Alloy Digest (1987) 36 (10): TS-482.
Published: 01 October 1987
... strength and long runs between grinds are necessary. Among its many applications are blanking dies, burnishing tools, beading rolls, lathe centers, plug gages, spinning tools, slitters and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also...
Journal Articles
Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... blanking and cold-drawing dies, punches, burnishing tools, slitter knives and gages. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating and machining. Filing Code: TS-361. Producer or source: Guterl Special Steel Corporation...
Journal Articles
Alloy Digest (1980) 29 (6): TS-364.
Published: 01 June 1980
... resistance and toughness. Among the many uses of Guterl A-2 are shear blades, blanking and forming dies, punches and burnishing tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining...
Journal Articles
Alloy Digest (1985) 34 (12): TS-451.
Published: 01 December 1985
... of applications includes can dies, coining dies, extrusion dies, slitters, roofing knives, burnishing tools and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-451...
Journal Articles
Alloy Digest (1966) 15 (3): TS-176.
Published: 01 March 1966
... VANADIUM Type H is a high carbon, chromium-vanadium alloy steel of the water-hardening or oil-hardening type having high wear resistance combined with toughness. It has good depth hardenability when water hardened. It is recommended for punches, dies, cutters, burnishing tools, caulking tools...
Journal Articles
Alloy Digest (1978) 27 (8): TS-337.
Published: 01 August 1978
..., toughness and red hardness. Forms Available: Round bars in various finishes. squares, flats, rod, wire, strip, billets, forgings and special shapes. Applications: Blanking dies, boring tools, broaches, burnishing tools, cast-iron cutting tools. chasers, chisels, countersinks, counterboring tools, cut-off...
Journal Articles
Alloy Digest (1963) 12 (4): TS-132.
Published: 01 April 1963
... and wire drawing dies, gauges, punches, burnishing tools, thread rolling dies, hot swaging dies, forming tools and rolls, trimmer &es. Manufacturer: Crucible Steel Co. of America Pittsburgh, Pennsylvania ...
Journal Articles
Alloy Digest (1976) 25 (9): TS-307.
Published: 01 September 1976
... in the annealed condition and ground in the hardened condition. Hot working is done in the range 1650.2OOOoF (900. 11OOoC). It has a wide range of applications. Forms Available: Billets, bars, forgings, rods. special shapes and strip. Applications: Blanking dies. boring tools. broaches. burnishing tools. cast...
Journal Articles
Alloy Digest (1955) 4 (10): TS-39.
Published: 01 October 1955
...-seiz- ing properties. Forms Available: Bars, billets, wire, sheets, strips, and forgings. Applications: Air hammer pistons, coining and drawing dies, blank- ing dies and punches, burnishing tools, circular sheat blades, heavy duty bushings, extrusion dies and plun- gers, nozzles, reamers, rolls...
Journal Articles
Alloy Digest (1987) 36 (2): TS-470.
Published: 01 February 1987
... duty), swaging dies, trim dies, thread-rolling dies, coining dies. punches. plug and ring gages, rolls (edge and forming). draw dies. shear blades. burnishing tools. slitters. lathe centers. extrusion dies, header-die inserts. forming mandrels and extrusion mandrels. Manufacturer: Columbia Tool Steel...
Journal Articles
Alloy Digest (1980) 29 (7): TS-366.
Published: 01 July 1980
..., crimping, cutting, drawing, extruding, forming, hobbing and punching; slotting dies; stamping dies; thread-rolling dies; trimming dies; blanking dies; brass-turning tools; burnishing tools; bushings; cutters; drill plugs; brick molds; plug and ring gages; punches; reamers; sand-blast nozzles, spindle...
Journal Articles
Alloy Digest (1978) 27 (11): TS-341.
Published: 01 November 1978
..., forming rolls, seaming rolls, burnishing tools, punches, gages, knurls, wear parts. Manufacturer: Most tool steel mills. Depth of Feed Cutting Speed, sfpm Cut, inch in/rev. High-Speed Steel Carbide l/32 l/64 54-62 200-244 l/16 l/32 4148 180-200 W3 l/32 3542 160-190 l/4 l/64 33-37 170-190 112 l/64 20-26...
Journal Articles
Alloy Digest (1985) 34 (10): TS-448.
Published: 01 October 1985
... and forgings. Applications: Cold-work dies. cams. cutters. engravers tools. circular thread tools. feed rolls. shear blades. broaches. coining dies. gages, master tools and burnishing tools. Manufacturer: Latrobe Steel Company Subsidiary of The Timken Company Latrobe, Pennsylvania 15650. ...
Journal Articles
Alloy Digest (1959) 8 (2): TS-79.
Published: 01 February 1959
... rounds, flats and forgings. Applications: Burnishing tools, tube drawing dies, wire drawing dies, draw dies for stainless steel, cold extruding dies, brass cutting tools, eyelet dies, reamers, msem for heading or siring dies, finish- ing tools, forming dies, quills, sectional blanking dies, piercing...
Journal Articles
Alloy Digest (1965) 14 (3): TS-160.
Published: 01 March 1965
..., master hubs, trimming dies, forming dies, precision tools, gauges, coining dies, burnishing tools, mandrels, shear blades, deep drawing dies. Manufacturer: Carpenter Steel Company Reading, Pennsylvania ...
Journal Articles
Alloy Digest (1981) 30 (6): TS-384.
Published: 01 June 1981
..., hand tools, trimmer dies, thread-rolling dies, burnishing tools, ceramic-tile liners, brick-mold liners, lathe centers, grinding wheel molds and deep- drawing dies. Manufacturers: Tool steel mills. ...
Journal Articles
Alloy Digest (1965) 14 (2): TS-12.
Published: 01 February 1965
... of sharp comers and edges also appears much less pronounced. Forms Available: Annealed billets. bats. castinas. forPings. drili rods. tool bits, and welding rods. Applications: Broaches, burnishing tools, bushings, slitting cutters, dies for blanking-coining-cutting.drawing-extruding- forming...
Journal Articles
Alloy Digest (1969) 18 (4): TS-218.
Published: 01 April 1969
... Forms Available: Bars, rods and forgings and sheet Applications: Blanking and trimming dies, forming and drawing dies, thread rolling dies, coining dies, punches, gauges, rolls, bushings, shear blades, lathe centers, spinning tools, slitting cutters, knurls, burnishing tools, broaches. Manufacturer...
Journal Articles
Alloy Digest (1973) 22 (6): TS-257.
Published: 01 June 1973
..., cutters, cold-drawing dies, feed rolls, coining dies, burnishing tools. Manufacturer: Cannon-Muskegon Corporation Muskegon, Michigan 49441. ...
Journal Articles
Alloy Digest (1956) 5 (6): TS-47.
Published: 01 June 1956
... and strip miIIs where a high degree of abrasion resistance and shock re- sistance are required. It has a higher shock resistance &an can be obtained with the higher carbon grades. Forms Available: Annealed billets, bars, forgings, driII rods, and welding rods. Applications: Broaches, burnishing tools...