Skip Nav Destination
Close Modal
Search Results for
cast iron
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 1628 Search Results for
cast iron
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1977) 26 (9): CI-44.
Published: 01 September 1977
... CENTRI-CAST GRAY IRON 40 is a centrifugally cast gray iron with a nominal tensile strength of 40,000 psi. It is produced in the form of tubing which has a wide range of uses in applications where size and shape are of paramount importance and freedom from pattern cost is an important consideration...
Abstract
View article
PDF
CENTRI-CAST GRAY IRON 40 is a centrifugally cast gray iron with a nominal tensile strength of 40,000 psi. It is produced in the form of tubing which has a wide range of uses in applications where size and shape are of paramount importance and freedom from pattern cost is an important consideration. Typical applications are automotive equipment, compressors, machine tools and general machinery applications. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on casting, heat treating, machining, and surface treatment. Filing Code: CI-44. Producer or source: Federal Bronze Products Inc..
Journal Articles
Alloy Digest (1978) 27 (10): CI-46.
Published: 01 October 1978
... CENTRI-CAST GRAY IRON 30 is a centrifugally cast gray iron with a nominal tensile strength of 30,000 psi. It is produced in the form of tubing which has a wide range of uses for applications where freedom from pattern cost is an important consideration and where size and shape are of paramount...
Abstract
View article
PDF
CENTRI-CAST GRAY IRON 30 is a centrifugally cast gray iron with a nominal tensile strength of 30,000 psi. It is produced in the form of tubing which has a wide range of uses for applications where freedom from pattern cost is an important consideration and where size and shape are of paramount importance. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on casting, heat treating, machining, and surface treatment. Filing Code: CI-46. Producer or source: Federal Bronze Products Inc..
Journal Articles
Alloy Digest (1979) 28 (9): CI-48.
Published: 01 September 1979
... CENTRI-CAST GRAY IRON 55 is a centrifugally cast gray iron with a nominal tensile strength of 55,000 psi. It is produced in the form of tubing which has a wide range of uses in applications where size and shape are of paramount importance and freedom from pattern cost is an important consideration...
Abstract
View article
PDF
CENTRI-CAST GRAY IRON 55 is a centrifugally cast gray iron with a nominal tensile strength of 55,000 psi. It is produced in the form of tubing which has a wide range of uses in applications where size and shape are of paramount importance and freedom from pattern cost is an important consideration. Typical applications are seals, bushings, farm machinery, casings and general machinery uses. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on casting, heat treating, machining, and surface treatment. Filing Code: CI-48. Producer or source: Federal Bronze Products Inc..
Journal Articles
Alloy Digest (1980) 29 (6): CI-50.
Published: 01 June 1980
... CENTRI-CAST GRAY IRON 45 has a nominal tensile strength of 45,000 psi. It is gray iron cast centrifugally in the form of tubing which has a wide range of uses for applications where freedom form pattern cost is an important consideration and where size and shape are of paramount importance. Its...
Abstract
View article
PDF
CENTRI-CAST GRAY IRON 45 has a nominal tensile strength of 45,000 psi. It is gray iron cast centrifugally in the form of tubing which has a wide range of uses for applications where freedom form pattern cost is an important consideration and where size and shape are of paramount importance. Its many applications include automotive equipment, farm machinery, bushings and machine tools. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on casting, heat treating, machining, joining, and surface treatment. Filing Code: CI-50. Producer or source: Federal Bronze Products Inc..
Journal Articles
Alloy Digest (1981) 30 (8): CI-51.
Published: 01 August 1981
... CENTRI-CAST GRAY IRON 50 is a centrifugally cast gray iron with a nominal tensile strength of 50,000 psi. It is cast in the form of tubing which has a wide range of uses in applications where size and shape are of paramount importance and freedom from pattern cost is an important consideration...
Abstract
View article
PDF
CENTRI-CAST GRAY IRON 50 is a centrifugally cast gray iron with a nominal tensile strength of 50,000 psi. It is cast in the form of tubing which has a wide range of uses in applications where size and shape are of paramount importance and freedom from pattern cost is an important consideration. Among its many applications are farm machinery, seals, bushings, machine tools and general machinery uses. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on casting, heat treating, machining, and surface treatment. Filing Code: CI-51. Producer or source: Federal Bronze Products Inc..
Journal Articles
Alloy Digest (2022) 71 (1): CI-89.
Published: 01 January 2022
... ACO Eurobar EN-GJL-150C (5.1102) is a low-tensile-strength gray cast iron that is produced by the continuous casting process. It is useful in situations where very high thermal conductivity, machinability, and damping capacity are important, but where tensile strength and hardness...
Abstract
View article
PDF
ACO Eurobar EN-GJL-150C (5.1102) is a low-tensile-strength gray cast iron that is produced by the continuous casting process. It is useful in situations where very high thermal conductivity, machinability, and damping capacity are important, but where tensile strength and hardness are not the crucial properties in service. The high carbon content of this material also imparts good lubricated bearing properties. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on heat treating. Filing Code: CI-89. Producer or source: ACO Eurobar GmbH.
