Alloy Digest (1966) 15 (3): TS-176.
Published: 01 March 1966
... VANADIUM Type H is a high carbon, chromium-vanadium alloy steel of the water-hardening or oil-hardening type having high wear resistance combined with toughness. It has good depth hardenability when water hardened. It is recommended for punches, dies, cutters, burnishing tools, caulking tools...
Journal Articles
Alloy Digest (1988) 37 (12): TS-494.
Published: 01 December 1988
..., vanstoning dies, concrete breakers, caulking tools, rivetbusters,beadingtools,trackchisels,pipecutterwheels, screw drivers and rivet sets. Manufacturer: Carpenter Technology Corporation Carpenter Steel Division Box 14662 Reading, Pennsylvania 19612 ...
Journal Articles
Alloy Digest (1974) 23 (10): SA-310.
Published: 01 October 1974
... shafts, pneumatic tools, shear blades, springs, punches, caulking tools, shanks for carbide tools, gears, pinions, bolts, housings, casings, wrenches, studs, tool forgings, and machinery parts subject to shock loading. Manufacturers: Practically all alloy steel mills. ...
Journal Articles
Alloy Digest (1972) 21 (9): TS-246.
Published: 01 September 1972
..., rods and forgings. Applications: Beading and caulking tools, boilermaker s tools, cold-battering hand and pneumatic tools, studs for service at elevated temper atures, shear blades, punches, forming dies, extrusion tools. rivet busters, concrete drills and breakers, hot-swaging dies, hubbing dies...
Journal Articles
Alloy Digest (1960) 9 (3): TS-91.
Published: 01 March 1960
..., billets, forgings. Applications: Shear blades, hot heading and forming dies, forging inserts, chisels, pneumatic tools, rivet busters, studs and bolts for ele- vated temperature, pavement breakers, caulking tools. After pack hardending, use for swage rollers, punches, scale cutters, broaches, blanking...
Journal Articles
Alloy Digest (1968) 17 (3): SA-223.
Published: 01 March 1968
... subject ro severe service, heavy duty punches, shanks for carbide tools, machine parts subject to shock, chisels, caulking tools and all types of severe or unusual service involving drastic or repeated impact at atmospheric temperatures. Manufacturer: Practically all alloy steel mills. ...
Journal Articles
Alloy Digest (1975) 24 (11): SA-320.
Published: 01 November 1975
... to that of carbon steel. Welding is possible with extensive precautions. The effect of boron, however, may be absent or greatly decreased in the weld metal and adjacent regions. Forms Available: Billets, bars, rods and forgings. Applications: Springs, axle. shafts, shear blades, punches, pneumatic tools, caulking...
Journal Articles
Alloy Digest (1987) 36 (4): SA-424.
Published: 01 April 1987
.... forgings, bars and rods. Applications: Typical uses for SAE 8655 alloy steel comprise axle shafts, pneumatic tools. shear blades, springs, punches, caulking tools, shanks for carbide tools, gears, pinions, bolts, housings. casings, wrenches, studs, tool forgings, and machinery parts subject to shock...
Journal Articles
Alloy Digest (1982) 31 (3): TS-396.
Published: 01 March 1982
... wear resistance, it is common practice to carburize the surface of tools, and still retain the shock resistance. Forms Available: Billets, bars and forgings. Applications: Beading and caulking tools, boilermaker s tools, cold- battering hand and pneumatic tools, shear blades, studs for service...
Journal Articles
Alloy Digest (1964) 13 (9): SA-167.
Published: 01 September 1964
..., rods, forgings. Applications: Heavy duty springs, shear blades, pneumatic tool, punches, shanks for carbide tools, machine parts subject to shock, chisels, caulking tools and all types of severe or unusual service involving drastic or repeated impact at armosphetic cempet- atutes. Manufacturer...
Journal Articles
Alloy Digest (1982) 31 (12): TS-408.
Published: 01 December 1982
... dies, crimping dies, swaging dies, wrenches, jaws, finders, shear blades, heavy- duty forming tools, heavy-duty coining dies, special knurls and stamps. Type S2 also is used for the fol- lowing battering tools : pneumatic chisels, van- stoning dies, concrete breakers, caulking tools, rivet busters...
Journal Articles
Alloy Digest (1983) 32 (7): TS-416.
Published: 01 July 1983
..., clock springs, hand stamps, stencil cutters, rock drills, stone-cutting tools, pipe dies, shear blades, caulking tools, punches, dies, files, broaches. cold-working tools, knurls, cutlery, reamers and drills. Manufacturers: Tool steel mills. ...
Journal Articles
Alloy Digest (1979) 28 (7): TS-352.
Published: 01 July 1979
... and forgings. Applications: Bolt header dies, chipping and caulking chisels, circular pipe cutters, concrete drills, expander rolls, forging dies, forming dies, grippers, mandrels, punches, pneumatic tools, rivet busters, scarfing tools, swaging dies, shear blades, track tools. Manufacturer: Universal Cyclops...
Journal Articles
Alloy Digest (1965) 14 (5): TS-164.
Published: 01 May 1965
... Jessop 259 is an extremely tough silico-manganese alloy tool steel with outstanding shock and abrasion resistance. It is recommended for shock resisting applications such as pneumatic tools, punches, concrete breakers, rivet busters, etc. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1977) 26 (1): TS-312.
Published: 01 January 1977
... coUets. In addition, it is suitable for pneumatic tools, chipping chisels, beading, caulking, flaring and starting tools, button sets, rivet sets, shear blades, clutch dogs, vise jaws, etc. It should be considered for use wherever extreme toughness is a requirement. Manufacturer: Carpenter Technology...
Journal Articles
Alloy Digest (1958) 7 (4): TS-69.
Published: 01 April 1958
.... Applications: Pneumatic tools, chipping chisels, backing-out punches; bead- ing, caulking, blaring and scarfing tools; button sets, concrete busters, rivet sets, shear blades, clutch dogs, vise jaws, spring collet~, sledges, mauls, heavy duty perforating punches, drift pins, knockout pins, track chisels...
Journal Articles
Alloy Digest (1965) 14 (6): SA-178.
Published: 01 June 1965
... for hardnesses under Rockwell C58. Forms Available: Billets, bars, rods, forgings. Applications: Springs, axle shafts, shear blades, pneumatic tools. punches, shanks for carbide cools, caulking cools, machinery parrs subject IO shock loading. Manufacturer: Practically all alloy steel mills. ...
Journal Articles
Alloy Digest (1956) 5 (5): TS-46.
Published: 01 May 1956
... punches, shanks for carbide tools, machine parts sub jea to shock, chisels, caulking rooh and all types of severe or unusual service Involving draxic or repeamd impad at atmospheric temperarums. Manufacturer: Allegheny-Ludlum Steel Corporatioo Brackenridge, Pennsylvania ...
Journal Articles
Alloy Digest (1956) 5 (7): TS-48.
Published: 01 July 1956
..., studs and ho10 for service at elevated temperatures, caulking and heading tools, shear blades, punches, cutting pliers. Hot work applications up to an o rating temperature of 1050 deg. F. for headers. piercers, ormiog tools, inserts for drop r forging dies, and heavy shear blades. Also for master hobs...