Journal Articles
Alloy Digest (1981) 30 (6): TS-384.
Published: 01 June 1981
... be austenitized, air cooled and tempered to very high hardness (as high as Rockwell C 65). Its numerous applications include brick-mold liners, knives, liners for sand and shot blasting machines, ceramic-tile liners, punches and hand tools. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1981) 30 (12): TS-392.
Published: 01 December 1981
... Type A7 (CHROMEWEAR) tool steel. Its many applications include brick-mold liners, granulator knives, liners for sand slingers and extrusion punches for ceramics. This datasheet provides information on composition and hardness. It also includes information on wear resistance as well as forming, heat...
Journal Articles
Alloy Digest (1981) 30 (3): TS-378.
Published: 01 March 1981
... and tempered to very high hardness (as high as Rockwell C 65). Its many applications include dies of various types, brick mold liners, grinding-wheel molds and wear-resisting parts. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming...
Journal Articles
Alloy Digest (1969) 18 (3): TS-215.
Published: 01 March 1969
... Truwear is a high-carbon high-chromium cold work tool steel having extremely high resistance to abrasion and wear. It is recommended for deep drawing dies, brick mold liners, valve seats, master gages, etc. This datasheet provides information on composition and hardness as well as fracture...
Journal Articles
Alloy Digest (1985) 34 (4): TS-439.
Published: 01 April 1985
... where extreme abrasive wear is needed. Its many applications include briquetting dies and punches, brick mold liners, pottery, tools, broaches, meat-chopper plates and cold-extrusion dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1980) 29 (10): TS-371.
Published: 01 October 1980
... abrasive wear is needed. Its many applications include briquetting dies and punches, brick mold liners, pottery tools, broaches, meat-chopper plates and cold-extrusion dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information...
Journal Articles
Alloy Digest (2007) 56 (4): TS-645.
Published: 01 April 2007
..., and grindability is shown in Fig. 2. Applications: Typical applications include brick mold liners, sand slinger liners, shot-blasting equipment liners, extrusion tools for ceramics, powder compaction tooling, and machine tool ways. Producer: Timken Latrobe Steel A Timken Company Subsidiary Latrobe, PA 15650-0031...
Journal Articles
Alloy Digest (2014) 63 (8): TS-725.
Published: 01 August 2014
... of hard abrasive particles such as sand, shot blast media, and ceramics. Applications: Typical applications for LSS D7 tool steel include brick mold liners, briquetting dies, shot blasting equipment liners, tools for ceramic extrusion and molding, powder compaction tooling, deep drawing dies, flattening...
Journal Articles
Alloy Digest (1956) 5 (1): TS-42.
Published: 01 January 1956
..., Chromewear should be con&d to applications where machining and grinding requirements are relatively simple. Forms Available: Bars and forgings. Applications: Brick mold liners, liners for shot blasting machines and sand s!ingers, derp drawing dies, ceramic molds, extrusion dies for ceramics, knives, lathe...
Journal Articles
Alloy Digest (1958) 7 (12): CI-24.
Published: 01 December 1958
... martensire at the wesring surface under even light erosive wear conditions. Forms Available: Castings. Applications: Sand pumps, flotation impellers, sand classifier wear shoes, pug mill blades, brick mold liners, chute liners. Manufacturer: Any suitable foundry. ...
Journal Articles
Alloy Digest (1963) 12 (5): TS-133.
Published: 01 May 1963
... of its high percentage of carbon and vanadium, it possesses a multitude of hard, abrasion-resisting vanadium carbides which accounts for its un- excelled wear resistaoce. Forms Available: Billets, bars and forgings. Applications: Cold working dies, brick mold liners, shot blast liners, ceramic tile...
Journal Articles
Alloy Digest (1979) 28 (5): TS-349.
Published: 01 May 1979
...-tile liners, brick-mold liners, deep-drawing dies and lathe centers. Manufacturer: Guterl Special Steel Corporation Lockport, New York 14094. ...
Journal Articles
Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... is ample for its many applications. Forms Available: Billets, bars, plates and sheets. Applications: Stamping, blanking and deepdrawing dies, sorting gages, lamination dies, briquetting dies and punches, core pins, closure dies, slitter knives, brick-mold liners, ceramic-mold dies, burnishing tools, cold...
Journal Articles
Alloy Digest (1986) 35 (7): TS-460.
Published: 01 July 1986
... mold liners and die plates. briquetting dies. deep-drawing dies, wear-resisting parts, lamination dies. flattening rolls and ceramic tools and dies. Manufacturer: Workability: BR-4 DIE STEEL should be preheated to 1450-1550 F (788- 843°C) then slowly to 2050-2100°F (1121-l149°C) for forging. Reheat...
Journal Articles
Alloy Digest (1962) 11 (8): TS-122.
Published: 01 August 1962
... service temperatures exceed 3500F. Forms Available: Billets and bars. Applications: Draw dies, punches, lamination dies, blanking dies, brick liner molds. Manufacturer: Carpenter Steel Company Reading, Pennsylvania ...
Journal Articles
Alloy Digest (2020) 69 (9): TS-799.
Published: 01 September 2020
... for the processing of highly abrasive ceramic materials; liner plates for the brick industry and for making refractories; press tools for the pharmaceutical industry; automatic lathe guide sleeves; guide bars in centerless grinding machines; cone pulleys and rings for wire drawing machines; sandblast nozzles; tools...
Journal Articles
Alloy Digest (2020) 69 (3): TS-788.
Published: 01 March 2020
... abrasive ceramic materials, liner plates for the brick industry and for making refractories, press tools for the pharmaceutical industry, automatic lathe guide sleeves, guide bars in centerless grinding machines, cone pulleys and rings for wire drawing machines, sandblast nozzles, and tools for the powder...