Journal Articles
Alloy Digest (2013) 62 (5): Ni-708.
Published: 01 May 2013
... Centralloy G4879 Micro is a cast nickel alloy with very good high-temperature properties. The alloy has carbides in a uniform dispersion that impede dislocation movement. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1986) 35 (7): Ni-334.
Published: 01 July 1986
... International Inc.. Producer or Source: Inco Alloys International Inc. Copyright © ASM International® 1996 1996 ASM International cast nickel alloys castability chemical composition corrosion-resistant alloys creep properties diesel engines heat treatability joinability machinability...
Journal Articles
Alloy Digest (1978) 27 (5): Ni-255.
Published: 01 May 1978
... CANNON-MUSKEGON Nickel Alloy C is a cast nickel-base alloy with exceptionally high resistance to corrosion and with excellent high-temperature properties. It also has outstanding oxidation resistance and strength at elevated temperatures. Its many uses include heat-treating equipment, aerospace...
Journal Articles
Alloy Digest (1977) 26 (11): Ni-251.
Published: 01 November 1977
... beryllium-nickel casting alloy that has been in use for over 40 years. Its many uses include tooling for plastics, glass-mold tooling, fuel-pump impellers, cores for Teflon molding and deep sour-well drilling components. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1982) 31 (10): Ni-279.
Published: 01 October 1982
... on corrosion and wear resistance as well as casting, heat treating, and joining. Filing Code: Ni-279. Producer or source: Cabot Corporation. Producer or Source: Cabot Corporation Copyright © ASM International® 1996 1996 ASM International BERYLCO ALLOY 42C cast nickel alloys castability chemical...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-12.
Published: 01 May 1996
.... Producer or source: Duriron Company Inc. Originally published November 1954, revised October 1980, revised May 1996. Producer or Source: Duriron Company Inc. Copyright © ASM International® 1996 1996 ASM International cast nickel alloys castability chemical composition Chlorimet 2 corrosion...
Journal Articles
Alloy Digest (1996) 45 (6): Ni-19.
Published: 01 June 1996
...: Ni-19. Producer or source: Duriron Company Inc. Originally published June 1955, revised November 1980, revised June 1996. Producer or Source: Duriron Company Inc. Copyright © ASM International® 1996 1996 ASM International cast nickel alloys castability chemical composition CHLORIMET 3...
Journal Articles
Alloy Digest (1963) 12 (8): Ni-85.
Published: 01 August 1963
... Nickel Copper Cast Alloy 410 is one of the most useful cast materials to withstand corrosives encountered in industry. It has tensile strength comparable to cast carbon steel and gives good performance under conditions of abrasion and erosion. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1974) 23 (2): Cu-275.
Published: 01 February 1974
... LEADED NICKEL BRONZE 65-20 is a cast copper-nickel zinc-tin alloy to which lead has been added to improve machinability. It is sometimes known as DAIRY BRONZE and has many marine, industrial and ornamental uses. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1993) 42 (2): Ni-84.
Published: 01 February 1993
... - DIGEST- WAUKESHA ALLOY 88* Filing Code: Ni-94 Nickel Alloy Revised FEBRUARY 1993 DATA ON WORLD WIDE METALS AND ALLOYS JULY 1963 P-by: AlloyDigest, lnc1201-677-9161 27 Canfll Stmel, Orange. NJ. 07060 I U.SA WAUKESHA ALLOY 88 (Nickel-Base Casting Alloy With Anti-Galling Properties) WAUKESHA METAL NO. 88...
Journal Articles
Alloy Digest (1993) 42 (3): Ni-49.
Published: 01 March 1993
... WAUKESHA METAL NO. 23 is a nickel-base casting alloy having high resistance to corrosion, good machinability, and freedom from any tendency to seize or gall. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1993) 42 (4): Ni-426.
Published: 01 April 1993
... WAUKESHA ALLOY 54C is a nickel-base casting alloy having high resistance to corrosion, superior resistance to galling or seizing in metal-to-metal application, and good castability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2020) 69 (4): Al-463.
Published: 01 April 2020
... Rio Tinto Alloy 242.2 is a heat-treatable, aluminum-copper-magnesium-nickel casting alloy. It is available in the form of ingots to be remelted for the manufacture of sand and permanent mold castings. Alloy 242.0 is used extensively for applications requiring high strength and hardness at elevated...
Journal Articles
Alloy Digest (1975) 24 (1): Ni-214.
Published: 01 January 1975
... Nickel-Copper Alloys 410 and 411 are strong and ductile casting alloys; they are generally used in conjunction with wrought counterparts. They can be cast readily into fittings such as elbows, tees, return bends, flanges and similar components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1975) 24 (2): Ni-215.
Published: 01 February 1975
... Nickel-Copper Alloys 505 and 506 are strong castings alloys. Both alloys combine high strength with good wear resistance. Alloy 505 (4% silicon) is employed where exceptional resistance to galling is needed. Alloy 506 (3% silicon) is recommended where good (but not exceptional) galling resistance...
Journal Articles
Alloy Digest (1968) 17 (9): Ni-138.
Published: 01 September 1968
... Brush Alloy 260-C is a beryllium nickel casting alloy having high strength, hardness and good corrosion resistance. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (2): Ni-142.
Published: 01 February 1969
... BRUSII Alloy 200C is a beryllium-nickel casting alloy having high resistance to wear, corrosion, thermal shock and oxidation. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1976) 25 (9): Cu-319.
Published: 01 September 1976
... Copper Alloy No. 962 is a cast copper-nickel alloy to which about 1.4% iron has been added to increase its resistance to corrosion by salt water. It is recommended where superior mechanical properties, weldability and corrosion resistance are needed. It is widely used for such parts as valves...
Journal Articles
Alloy Digest (1986) 35 (12): Cu-519.
Published: 01 December 1986
... Copper Alloy No. C91700 is a medium strength casting alloy. Formerly it was known as Nickel Gear Bronze and 861/2-12- 0-0-11/2; these names are no longer recommended. It has a good combination of strength, ductility and resistance to corrosion and wear. Its typical tensile strength is 60,000 psi...
Journal Articles
Alloy Digest (1956) 5 (9): Ni-27.
Published: 01 September 1956
... Jersey BERYLCO CR-l (Beryllium Nickel Casting Alloy) BERYLCO CR-1 is a high strength, corrosion resistant beryllium-nickel alloy which responds readily to an age-hard- ening heat treatment. Composition: Nominal Beryllium 2.75 C&On 0.50 max. Nickel balance PROPERTIES Table 1 - AS-CAST PROPERTIES - MINIMUM...