Skip Nav Destination
Close Modal
Search Results for
boiler tube
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 155 Search Results for
boiler tube
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2005) 54 (7): SS-934.
Published: 01 July 2005
... with a creep rupture strength at 600-700 deg C (1110-1290 deg F) that is 30% higher than that of AISI TP347H. This steel tube, called TEMPALOY AA-1, is expected to be a candidate material for ultra-supercritical boilers. This datasheet provides information on composition and tensile properties as well as creep...
Abstract
View article
PDF
In the late 1990s boilers were designed for higher temperatures and pressures than those in the past and required steels with high-temperature strength that is greater than that of conventional 18-8 austenitic stainless steels. A heat-resisting steel (0.1C-18Cr-10Ni-3Cu-Ti-Nb) was developed with a creep rupture strength at 600-700 deg C (1110-1290 deg F) that is 30% higher than that of AISI TP347H. This steel tube, called TEMPALOY AA-1, is expected to be a candidate material for ultra-supercritical boilers. This datasheet provides information on composition and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: SS-934. Producer or source: Tenaris NKKTubes.
Journal Articles
Alloy Digest (2014) 63 (6): SS-1175.
Published: 01 June 2014
...-8542 www.asminternational.org Filing Code: SS-1175 Stainless Steel June 2014 Sumitomo XA704 is an advanced alloy for ultra-supercritical boilers and other high temperature applications. SUMITOMO XA704 (High Temperature Boiler Tube Alloy) SUMITOMO XA704 Chemical Composition, wt Carbon 0.10 max Silicon...
Abstract
View article
PDF
Sumitomo XA704 is an advanced alloy for ultra-supercritical boilers and other high temperature applications. This datasheet provides information on composition, and elasticity as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-1175. Producer or source: Sumitomo Metal USA Corporation.
Journal Articles
Alloy Digest (1994) 43 (12): SA-480.
Published: 01 December 1994
... HCM2S is a high strength ferritic boiler tube alloy with strength at temperature more than 50% that of the commonly used 2.25 Cr alloy. The alloy, with very low carbon, needs no preheat nor post-weld heat treatment. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
HCM2S is a high strength ferritic boiler tube alloy with strength at temperature more than 50% that of the commonly used 2.25 Cr alloy. The alloy, with very low carbon, needs no preheat nor post-weld heat treatment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SA-480. Producer or source: Sumitomo Metal USA Corporation.
Journal Articles
Alloy Digest (1996) 45 (7): SA-482.
Published: 01 July 1996
... Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys fatigue properties heat treatability joinability microstructure physical properties recovery boilers SANDVIK 3R12/4L7 tubes workability CXc$yrl~l19S ASM Imematil. AU lights mse...
Abstract
View article
PDF
Sandvik 3R12/4L7 is a composite tube consisting of type 304L stainless steel for corrosion resistance on the outside diameter and having carbon steel (A210 Gr. A1) as the inside component for both water wetted service and the design load. The major application is tubing to handle the corrosive conditions in black liquor recovery boilers. This datasheet provides information on composition, physical properties, microstructure as well as fatigue. It also includes information on forming, heat treating, and joining. Filing Code: SA-482. Producer or source: Sandvik.
Journal Articles
Alloy Digest (2009) 58 (10): Ni-673.
Published: 01 October 2009
... Sandvik Sanicro 67 is a composite tube for various boiler applications. The outer tube layer is of Sanicro 67, an austenitic nickel-base alloy with excellent corrosion and stress-corrosion cracking resistance. This datasheet provides information on composition and physical properties. It also...
Abstract
View article
PDF
Sandvik Sanicro 67 is a composite tube for various boiler applications. The outer tube layer is of Sanicro 67, an austenitic nickel-base alloy with excellent corrosion and stress-corrosion cracking resistance. This datasheet provides information on composition and physical properties. It also includes information on forming and joining. Filing Code: Ni-673. Producer or source: Sandvik Steel Company and Sandvik AB.
Journal Articles
Alloy Digest (2011) 60 (11): Ni-692.
Published: 01 November 2011
... DMV 617 Modified is a superheater boiler tubing grade with strength and corrosion resistance for ultra supercritical boilers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes...
Abstract
View article
PDF
DMV 617 Modified is a superheater boiler tubing grade with strength and corrosion resistance for ultra supercritical boilers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-692. Producer or source: Salzgitter Mannesmann Stainless Tubes USA Inc..
Journal Articles
Alloy Digest (2001) 50 (2): SA-508.
