Alloy Digest (2004) 53 (9): SA-138.
Published: 01 September 2004
... Durehete 900 is a high-strength steel bolting material often used in steam turbine and other power-plant applications. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on high...
Journal Articles
Alloy Digest (2005) 54 (10): SA-145.
Published: 01 October 2005
... Durehete 950 is a high-strength steel bolting material often used in steam turbine and other power plant applications. It is usually supplied in the heat treated condition. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (2016) 65 (12): SA-774.
Published: 01 December 2016
... Physical Properties: Density, 20 °C (68 °F), kg/m3 (lb/in.3) 7830 (0.282) See Table 1. Copyright © 2016, ASM International®. All rights reserved. DUREHETE® 1055 (Bolting Alloy) Filing Code: SA-774 Steel Alloy :: December 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542...
Journal Articles
Alloy Digest (1961) 10 (2): SA-111.
Published: 01 February 1961
... bolting to 105OOF operating tem- peratures. Manufacturer: General Characteristics: This steel has been developed co meet the demand for bolting materials operating at metal temperatures up to 105OoF. It has a high level of structural stability and possesses a high resistance to creep and srress relaxation...
Journal Articles
Alloy Digest (1995) 44 (7): Cu-602.
Published: 01 July 1995
... corrosion resistant high strength bolting material for the most severe duties in offshore environments and on naval vessels. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2007) 56 (7): SS-993.
Published: 01 July 2007
... SY286 is age hardenable and corrosion resistant. Because of its strength, it is often used as bolting material. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion...
Journal Articles
Alloy Digest (1995) 44 (3): Ni-479.
Published: 01 March 1995
... 8.11 8.21 8.90 8.3 8.33 Table 2 - TYPICAL ROOM-TEMPERATURE MATERIAL PROPERTIES Ultimate tensile strength 220 ksi 0.2% yield strength 190 ksi Elongation 20% Reduction in area 35% DoubIe shear strength 135 ksi Charpy V-notch impact energy 45 ft-lbs Table 3 - MINIMUM PROPERTIES - AEREX 350 BOLTS (Per SPS...
Journal Articles
Alloy Digest (1984) 33 (1): Cu-465.
Published: 01 January 1984
... AMBRALOY 610 is an aluminum bronze; nominally it contains 92% copper and 8% aluminum. It is an engineering material of medium strength and ductility and a good capacity for being hot worked or cold worked. It has excellent esistance to corrosion and an attractive gold color which makes it highly...
Journal Articles
Alloy Digest (1986) 35 (1): CS-109.
Published: 01 January 1986
... AISI 1017 is a carbon steel with a relatively low manganese content (0.30-0.60%); this contributes to relatively low hardenability in all applications and increased ductility with decreased hardness and strength in the core of carburized material and in uncarburized uses. It combines good hot and...
Journal Articles
Alloy Digest (1980) 29 (10): CS-84.
Published: 01 October 1980
... SAE 1017 is a carbon steel with a relatively low manganese content (0.30-0.60%) which contributes to relatively low hardenability in all applications and increased ductility with decreased hardness and strength in the core of carburized material and in uncarburized uses. It combines good hot and...
Journal Articles
Alloy Digest (1968) 17 (10): TS-211.
Published: 01 October 1968
... CROMO-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. It is recommended for hot shear blades, forging and bolt heading dies, punches and other types of hot work tools. This datasheet provides information on...
Journal Articles
Alloy Digest (1967) 16 (8): SA-214.
Published: 01 August 1967
... FAGERSTA K825 is a tough, shock resistant alloy steel having high tensile strength and endurance limit in the heat treated condition. It is recommended for shafts, bolts, countershafts, etc. in moderately stressed applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1968) 17 (9): SA-230.
Published: 01 September 1968
... Rycut 50 is a leaded chromium-molybdenum alloy steel having high machinability rating combined with good tensile and fatigue properties. It is recommended for gears, shafts, bolts, and other machinery parts. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2019) 68 (10): TS-777.
Published: 01 October 2019
... Cryodur 2833 is a wear-resistant water-hardening steel with resistance to overheating. Applications include cold heading dies; first and finish upsetting punches; cold stamps; dies for the manufacturing of screws, rivets, and bolts; and compression pistons. This datasheet provides information on...
Journal Articles
Alloy Digest (1968) 17 (4): SA-225.
Published: 01 April 1968
... applications such as rocket motor cases and accessories, bolts and fasteners and aircraft structural components- particularly landing gear. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1964) 13 (1): SA-159.
Published: 01 January 1964
... Algo-Loy 1317 is a high-strength low-alloy structural steel for bolted and riveted construction. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1996) 45 (4): Ni-339.
Published: 01 April 1996
... Nimonic alloy 901 is a nickel-base alloy strengthened by additions of molybdenum, titanium, and aluminum. It possesses high creep and rupture strength from 1000 to 1400 deg F. Applications include components for gas turbines, bolting, and valve stems for power applications. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (4): SS-851.
Published: 01 April 2002
... applications include turbine wheel blades, frames, housings, afterburners, and tail cone parts; fasteners; and miscellaneous hardware. This material is also finding applications in such nonaerospace fields as linear material for steel, high-temperature extrusion presses, autoclave chambers, and bolting...
Journal Articles
Alloy Digest (1981) 30 (2): SS-382.
Published: 01 February 1981
... continuous service to 1500 F and in intermittent service to 1800 F. Its many high-temperature applications include jet-engine turbine wheels and blades, bolting and afterburner parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2015) 64 (4): SS-1205.
Published: 01 April 2015
... engines and superchargers for various high-temperature components and is one of the few age-hardenable alloys used for bolting in the ASME Boiler and Pressure Vessel Code. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture...