Skip Nav Destination
Close Modal
Search Results for
car electrical systems
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 22 Search Results for
car electrical systems
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (2002) 51 (8): Cu-686.
Published: 01 August 2002
... Wieland-B14 is a phosphor bronze with a composition that optimizes conductivity while maintaining a reasonable cost. Application is in high-current connectors, especially for car electrical systems. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View article
PDF
Wieland-B14 is a phosphor bronze with a composition that optimizes conductivity while maintaining a reasonable cost. Application is in high-current connectors, especially for car electrical systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CU-686. Producer or source: Wieland Metals Inc., Wieland-Werke AG.
Journal Articles
Alloy Digest (2009) 58 (8): SS-1039.
Published: 01 August 2009
... applications for Nikrothal 30 are solid hot plates, open coil heaters in HVAC systems, night-storage heaters, convection heaters, heavy-duty rheostats, and fan heaters. Nikrothal 30 is also used in heating cables and rope heaters in defrosting and deicing elements, electric blankets and pads, car seats...
Abstract
View article
PDF
Nikrothal 30 is one of a family of austenitic alloys used in resistance wires for electric heating. It has good ductility after use, good corrosion resistance except in sulfur-containing atmospheres and certain controlled atmospheres, and excellent weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: SS-1039. Producer or source: Kanthal AB.
Journal Articles
Alloy Digest (1976) 25 (12): Cu-323.
Published: 01 December 1976
... DZR Yellow Brass is a new, corrosion-resistant brass. It has excellent resistance to dezincification which makes it highly suitable for water-system applications, marine hardware, ornaments and door handles. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
DZR Yellow Brass is a new, corrosion-resistant brass. It has excellent resistance to dezincification which makes it highly suitable for water-system applications, marine hardware, ornaments and door handles. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Cu-323. Producer or source: Federated Metals Corporation.
Journal Articles
Alloy Digest (2001) 50 (5): SS-823.
Published: 01 May 2001
... Aluchrom I SE is an oxidation resistant ferritic stainless steel alloyed with aluminum and rare earth elements. Applications include framework for catalytic automobile muffler systems. This datasheet provides information on composition, physical properties, and tensile properties as well as creep...
Abstract
View article
PDF
Aluchrom I SE is an oxidation resistant ferritic stainless steel alloyed with aluminum and rare earth elements. Applications include framework for catalytic automobile muffler systems. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-823. Producer or source: Krupp VDM.
Journal Articles
Alloy Digest (2009) 58 (3): Mg-76.
Published: 01 March 2009
... and other power systems, helicopter transmissions, missiles, and racing and high- performance cars. Producer: Magnesium Elektron Wrought Products, North America Madison, IL 62060 Tel: 618-452-5190 Fax: 618-452-7929 In United Kingdom: Magenium Elektron UK Operations Swinton, Manchester England M27 8DD Tel...
Abstract
View article
PDF
Elektron WE43 was developed by Magnesium Elektron for use to 300 deg C and has good mechanical properties at these temperatures. The alloy is used in military and motorsport applications where these properties are at a premium. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: MG-76. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... CARPENTER STAINLESS TYPE 430 is a chromium stainless steel that is especially useful for all types of decorative trim. This steel is suitable for trim on automobiles, cameras, vending machines, counters and showcases, electrical appliances and finished hardware in the building trade. The alloy...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 430 is a chromium stainless steel that is especially useful for all types of decorative trim. This steel is suitable for trim on automobiles, cameras, vending machines, counters and showcases, electrical appliances and finished hardware in the building trade. The alloy also has many applications in both the petrochemical and chemical area. Type 430 has moderate strength and good ductility. It can be cold worked readily for producing trim and can be joined successfully by several methods. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, and deformation. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-384. Producer or source: Carpenter. Originally published March 1981, revised April 1995.
Journal Articles
Alloy Digest (1998) 47 (7): SS-723.
Published: 01 July 1998
.... Applications: Automobile molding and trim. wheel covers, conveyor belts. kitchen equipment, roof drainage systems, hose ctarnps. springs. truck and trailer bodies, railway and subway cars Products Available: Cold-rolled strip. sheets, plates Producer: Allegheny Ludlum Corporation Pittsburgh PA 15222.5479 (412...
Abstract
View article
PDF
Allegheny Ludlum type 301 is the basic 18-8 chromium-nickel austenitic stainless steel with both chromium and nickel content lower than types 302 and 304. The steel is capable of attaining high tensile strength with good ductility by moderate or severe cold working. A typical application is conveyor belts in the food processing industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as heat treating. Filing Code: SS-723. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1988) 37 (11): Al-292.