Published: 01 February 2001
... Vallourec and Mannesmann Tubes alloy T24 is a development in power-plant boiler-tubing alloys. It was developed to resist increasing operating parameters of pressure and temperature, particularly in ultra-super-critical boilers. This datasheet provides information on composition, physical...
Abstract
View article
PDF
Vallourec and Mannesmann Tubes alloy T24 is a development in power-plant boiler-tubing alloys. It was developed to resist increasing operating parameters of pressure and temperature, particularly in ultra-super-critical boilers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SA-508. Producer or source: Vallourec & Mannesmann.
Journal Articles
Alloy Digest (1993) 42 (8): SA-467.
Published: 01 August 1993
... NF616, nominally 9Cr-0.5 Mo-1.8W-Cb(Nb)-V, is an alloy in the 9 Cr system developed to overcome the disadvantages of high expansion with austenitic alloys for boiler operations, while maintaining high strength. NF 616 is expected to find use in boiler tubing and main steam piping. This datasheet...
Abstract
View article
PDF
NF616, nominally 9Cr-0.5 Mo-1.8W-Cb(Nb)-V, is an alloy in the 9 Cr system developed to overcome the disadvantages of high expansion with austenitic alloys for boiler operations, while maintaining high strength. NF 616 is expected to find use in boiler tubing and main steam piping. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SA-467. Producer or source: Nippon Steel Corporation.
Journal Articles
Alloy Digest (2014) 63 (8): Ni-716.
Published: 01 August 2014
... Alloy 740H (see Alloy Digest Ni-613, September 2003) is a precipitation-hardenable Ni-Cr-Co alloy containing molybdenum and niobium. The primary application for the alloy is boiler tubes for advanced ultra-supercritical steam boilers. This data sheet covers a modification of that alloy to correct...
Abstract
View article
PDF
Alloy 740H (see Alloy Digest Ni-613, September 2003) is a precipitation-hardenable Ni-Cr-Co alloy containing molybdenum and niobium. The primary application for the alloy is boiler tubes for advanced ultra-supercritical steam boilers. This data sheet covers a modification of that alloy to correct two problems, i.e., the eta-phase formation with a loss of impact strength between 750–800 deg C (1382–1472 deg F) and to render the alloy more weldable. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-716. Producer or source: PCC Energy Group.
Journal Articles
Alloy Digest (2008) 57 (11): SS-1022.
Published: 01 November 2008
... DMV 347 HFG is produced as seamless tubing suitable as a replacement for old reheater and superheater boiler tubes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Abstract
View article
PDF
DMV 347 HFG is produced as seamless tubing suitable as a replacement for old reheater and superheater boiler tubes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1022. Producer or source: Mannesmann DMV Stainless USA Inc.
Journal Articles
Alloy Digest (2001) 50 (1): SA-507.
Published: 01 January 2001
... Vallourec and Mannesmann (V and M) Tubes T23 is a power plant boiler tubing alloy developed to resist increasing operating parameters of pressure and temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Abstract
View article
PDF
Vallourec and Mannesmann (V and M) Tubes T23 is a power plant boiler tubing alloy developed to resist increasing operating parameters of pressure and temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on forming, heat treating, and joining. Filing Code: SA-507. Producer or source: Vallourec & Mannesmann.
Journal Articles
Alloy Digest (2003) 52 (6): Ni-608.
Published: 01 June 2003
... Sulzer Metco 8500 is a nickel-chromium alloy wire for electric arc spraying. The nominal composition is Ni-45Cr, and applications are in the protection of power-plant boiler tubes. This datasheet provides information on composition, physical properties, and microstructure. It also includes...
Abstract
View article
PDF
Sulzer Metco 8500 is a nickel-chromium alloy wire for electric arc spraying. The nominal composition is Ni-45Cr, and applications are in the protection of power-plant boiler tubes. This datasheet provides information on composition, physical properties, and microstructure. It also includes information on machining, joining, and surface treatment. Filing Code: Ni-608. Producer or source: Sulzer Metco.
Journal Articles
Alloy Digest (2003) 52 (9): Ni-613.
Published: 01 September 2003
... Alloy 740 is a precipitation-hardenable Ni-Cr-Co alloy containing molybdenum and niobium. The primary application for the alloy is boiler tubes for the European advanced electricity generation program (Thermie). This datasheet provides information on composition, physical properties, elasticity...
Abstract
View article
PDF
Alloy 740 is a precipitation-hardenable Ni-Cr-Co alloy containing molybdenum and niobium. The primary application for the alloy is boiler tubes for the European advanced electricity generation program (Thermie). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-613. Producer or source: Special Metals Corporation.
Journal Articles
Alloy Digest (2002) 51 (12): Ni-597.
