Alloy Digest (2009) 58 (10): Ni-673.
Published: 01 October 2009
... Sandvik Sanicro 67 is a composite tube for various boiler applications. The outer tube layer is of Sanicro 67, an austenitic nickel-base alloy with excellent corrosion and stress-corrosion cracking resistance. This datasheet provides information on composition and physical properties. It also...
Journal Articles
Alloy Digest (2006) 55 (8): SS-971.
Published: 01 August 2006
... Sandvik Esshete 1250 is a fully austenitic chromium-nickel steel with excellent high-temperature strength and good resistance to corrosion in boiler applications. The material is easily fabricated. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (2014) 63 (8): Ni-716.
Published: 01 August 2014
... Alloy 740H (see Alloy Digest Ni-613, September 2003) is a precipitation-hardenable Ni-Cr-Co alloy containing molybdenum and niobium. The primary application for the alloy is boiler tubes for advanced ultra-supercritical steam boilers. This data sheet covers a modification of that alloy to correct...
Journal Articles
Alloy Digest (2003) 52 (6): Ni-608.
Published: 01 June 2003
... Sulzer Metco 8500 is a nickel-chromium alloy wire for electric arc spraying. The nominal composition is Ni-45Cr, and applications are in the protection of power-plant boiler tubes. This datasheet provides information on composition, physical properties, and microstructure. It also includes...
Journal Articles
Alloy Digest (1993) 42 (8): SA-467.
Published: 01 August 1993
... the producer. General Characteristics: NF 616 has recently been developed in Japan for boiler applications. This steel has much higher creep-rupture strength than other ferritic steels, including T91, owing to solid solution hardening by tungsten and precipitation 400 CT g 300 9 I 200 3 E P a 3 100 0 NF616 191...
Journal Articles
Alloy Digest (2005) 54 (8): SA-550.
Published: 01 August 2005
... to economizer tubes and gas-gas heat exchanger tubes for power boilers. Therefore, S-TEN1 tubes have been standardized in the MET1 (The Minister of Economy, Trade and Industry, Japan) Code as Ka-STB380J1 for tubes and Ka-STPT380J1 for pipes and used in sever- al power boilers. Applications are underway for ASTM...
Journal Articles
Alloy Digest (2001) 50 (3): SA-509.
Published: 01 March 2001
... V and M T/P92 is a ferritic alloy with improved high-temperature strength and creep behaviors compared to those of other ferritic steel alloys. Applications include both superheater tubes and main steam piping in advanced boilers. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2003) 52 (9): Ni-613.
Published: 01 September 2003
... Alloy 740 is a precipitation-hardenable Ni-Cr-Co alloy containing molybdenum and niobium. The primary application for the alloy is boiler tubes for the European advanced electricity generation program (Thermie). This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1998) 47 (3): SS-710.
Published: 01 March 1998
... Allloy AC 66 is a high temperature austenitic steel with alloying additions to improve oxidation resistance and alloying limitations to improve internal oxidation. Typical applications are waste handling to energy boilers and coal gasification plants. This datasheet provides information...
Journal Articles
Alloy Digest (1998) 47 (11): SS-730.
Published: 01 November 1998
... and 899 C (800 and 1650 F). It is nonmagnetic in the annealed condition but is slightly magnetic in the cold-worked condition. Among its many applications are aircraft-engine exhaust manifolds, boiler shells, and high-temperature handling equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2014) 63 (6): SS-1175.
Published: 01 June 2014
... Sumitomo XA704 is an advanced alloy for ultra-supercritical boilers and other high temperature applications. This datasheet provides information on composition, and elasticity as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2010) 59 (3): SS-1059.
Published: 01 March 2010
... With excellent resistance to sulfuric acid dew-point corrosion, NAS 155N (UNS S31727) is a stainless steel custom made for the heat exchangers, flues, and chimneys of heavy oil-fired boilers. This alloy is suitable in a wide range of material applications for antipollution equipment and other...
Journal Articles
Alloy Digest (1996) 45 (7): SA-482.
Published: 01 July 1996
... 304L stainless steel for corrosion resistance on the outside diameter and having carbon steel (A210 Gr. Al) as the inside component for both water wetted service and the design load. The major application is tubing to handle the corrosive conditions in black liquor recovery boilers. Sandvik...
Journal Articles
Alloy Digest (1983) 32 (12): SS-436.
Published: 01 December 1983
... austenitic chromium-nickel steel that IS particularly adaptable for use at temperatures between 800and 1650 F. It is non-magnetic in the annealed condition but is slightly magnetic in the cold-worked condition. Among its many applications are aircrafttngine exhaust manifolds. boiler shells and high...
Journal Articles
Alloy Digest (1984) 33 (3): SS-441.
Published: 01 March 1984
... and structures can be fabricated easily and it can be machined readily. It can be welded easily and gives strong, ductile welds. Some of its many applications are annealing boxes, boiler baffles, dryers, furnace parts, heat exchangers and oil-refining equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-459.
Published: 01 August 1994
... and higher AWE boiler and pressure-vessel design stress allowables than C800 H. The alloy resists stress-corrosion cracking, resists sulfur attack, internal oxidation, scaling and corrosion in thermal processing and heat-transfer applications. The strength is obtained by a selective chemistry range within...
Journal Articles
Alloy Digest (2001) 50 (2): SA-508.
Published: 01 February 2001
.... These properties open additional perspectives in applications for super- heaters of new conventional boilers as well as for repair jobs in old boilers. The steel grade is an effective candidate to replace T22. Beyond that, the material could also be of interest as piping material. High creep strengths...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-597.
Published: 01 December 2002
.... Applications: INCOCLAD alloy 625/Steel bimetallic clad tubes are designed for service as boiler tubes for steam generation and heating in municipal solid waste (MSW) fired boilers in waste-to-energy (WTE) incineration systems. Boiler tubes in these environments are exposed to corrosion by halogens...
Journal Articles
Alloy Digest (2011) 60 (11): Ni-692.
Published: 01 November 2011
... outer diameter is 150 mm (6 in.) and the maximum wall thickness is 17 mm (0.7 in Other sizes are available upon request. Applications: Designed for application as superheater and reheater boiler tubing. This alloy is suitable for the most advanced coal fired power stations using steam temperatures...
Journal Articles
Alloy Digest (2005) 54 (7): SS-934.
Published: 01 July 2005
... In the late 1990s boilers were designed for higher temperatures and pressures than those in the past and required steels with high-temperature strength that is greater than that of conventional 18-8 austenitic stainless steels. A heat-resisting steel (0.1C-18Cr-10Ni-3Cu-Ti-Nb) was developed...