Journal Articles
Alloy Digest (1959) 8 (3): CI-26.
Published: 01 March 1959
... PEARLITIC MALLEABLE IRON is a high strength cast iron recommended for dependable service, strength and machinability in highly stressed parts at work in mobile and stationary mechanisms. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Abstract
View article
PDF
PEARLITIC MALLEABLE IRON is a high strength cast iron recommended for dependable service, strength and machinability in highly stressed parts at work in mobile and stationary mechanisms. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: CI-26. Producer or source: Albian Malleable Iron Company.
Journal Articles
Alloy Digest (1972) 21 (12): CI-37.
Published: 01 December 1972
...-br. VN%& Upper I SORBO-MAT DUCTILE IRON (Ductile Cast Iron) SORBQ-MAT DUCTILE IRON is a highcarbon ferrous material It is produced in five varieties providing various combinations of strength and toughness. COmpoSitiOll: SlU-60-E Total carbon 33ck3 SO Silicon 2.2G2.80 Manganese 020-0.40 Phosphorus...
Abstract
View article
PDF
SORBO-MAT DUCTILE IRON is a high-carbon ferrous material. It is produced in five varieties providing various combinations of strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on casting, heat treating, machining, and joining. Filing Code: CI-37. Producer or source: Sorbo-Mat Process Corporation.
Journal Articles
Alloy Digest (1990) 39 (7): CI-61.
Published: 01 July 1990
... DURA-BAR G1A alloyed iron is engineered for the glass mold industry. It is produced by continuous casting which results in fine graphite flake size and size and fine matrix structure. This datasheet provides information on composition, microstructure, and hardness. It also includes information...
Abstract
View article
PDF
DURA-BAR G1A alloyed iron is engineered for the glass mold industry. It is produced by continuous casting which results in fine graphite flake size and size and fine matrix structure. This datasheet provides information on composition, microstructure, and hardness. It also includes information on heat treating and machining. Filing Code: CI-61. Producer or source: Federal Bronze Products Inc..
Journal Articles
Alloy Digest (1956) 5 (9): CI-16.
Published: 01 September 1956
... properties tensile properties - h 1 Filing Code: Cl-16 DUCTILE IRON Cast Iron SEPTEMBER 1956 - DATA ON WORLD WIDE METALS AND ALLOYS . Pvblishd by. Ihgkemg Allpys Digest, Inc Upper hfomhr, New Jew DUCTILE IRON (Ductile Cast Iron) DUCTILE IRON is a high carbon ferrous mateA having high strength, high...
Abstract
View article
PDF
DUCTILE IRON is a high carbon ferrous material having high strength, high ductility, toughness, good castability and ready machinability. It is a family of materials and is produced in six different commercial types providing various combinations of strength, ductility and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on heat treating, machining, and joining. Filing Code: CI-16. Producer or source: International Nickel Company Inc..
Journal Articles
Alloy Digest (2020) 69 (9): CI-73.
Published: 01 September 2020
... ISO 185/JL/225 is an intermediate-tensile-strength gray cast iron that has a predominantly pearlitic matrix, and a tensile strength of 225–325 MPa (33-47 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray...
Abstract
View article
PDF
ISO 185/JL/225 is an intermediate-tensile-strength gray cast iron that has a predominantly pearlitic matrix, and a tensile strength of 225–325 MPa (33-47 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades, ISO 185/JL/225 contains lower carbon and silicon contents, while still maintaining excellent thermal conductivity, damping capacity, and machinability. This datasheet provides information on composition, physical properties, tensile properties, and compressive strength as well as fatigue. It also includes information on heat treating. Filing Code: CI-73. Producer or source: International Organization for Standardization (ISO).
Journal Articles
Alloy Digest (2020) 69 (11): CI-75.
Published: 01 November 2020
... Meehanite GB300 is a pearlitic gray cast iron that has a minimum tensile strength of 300 MPa (44 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. This grade exhibits high strength while still maintaining good thermal conductivity and good...
Abstract
View article
PDF
Meehanite GB300 is a pearlitic gray cast iron that has a minimum tensile strength of 300 MPa (44 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. This grade exhibits high strength while still maintaining good thermal conductivity and good machinability. It is generally used for applications where the thermal conductivity requirements preclude the use of other higher-strength materials, such as spheroidal graphite cast irons, which have inferior thermal properties. This datasheet provides information on physical properties, hardness, tensile properties, and compressive strength as well as fatigue. It also includes information on low and high temperature performance as well as heat treating, machining, and joining. Filing Code: CI-75. Producer or source: Meehanite Metal Corporation.
Journal Articles
Alloy Digest (1967) 16 (10): CI-34.
