01 November 1977
... SUPERTHERM is a cast nickel-chromium-iron alloy stabilized with cobalt and tungsten. It is used worldwide in extremely high-temperature applications and has unexcelled performance to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace...
Journal Articles
Alloy Digest (2018) 67 (6): Ni-744.
Published: 01 June 2018
... design. Applications Applications include highly stressed furnace parts, sintering and calcining muffles, cement kiln components resistant to hot abrasion, radiant tubes, and pyrolysis coils. Table 1 At high temperatures short time tests Temperature, °C (°F) Yield strength, MPa (ksi) Ultimate tensile...
Journal Articles
Alloy Digest (2018) 67 (7): Ni-745.
Published: 01 July 2018
... stressed furnace parts, sintering and calcining muffles, cement kiln components resistant to hot abrasion, radiant tubes, and pyrolysis coils. Table 1 Chart of stress-rupture properties Temperature, °C (°F) Avg initial stress for 100,000 h creep rupture, MPa (ksi) Avg stress for a creep rate of 0.0001 %/h...
Journal Articles
Alloy Digest (2012) 61 (2): SS-1115.
Published: 01 February 2012
... to greater ease of fabrication. Product Forms Available: Horizontal and vertical centrifugal castings; static castings Applications: Cement kiln chain, shackles and hangers; furnace rails, hearth plates, conveyor belts, furnace rolls, and tube sheets Producer: Kubota Metal Corporation, Fahramet Division...
Journal Articles
Alloy Digest (1978) 27 (6): SS-352.
Published: 01 June 1978
.... Applications: Reformer tubes, steel-mill parts, cement-kiln parts, heat-treating furnace parts, parts for petrochemical furnaces and components for smelting and refining furnaces. Manufacturer: Abex Corporation Engineered Products Division Elyria, Ohio 44035. ...
Journal Articles
Alloy Digest (1997) 46 (5): SS-682.
Published: 01 May 1997
... is observed for this grade. Silicon is heIpfu1 in confer- ring resistance in the aIIoy to carburization, but is normaBy held to 2.00% maximum because higher amounts promote Q forma- tion. Forms Available: Castings. Applications: This ahoy is used for billet skids. brazing fixtures. calcining Cubes. cement...
Journal Articles
Alloy Digest (2006) 55 (11): SS-980.
Published: 01 November 2006
... centrifugal castings, and static castings. Applications: Rabble arms and blades, grate bars, cement kiln cooling chain and shackles, tuyeres, furnace burner nozzles, radiant heater tubes and fittings, tube supports and hangers, tube sheets, heat treatment furnace hardware and furnace retorts and muffles...
Journal Articles
Alloy Digest (1963) 12 (9): Ni-86.
Published: 01 September 1963
... from atmosphetes (oxidizing and reducing) high in sulphut. Forms Available: Sheer, place, Abe. Applications: Nitric acid equipment, glass and brick industries components, cement kilns, tadianr tubes, pyrometer sheaths, f?uidized beds, salt baths, gas woks. Manufacturer: Hemy Wiggin % Co., Ltd...
Journal Articles
Alloy Digest (1974) 23 (12): SS-303.
Published: 01 December 1974
... is helpful in conferring resistance of the alloy to carburization. but is normally held to 2.00 per cent maximum since higher amounts promote sigma formation. Forms Available: Castings. Applications: This alloy is used for biller skids. brazing fixtures. calcining tubes, cement kiln nose segments, conveyor...
Journal Articles
Alloy Digest (2017) 66 (12): SS-1272.
Published: 01 December 2017
... Furnace and boiler construction: grates and grate segments, fittings, conveyor components, supporting and walking beams, rams, rails, rollers, doors, gates and traps, housings, recuperators, fans, superheater suspensions, tube clamps, soot blower pipes Glass, porcelain, enamel, cement, and ceramic...
Journal Articles
Alloy Digest (2017) 66 (10): SS-1270.
Published: 01 October 2017
... suspensions, tube clamps, soot blower pipes Glass, porcelain, enamel, cement, and ceramic industries: burner tips, rings, segments, and components for rotary and lepol kilns Mechanical engineering:. grid bars, valves and spindles, stirrer arms and teeth, sheath tubes for thermocouples, fittings, drums...
Journal Articles
Alloy Digest (2017) 66 (11): SS-1271.
Published: 01 November 2017
..., enamel, cement, and ceramic industries: burner tips, rings, segments, and components for rotary and lepol kilns Mechanical engineering: grid bars, valves and spindles, stirrer arms and teeth, sheath tubes for thermocouples, fittings, drums, bolts, nuts, rivets Petroleum industry: tubes and tubular...
Journal Articles
Alloy Digest (2004) 53 (10): SS-910.
Published: 01 October 2004
... and preheaters for ladles in continuous casting plants; flue gas ducts, burners, electrical resistance components for furnace, and rollers in rolling mills; working beams, doors, burners, and heat recuperators in heat treatment furnaces; feeding and discharging systems, rotary kilns, refractory anchors, burners...
Journal Articles
Alloy Digest (2005) 54 (9): SS-941.
Published: 01 September 2005
... is designed for high-temperature applications up to 1000 °C (1832 °F) in sulfur-containing atmospheres. Higher sulfur con- tent in gases will result in lower maximum temperatures of uses. The alloy can be also used in slightly oxidizing atmospheres, nitriding, and cementing conditions as well as with thermal...
Journal Articles
Alloy Digest (2005) 54 (10): SS-945.
Published: 01 October 2005
... applications up to 1100 °C (2012 °F) in oxidizing atmospheres. The alloy can be also used in slightly oxidizing atmospheres, nitriding, cementing, and sulfur- izing conditions as well as with thermal cyclings, but the maxi- mum temperature of use will be reduced. When heated between 650 and 950 °C (1202...