Published: 01 December 2002
... cladding of the INCO- CLAD tubes is the same as that of conventional alloy 625 tubes and is specified by ASTM B 444, UNS N06625. The grade and composition of the steel substrate are dependent on the steel specified. Some of the common boiler steel grades used for the tube core are ASTM A 210 grade A-1...
Abstract
View article
PDF
INCOCLAD625/Steel is a bimetallic clad tube with alloy 625 (UNS N06625) on the outside and with a metallurgical bond holding the alloys together. This datasheet provides information on composition. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ni-597. Producer or source: Special Metals Corporation.
Journal Articles
Alloy Digest (2001) 50 (9): SS-831.
Published: 01 September 2001
... NOx firing. For example, the material is used in waterwalls, evaporators such as municipal refuse, black liquor recovery and coal fired boilers, copper flash smelting, and coal gasification syngas waste heat boilers. Specification Equivalents: Sandvik tube specification 7-1-0009 or 7-1-1169 ASME Code...
Abstract
View article
PDF
Sandvik Sanicro 28 composite tube is used in services as superheater material for waste-derived fuel plants. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-831. Producer or source: Sandvik Steel Company. See also Alloy Digest SS-442, March 1984.
Journal Articles
Alloy Digest (2001) 50 (8): Ni-572.
Published: 01 August 2001
... on the load-carrying inner component, which is a normal boiler-tube material (see below). The clad- ding, which typically is considered only as a corrosion protection, will, in practice, add significant strength to the tube. Typical Inner Components consist of normal boiler tube materials such as Sandvik 4L7...
Abstract
View article
PDF
Sandvik Sanicro 63 was developed specifically for use as outer cladding of composite tubes in service as superheater materials for waste-derived fuel plants. It is a modification of UNS N06625. Typical inner components of the composite tubes are Sandvik 4L7 and Sandvik HT8. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming and joining. Filing Code: Ni-572. Producer or source: Sandvik.
Journal Articles
Alloy Digest (2020) 69 (9): Ni-762.
Published: 01 September 2020
... Forms Bars, seamless pipes and tubes Applications Advanced ultra-supercritical (A-USC) boiler tubes, header pipes, and seamless steam reheat piping Supplier Special Metals Corporation 4317 Middle Settlement Road New Hartford, New York 13413, USA Tel: +1 315 798 2900 Web: www.specialmetals.com...
Abstract
View article
PDF
Special Metals Inconel 740H (UNS N07740) is a precipitation hardenable, nickel-base superalloy that offers a unique combination of high strength and creep resistance at elevated temperatures along with resistance to coal ash corrosion. This alloy was originally targeted for use in advanced ultra-supercritical (A-USC) power plants. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-762. Producer or source: Special Metals Corporation.
Journal Articles
Alloy Digest (2008) 57 (10): SS-1019.
Published: 01 October 2008
.... Specification Equivalents: 1.4907 X 10CrNiCuNb 18 9 3 To VDTÜV data sheet 550, 09.2003 ASME Boiler & Pressure Vessel Code Case 2328-1 General Characteristics: DMV 304HCu has been designed for application as superheater and reheater boiler tube grade, 304HCu has proved to be suitable in most advanced coal-fired...
Abstract
View article
PDF
DMV 304 HCu is produced as seamless tubing and designed for application as superheaters. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1019. Producer or source: Mannesmann DMV Stainless USA Inc.
Journal Articles
Alloy Digest (2014) 63 (10): Ni-718.
Published: 01 October 2014
... corrosion and stress corrosion cracking due to optimized Ni, Mo, N, and extra low C content Applicable as mono-wall tube and outer component of composite tube Enough formability and weldability for boiler tube applications due to good phase stability Fig. 2 Creep rupture test results of welded joints...
Abstract
View article
PDF
Sumitomo HR11N is a high temperature nickel alloy with a high chromium content to provide excellent corrosion and oxidation resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: Ni-718. Producer or source: Sumitomo Metal USA Corporation.
Journal Articles
Alloy Digest (2001) 50 (3): SA-509.
Published: 01 March 2001
... V and M T/P92 is a ferritic alloy with improved high-temperature strength and creep behaviors compared to those of other ferritic steel alloys. Applications include both superheater tubes and main steam piping in advanced boilers. This datasheet provides information on composition, physical...
Abstract
View article
PDF
V and M T/P92 is a ferritic alloy with improved high-temperature strength and creep behaviors compared to those of other ferritic steel alloys. Applications include both superheater tubes and main steam piping in advanced boilers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-509. Producer or source: Vallourec & Mannesmann Tubes Corporation.