Published: 01 October 1967
... properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: CI-34. Producer or source: Alloy iron foundries. Producer or Source: Alloy iron foundries...
Abstract
View article
PDF
Ni-Hard Type 4 is a wear-resistant martensitic white iron with improved resistance to fracture under repeated impact. It is recommended for jaw crushers, hammer mills, pulverizers and similar heavy duty wear resistant components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: CI-34. Producer or source: Alloy iron foundries.
Journal Articles
Alloy Digest (2020) 69 (12): CI-76.
Published: 01 December 2020
... ISO 185/JL/250 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 250–350 MPa (36–51 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Abstract
View article
PDF
ISO 185/JL/250 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 250–350 MPa (36–51 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades, ISO 185/JL/250 contains lower carbon and silicon contents and has superior wear resistance, while still maintaining good thermal conductivity, damping capacity, and machinability. This datasheet provides information on composition, physical properties, and tensile properties as well as fatigue. It also includes information on casting and heat treating. Filing Code: CI-76. Producer or source: ISO Central Secretariat.
Journal Articles
Alloy Digest (2021) 70 (1): CI-77.
Published: 01 January 2021
... Dura-Bar G2A is a gray cast iron that is used for the production of continuous cast products. It contains Type VII, Distribution D flake graphite in a predominantly pearlitic matrix and is typically used in permanent mold applications requiring a combination of optimal strength and wear resistance...
Abstract
View article
PDF
Dura-Bar G2A is a gray cast iron that is used for the production of continuous cast products. It contains Type VII, Distribution D flake graphite in a predominantly pearlitic matrix and is typically used in permanent mold applications requiring a combination of optimal strength and wear resistance, and superior surface finish. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties as well as fatigue. It also includes information on heat treating. Filing Code: CI-77. Producer or source: Charter Dura-Bar, Inc.
Journal Articles
Alloy Digest (2021) 70 (2): CI-78.
Published: 01 February 2021
... Meehanite GC275 is a pearlitic gray cast iron that has a minimum tensile strength of 275 MPa (40 ksi) when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter, test bars. This intermediate-tensile-strength grade has a fine, close-grained structure that is ideal...
Abstract
View article
PDF
Meehanite GC275 is a pearlitic gray cast iron that has a minimum tensile strength of 275 MPa (40 ksi) when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter, test bars. This intermediate-tensile-strength grade has a fine, close-grained structure that is ideal for finishing cuts. It is used for a wide variety of applications on account of its useful combination of good all round properties with adaptability to production of small and large volumes. This datasheet provides information on physical properties, hardness, and tensile properties as well as fatigue. It also includes information on heat treating, machining, and joining. Filing Code: CI-78. Producer or source: Meehanite Metal Corporation.
Journal Articles
Alloy Digest (2021) 70 (3): CI-79.
Published: 01 March 2021
... ISO 185/JL/275 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 275–375 MPa (40–54 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades...
Abstract
View article
PDF
ISO 185/JL/275 is an intermediate-tensile-strength gray cast iron that has a pearlitic matrix and a tensile strength of 275–375 MPa (40–54 ksi), when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter test bars. Compared with the lower strength gray cast iron grades, ISO 185/JL/275 contains lower carbon and silicon contents, while still maintaining good thermal conductivity and damping capacity. Owing to its higher tensile strength and hardness, it exhibits superior wear properties. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information on casting and heat treating. Filing Code: CI-79. Producer or source: International Organization for Standardization.
Journal Articles
Alloy Digest (1952) 1 (4): CI-1.
Published: 01 December 1952
... NODULOY is a magnesium inoculated ductile cast iron in which the graphite is in the nodular form. It offers excellent castability, high mechanical properties, good machinability, pressure tightness, high modulus, and excellent shock resistance. It has extraordinary high ductility in the annealed...
Abstract
View article
PDF
NODULOY is a magnesium inoculated ductile cast iron in which the graphite is in the nodular form. It offers excellent castability, high mechanical properties, good machinability, pressure tightness, high modulus, and excellent shock resistance. It has extraordinary high ductility in the annealed state. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: CI-1. Producer or source: Dominion Wheel & Foundries Ltd.
Journal Articles
Alloy Digest (1961) 10 (8): CI-30.
Published: 01 August 1961
... Alten 50 WR is a low alloy cast iron recommended for high strength and pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code...
Abstract
View article
PDF
Alten 50 WR is a low alloy cast iron recommended for high strength and pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: CI-30. Producer or source: Alten Foundry & Machine Works Inc..
Journal Articles
Alloy Digest (1953) 2 (9): CI-2.
Published: 01 September 1953
... AFCOMET 40 is a dense, close-grained nickel-molybdenum cast iron with good resistance to wear and abrasion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness...
Abstract
View article
PDF
AFCOMET 40 is a dense, close-grained nickel-molybdenum cast iron with good resistance to wear and abrasion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: CI-2. Producer or source: Atlas Foundry Company.