1-20 of 916 Search Results for

cast copper alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (12): Cu-504.
Published: 01 December 1985
.... Filing Code: Cu-504. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast copper alloys castability chemical composition Copper alloy no. C81400 elasticity hardness heat treatability...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (4): Cu-508.
Published: 01 April 1986
... Copper Alloy No. C813000 is a cast copper-base alloy containing nominally 0.8% cobalt and 0.06% beryllium. Thus it is a beryllium-modified copper-cobalt alloy. Because of its beryllium content, its manufacture may present a health hazard. C81300 is a precipitation-hardenable alloy with moderate...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (5): Cu-332.
Published: 01 May 1977
... Copper Alloy No. 815 is an age-hardenable cast copper-chromium alloy. It is characterized by high electrical and thermal conductivities combined with medium hardness and strength in the age-hardened condition. It is used for components requiring high electrical conductivity or high thermal...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (7): Cu-574.
Published: 01 July 1992
... BRUSH CASTING ALLOY 3C is in the beryllium copper family, offering high thermal and electrical conductivity with moderate strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (7): Cu-573.
Published: 01 July 1992
... BRUSH CASTING ALLOY 10C, a beryllium copper alloy, offers excellent thermal and electrical conductivity with moderate strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (12): Cu-531.
Published: 01 December 1987
... Copper Alloy No. C91000 is a cast copper-tin alloy which also is known by names formerly used (but not recommended): 197, Tin Bronze and 85-14-0-1. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Its uses include piston rings...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (3): Cu-494.
Published: 01 March 1985
... Copper Alloy No. C90900 is a cast copper-tin alloy which also is known by names formerly used (but not recommended): Tin Bronze, 199 and 87-13-0-0. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Its uses include bearings, bushings...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (9): Cu-319.
Published: 01 September 1976
... Copper Alloy No. 962 is a cast copper-nickel alloy to which about 1.4% iron has been added to increase its resistance to corrosion by salt water. It is recommended where superior mechanical properties, weldability and corrosion resistance are needed. It is widely used for such parts as valves...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (2): Cu-506.
Published: 01 February 1986
... Copper Alloy No. C87400 is a copper-base casting alloy containing nominally 14% zinc and 3.5% silicon. It possesses a combination of high strength, good ductility and good-to-excellent resistance to corrosion. This alloy cannot be hardened nor strengthened by any thermal treatment. It is used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (6): Cu-525.
Published: 01 June 1987
... on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-525. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright ©...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (8): Cu-527.
Published: 01 August 1987
... Copper Alloy No. C82600 is an age-hardenable copper-base casting alloy. Nominally it contains 2.3% beryllium. It is characterized by high strength, toughness and good corrosion resistance. Typical uses comprise bearings and molds for plastics. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (6): Cu-460.
Published: 01 June 1983
... Copper Alloy No. C90700 is a cast copper-tin alloy known also by names formerly used (but not recommended): Tin Bronze, 205 and 89-11. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Among its many uses are gears, bearings, bushings...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (4): Cu-523.
Published: 01 April 1987
... Copper Alloy No. C82000 is an age-hardenable copper-base casting alloy containing nominally 0.6% beryllium. Its common name is Beryllium Copper Casting Alloy 10C. It offers fairly high strength and moderate ductility with good resistance to corrosion. Its applications include bearings and bushings...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (4): Cu-370.
Published: 01 April 1979
... on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-370. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast copper alloys...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (2): Cu-521.
Published: 01 February 1987
... treating, machining, joining, and surface treatment. Filing Code: Cu-521. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast copper alloys castability chemical composition Copper alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (3): Cu-507.
Published: 01 March 1986
... includes information on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-507. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (1): Cu-795.
Published: 01 January 2011
... as fracture toughness and fatigue. It also includes information on casting. Filing Code: Cu-795. Producer or source: AMPCO Engineered Alloys. Producer or Source: AMPCO Engineered Alloys Copyright © ASM International® 2011 2011 ASM International AMPCO 18.136 AMPCO 18.22 cast copper alloys...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (9): Cu-340.
Published: 01 September 1977
... BELMONT ALLOY 4977 is a high-strength alloy for casting. Its high strength is achieved by solution treating and precipitation (age) hardening. It has good resistance to corrosion. This alloy is the most widely used high-strength beryllium-copper casting alloy; among its many uses are valves, pump...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (9): Cu-380.
Published: 01 September 1979
... AMPCOLOY 525 is a cast copper-nickel alloy to which norminally 1.5% iron has been added to increase its resistance to corrosion by salt water. It is recommended where superior corrosion resistance. weldability and mechanical properties are required. Among its many uses are parts that must...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (1): Cu-346.
Published: 01 January 1978
... Copper Alloy No. 838 is a free-cutting copper-base alloy for castings. It was formerly identified as Commercial Red Brass or 83-4-6-7 alloy. It offers an excellent combination of corrosion resistance, machinability, moderate strength and good casting characteristics. Its wide use includes...