Alloy Digest (1976) 25 (3): SS-326.
Published: 01 March 1976
... AQUAMET 17 is a precipitation-hardening stainless steel that provides the best combination of strength, toughness, wear resistance and corrosion resistance available for shafting where extra strength and precision straightness are needed. It is in wide use in various types of boats. This datasheet...
Journal Articles
Alloy Digest (1976) 25 (8): SS-332.
Published: 01 August 1976
... AQUAMET 18 is a low-nickel austenitic stainless steel having seawater corrosion resistance better than AISI Type 304 and approaching that of AISI Type 316 stainless steel. Its good strength and super toughness make it an ideal material for pleasure and work boats. This datasheet provides...
Journal Articles
Alloy Digest (1977) 26 (4): SS-338.
Published: 01 April 1977
... AQUAMET 22 is an austenitic stainless steel with an outstanding combination of strength, toughness and corrosion resistance. Its corrosion resistance is equal to or better than any other boat shafting material, even better than most high-nickel alloys. It is the best material available...
Journal Articles
Alloy Digest (1981) 30 (12): Al-28.
Published: 01 December 1981
... ALUMINUM 5086 is a non-heat-treatable aluminum alloy. It is characterized by high strength, excellent weldability and excellent resistance to corrosion. Among its many uses are structural towers, welded boat hulls, tanks and pipe lines. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2021) 70 (11): Mo-21.
Published: 01 November 2021
..., wt% loads, such as furnace rails, sintering boats, annealing boats, 99.30 99.70 trays, grids, and racks, and similar items. Element 0.3 0.7 Molybdenum Machining Lanthanum Oxide (La2O3) Molybdenum and molybdenum alloys can be machined by Physical Properties all of the common metal machining processes...
Journal Articles
Alloy Digest (2009) 58 (2): Cu-766.
Published: 01 February 2009
... resistance to all types of water, saline fogs, and a wide variety of other corrosives. C65100 hull and deck fastenings are the standard materials with yacht designers and the majority of builders of stock power boats. The alloy is also used for cable connectors, mast tangs, deck and pilot house hardware...
Journal Articles
Alloy Digest (1991) 40 (11): Cer-7.
Published: 01 November 1991
..., use an abrasive cut-off wheel. Use soft jaws and light clamping pressure in hold- ing the work for machining. Boats. crucibles, plates, nuts, round and rectangular rod, screws, tapered pins, tubing and wafers can normally be manufactured to customer order. Some general maximum size limitations...
Journal Articles
Alloy Digest (2023) 72 (2): Al-494.
Published: 01 February 2023
... alkaline conditions. The resistance of Austral Wright 5251 to corrosion in marine atmospheres is excellent, exceeding that of alloy 5005. Hence, the frequent use of Austral Wright 5251 in marine applications such as small boats and dinghies. The corrosion resistance of aluminum alloys relies...
Journal Articles
Alloy Digest (2022) 71 (10): SS-1352.
Published: 01 October 2022
... in aerospace and chemical plant applications, and boat propeller shafts. It is also available as investment castings for applications such as boat fittings. Supplier Austral Wright Metals 133 139 Cowpasture Road Wetherill Park, New South Wales 2164, Australia Tel: +61 02 9827 0790 Web: www.australwright.com.au...
Journal Articles
Alloy Digest (2003) 52 (1): SS-870.
Published: 01 January 2003
... to that of Type 316 stainless steel. Product Forms Available: The alloy is supplied as semifinished or fully machined compo- nents up to 35 ft in length. Applications: Typical applications are nonmagnetic drill string components, marine engineering applications, fasteners, pump and valve parts, boat shafting...
Journal Articles
Alloy Digest (1960) 9 (4): Al-90.
Published: 01 April 1960
... Shipbuilding, structural parts where good strength and hardens rapidly, becoming extremely tough. It was corrosion resistance are required, welded boat hulls, developed qecially to meet the need for high strength guided missile containers, trusses, girders, truck and trailer frames. non-h& treatable alloy...
Journal Articles
Alloy Digest (1991) 40 (11): P-31.
Published: 01 November 1991
... applicable to thermosetting products. It has excellent thermal and electrical insulation properties and is resistant to corrosion in a wide variety of chemical environments. Applications: Reinforced DERAKANE 8084 vinyl ester resin is used in plastic boats and other recreational equipment, as well as a wide...
Journal Articles
Alloy Digest (2019) 68 (12): SA-857.
Published: 01 December 2019
... for jack-up rigs and lift boats in offshore applications. Producer Voestalpine Grobblech GmbH 4020 Linz, Austria Tele: +43/50304/15-9440 www.voestalpine.com ISSN: 002-614X SA-857B ...
Journal Articles
Alloy Digest (1972) 21 (2): Zn-13.
Published: 01 February 1972
...; radio and television shielding cans; radio brackets; handles; terminals; jewelry; decorative trim for auto- mobiles; boats; appliances; automotive spring liners; roofing, flashing, and roof-drainage goods; building accessories such as regelets, cavity wall ties, louvers, etc.; decorative...
Journal Articles
Alloy Digest (2020) 69 (9): Mo-19.
Published: 01 September 2020
... in electronic tubes; radiation sheets in high-temperature furnace construction; resistance welding electrodes/discs for copper and brass; sintering boats. Supplier Wieland Duro GmbH Albert-Einstein-Str. 1 70806 Kornwestheim, Germany Tel: +49 7154 8255 0 Web: www.wieland-duro.com ISSN: 002-614X Mo-19B ...
Journal Articles
Alloy Digest (1957) 6 (4): SA-56.
Published: 01 April 1957
..., flat rolled stock. Applications: Light weight construction, buses, trucks, railroad cars, portable and stationary structures, ovens, smoke stacks, mine cars, autos, hulls of boats and barges, tanks, loading skids, road paving machinery. Manufacturer: Alan Wood Steel Company Conshohocken, Pennsylvania ...
Journal Articles
Alloy Digest (1961) 10 (5): SA-115.
Published: 01 May 1961
..., barges, materials handling equipment, construction equipment, military equipment, structural applications, tanks, mine cars, hulls of boats, road paving equipment. Manufacturer: Armco Steel Corporation Middletown, Ohio ...
Journal Articles
Alloy Digest (1997) 46 (5): SS-680.
Published: 01 May 1997
... edge, a sheared edge or a plasmaat edge. Duracotr hot-roiled sheet and CIvlP are available with a mill edge or a No. 3 slit edge. ASTM A480 specification and tolerances apply. Applications: Boat docks, cement plant equipment, coal cars. coal-hand.ling equipment, drain covers, fertilizr-handling...
Journal Articles
Alloy Digest (1988) 37 (4): Mo-13.
Published: 01 April 1988
... equipment such as reflective heat shields, boats, trays, skids and racks; electrical heating or heat-booster electrodes in continuous glass making operations (container and fiber production); miscellaneous electronic components; crystal growing devices. Manufacturer: Amax Specialty Metals Corp. Cleveland...
Journal Articles
Alloy Digest (2019) 68 (8): SA-850.
Published: 01 August 2019
..., in mining equipment, and pressure piping. Also supplied are hot-formed chords for jack-up rigs and lift boats in offshore applications. Producer Voestalpine Grobblech GmbH 4020 Linz, Austria Tel: +43-50304-15-9440 www.voestalpine.com ISSN: 002-614X SA-850B Table 1 Mechanical properties Thickness, mm...