Journal Articles
Alloy Digest (2020) 69 (6): Cu-909.
Published: 01 June 2020
... Wieland C21000, also known as gilding metal, is a 95Cu-5Zn alloy. This versatile, low-cost alloy is often the choice of engineers for deep drawn parts such as bullet jackets and coined products. The combination of moderate conductivity and improved strength make C21000 a valuable option...
Journal Articles
Alloy Digest (1980) 29 (11): Cu-406.
Published: 01 November 1980
... characteristics are its greater resistance to season cracking than the yellow brasses, and its durability when exposed to the rigors of outdoor services. These properties have greatly extended Alloy 210 s use for general engineering purposes and in the manufacture of such ammunition components as bullet jackets...
Journal Articles
Alloy Digest (2009) 58 (5): Cu-770.
Published: 01 May 2009
... characteristics are its great resistance to season cracking, compared with yellow brasses, and its durability when exposed to the rigors of outdoor services. These properties have greatly extended its use to general engineering purposes and to the manufacture of small arms ammunition components such as bullet...
Journal Articles
Alloy Digest (1972) 21 (5): Cu-255.
Published: 01 May 1972
..., medals, and plaques. It is an excellent base for finishes and is often gold plated or enameled. Forms Available: Bar, extrusions, forgings, plate, sheet, strip, rod, pipe, tube, wire. Applications: Coins, medals, tokens, emblems, jewelry, plaques, bullet jackets, firing pin support shells, fuse caps...
Journal Articles
Alloy Digest (1961) 10 (1): Cu-95.
Published: 01 January 1961
... its gold color but is a true brass. Forms Available: Rolled and drawn flat products, wire, rolled or drawn strip. Applications: Coins, medals, tokens, bullet jackets, firing pin support shells, fuse caps, primers, emblems, jew- elry, plaques, base for gold plate and for vitreous enamel. Manufacturer...
Journal Articles
Alloy Digest (2009) 58 (6): Cu-771.
Published: 01 June 2009
... hardware, and munitions applications where fully exposed outdoor service or rigorous service exists. This includes its use as etching bronze, grillwork, chain links, screen cloth, escutcheons, line clamps, rivets, screws, bolts, and bullet jackets. For appearance, its pleasing color also finds use...
Journal Articles
Alloy Digest (1981) 30 (2): Cu-411.
Published: 01 February 1981
... clamps, kick plates, studs, bolts and screws. And for more rigorous service, this alloy is employed in the fabrication of primer caps, small arms cartridge cases and bullet jackets. Manufacturer: Anaconda Brass Division Anaconda Industries Division of The Anaconda Company Waterbury, Connecticut 06720. ...
Journal Articles
Alloy Digest (2002) 51 (10): Cu-690.
Published: 01 October 2002
...) and strip width is from 3 mm (0.118 in.) with a minimum of 10 times the strip thickness. Strip and sheet are supplied with a protective coating. Applications: Typical applications include coins, medals, tokens, bullet jackets, shells, fuse caps and primers, emblems, jewelry plaques, base for gold plate...