Published: 01 November 1988
... Constants: Density, lb/cu in. specific gravity Melting range, OF Thermal coef. expansionpF(68-212°F) Thermal conductivity, Btu/hr/sq ftpFlin. Electrical conductivity, % IACS Electrical resistivity, microhm-cm Modulus of elasticity, psi Modulus of rigidity, psi 0.098 2.70 1080-1205 13.1 x 104 1250 47 3.7...
Abstract
View article
PDF
UNS A96061 is a wrought precipitation-hardenable aluminum alloy having excellent resistance to corrosion and good mechanical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-292. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1973) 22 (1): Al-205.
Published: 01 January 1973
... Physical Constants: Density, Ib/cu in. specik gravity Melting range, oF Tkmal coef. expansion/aF (68-2120F) Tlmmal coahctivity, Btu/hx/sq ft/oF/in. Electrical conductivity, 96 IACS Electrical resislivity, microhm-cm Modulus of elasticity, psi Modulus of rigidity, psi 0.098 2.70 lwt-1205 13.1 x 10-6 1250 47...
Abstract
View article
PDF
ALUMINUM 6061 is a wrought precipitation-hardenable aluminum alloy having excellent resistance to corrosion and good mechanical properties. (This alloy is covered under its old designation, ALUMINUM 61S, in Alloy Digest Al-3, November 1952.) This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-205. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (2004) 53 (1): SS-898.
Published: 01 January 2004
...) Specific heat capacity, 0 100 °C (32 212 °F), J/kg K (Btu/lb °F) 502 (0.12) Coefficient of linear thermal expansion, 10 6/K (10 6/°F) 0 100 °C (32 212 °F) 16.7 (9.3) 0 316 °C (32 600 °F) 17.9 (9.5) 0 558 °C (32 1000 °F) 18.5 (10.3) 0 649 °C (32 1200 °F) 19.3 (10.7) Electrical resistivity, 21 °C (70 °F...
Abstract
View article
PDF
Type 347 (UNS S34700) and type 348 (UNS S34800) are austenitic chromium-nickel stainless steels containing columbium and tantalum. These grades are recommended where it is preferred to omit the annealing operation after welding. They are also recommended for service at temperatures between 425 and 900 deg C (800 and 1650 deg F). Type 348 is used in applications that require a restricted tantalum content such as those encountered in radioactive service. These types are essentially non-magnetic when annealed and become slightly magnetic when cold worked. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-898. Producer or source: J & L Specialty Steel Inc.
Journal Articles
Alloy Digest (1994) 43 (1): SS-560.
Published: 01 January 1994
... with good tools of high speed steel (good cooling required) or preferably with tungsten car- bide tools. Physical Properties: Density lb/m3 (g/cxn3) Electrical resistivity at RI microhm-crn (ohm-rnrn*/m> Coefficient of thermal expansion between Rt and [lOdin/in*°F(lWm/n+ C)J 210°F (1OOT) 390°F (2OO C) 570°F...
Abstract
View article
PDF
REMANIT 4539 is a low carbon corrosion resistant austenitic stainless steel with good levels of chromium, nickel, molybdenum, copper and nitrogen to show good resistance to reducing acids and chloride solutions. It was one of the early alloys used in flue gas desulfurization equipment. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-560. Producer or source: Thyssen Stahl AG.
Journal Articles
Alloy Digest (1986) 35 (2): SS-424.
Published: 01 February 1986
... (Zl-204°C) (21-427 (Z) (21-871 C) Thermal conductivity, Btu/ft*/hr/ft/ OF (At 4OO F) (At 16OO F) W,:mI°C (At 204 C) (At 871 C) Electrical resistivity. microhm-cm (At 70 F) Modulus of elasticity, psi (Tension) MPa (Tension) PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES OF 1950°F ANNEALED ALLOY...
Abstract
View article
PDF
ARMCO 12 SR was developed specifically for automotive exhaust applications. It has greater oxidation resistance than AISI Type 409 and it exhibits formability and weldability comparable to more highly alloyed ferritic grades. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-424. Producer or source: Armco Inc., Eastern Steel Division. Originally published April 1983, revised February 1986.
Journal Articles
Alloy Digest (2023) 72 (6): SS-1359.
Published: 01 June 2023
...; high strength; good ductility; excellent corrosion resistance; good oxidation resistance. Product Forms Cold rolled plate, sheet, and strip. Applications Automobile molding and trim; hose clamps; kitchen equipment; railway and subway cars; roof drainage systems; springs; truck and trailer bodies; wheel...
Abstract
View article
PDF
ATI 301 (UNS S30100) is an austenitic stainless steel with a nominal composition of 17 percent chromium and 7 percent nickel. The high strength of this grade of steel in the six available conditions or tempers, its resistance to atmosphere corrosion, and its bright, attractive surface make it an excellent choice for decorative structural applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: SS-1359. Producer or source: ATI.
Journal Articles
Alloy Digest (1982) 31 (11): SS-416.
Published: 01 November 1982
...-pressure systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface...
Abstract
View article
PDF
JESSOP JS15Cr-5Ni is a martensitic, precipitation-hardening, chromium-nickel-copper stainless steel. It offers high strength and hardness in combination with good resistance to corrosion. Typical applications include aircraft components and a variety of fabricated parts for use in corrosive, high-pressure systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-416. Producer or source: Jessop Steel Company.
Journal Articles
Alloy Digest (2001) 50 (3): SS-820.
Published: 01 March 2001
... Properties: (Typical) Density, kg/m3 (lb/in.3 ) 7900 (0.2844) Electrical resistivity at 20 °C (68 °F), µ · m ( circular-mil/ft) 0.85 (510) Magnetic permeability Nonmagnetic Thermal conductivity at 20 °C (68 °F), W/m · K (Btu/(ft · h · °F)) 15 (8.7) Specific heat capacity at 20 °C (68 °F), J/kg · K (Btu/lb...
Abstract
View article
PDF
ALZ 309 is a high-silicon, austenitic stainless steel combining high resistance to oxidation with high tensile and creep strength at elevated temperatures. Corrosion resistance is excellent. The steel has good ductility and is readily welded so that difficult shapes and structures are easily fabricated. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-820. Producer or source: ALZ nv.
Journal Articles
Alloy Digest (1974) 23 (8): Cu-283.
Published: 01 August 1974
... range, oF (Liquidus) (Solidus) Specific heat, Btu/lb/oF (At 680F) Thermal coef. expansion/OF 68-2120F) 1 Thermal conductivity, Btu/ft /ft/hr/oF (At 680F) Electrical resistivity, Ohm/& mil/ft (At 680F) Electrical conductivity,* % IACS (At 680F) Modulus of elasticity, psi Modulus of rigidity, psi *Volume...
Abstract
View article
PDF
COPPER ALLOY NO. 953 is an age-hardenable alloy offering high strength and hardness, good resistance to fatigue and wear, and excellent corrosion resistance. It can be used at temperatures up to 750 F. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-283. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1992) 41 (4): Ni-401.
Published: 01 April 1992
... Specific heat, Btu/lb* F 0.12 Carbon 0.02 max. J/kg-=C 500 Manganese 2.0 max. Thermal conductivity, Btu*in/ftz=h- F 116 Phosphorus 0.030 max. W/m= C 16.7 Sulfur 0.010 max. Thermal coef. of expansion (68-212 F), IOin- F 8.4 Silicon 0.50 max. (20-lOO C), lO m/m- C 15.1 Iron Remainder Electrical resistivity...
Abstract
View article
PDF
INCO Alloy 25-6 MO is a highly alloyed austenitic nickel/iron alloy that is especially resistant to non-oxidizing acids such as sulfuric and phosphoric. It is also well suited to handle high-chloride environments and to combat microbially influenced corrosion. (See updated alloy Incoloy Alloy 25-6Mo, Alloy Digest SS-962, May 2006.) This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-401. Producer or source: Inco Alloys International Inc..
Journal Articles
Alloy Digest (2009) 58 (4): Mg-77.
Published: 01 April 2009
... of power systems, transmissions, missiles, high\- performance cars, and other high-technology applications. Producer: Magnesium Elektron Wrought Products, North America Madison, IL 62060 Tel: 618-452-5190 Fax: 618-452-7929 In United Kingdom: Magnesium Elektron UK Operations Swinton, Manchester, England M27...
Abstract
View article
PDF
ElektronWE54 is fully heat treatable for use to 300 deg C (570 deg F) and is free of silver and thorium. The alloy is used in military and motorsport applications where these properties are at a premium. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: MG-77. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
Alloy Digest (2001) 50 (10): SS-833.
Published: 01 October 2001
.... Applications include sheathing for electric heating elements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating...
Abstract
View article
PDF
Allegheny Ludlum Type 334 is an austenitic stainless steel with alloying elements of aluminum and titanium. These additions, along with its higher chromium and nickel levels, give the alloy excellent strength and oxidation resistance, especially when compared to Type 304 stainless steel. Applications include sheathing for electric heating elements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-833. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1993) 42 (11): SS-556.
Published: 01 November 1993
... + 30 x % N) Fig. 1 -Critical pitting temperature tested in aerated 3% NaCI- solution at 950 mV vs. SHE as a function of the pitting index. Heat Treatment All products are normally delivered in the solution-annealed and quenched condition. The annealing heat treatment is car- ried out between 1905.2050...
Abstract
View article
PDF
REMANIT 4439 is a highly corrosion resistant steel with low carbon content, an addition of nitrogen to enhance both mechanical properties and corrosion resistance, and higher molybdenum than most stainless steels to resist pitting and crevice corrosion in chloride media. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-556. Producer or source: Thyssen Stahl AG.