... YSS YXR7 is a high-speed tool steel with good toughness and wear resistance. It is used for blanking dies, forging dies, heading dies, and thread forming dies. This datasheet provides information on composition, physical properties, hardness, and bend strength. It also includes information on heat...
Journal Articles
Alloy Digest (1986) 35 (11): TS-465.
Published: 01 November 1986
...-work applications. Another feature of this versatile die steel is its outstanding secondary hardness associated with remarkable tempering resistance up to 900 F. Typical applications comprise blanking dies, swaging dies, hot and cold-piercing punches, forming rolls, shear blades and coining dies...
Journal Articles
Alloy Digest (1977) 26 (7): TS-320.
Published: 01 July 1977
..., punches and blanking dies. This datasheet provides information on composition, physical properties, elasticity, and compressive strength as well as fracture toughness. It also includes information on wear resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-320...
Journal Articles
Alloy Digest (1985) 34 (2): TS-435.
Published: 01 February 1985
... excellent non-deforming characteristics. It is well suited for applications requiring toughness and fairly high resistance to abrasion. Typical applications for AIRKOOL include blanking dies, forming dies, punches and shear blades. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1981) 30 (8): TS-385.
Published: 01 August 1981
... many applications include blanking dies, coining, cold shears and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-385. Producer or source: Jessop Steel...
Journal Articles
Alloy Digest (1981) 30 (9): TS-386.
Published: 01 September 1981
... are blanking dies, cold-forming dies, punches and cold and hot shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-386. Producer or source...
Journal Articles
Alloy Digest (1982) 31 (9): TS-404.
Published: 01 September 1982
... for a wide range of cold-working tools such as broaches, blanking dies, punches, thread-rolling dies, paper knives and wood-working tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining...
Journal Articles
Alloy Digest (2019) 68 (8): TS-773.
Published: 01 August 2019
... YSS HAP10 is a powder metallurgy high-speed tool steel with very high toughness for cold forging dies and fine blanking dies. This datasheet provides information on composition, physical properties, and hardness. It also includes information on wear resistance as well as heat treating. Filing Code...
Journal Articles
Alloy Digest (1987) 36 (10): TS-482.
Published: 01 October 1987
... strength and long runs between grinds are necessary. Among its many applications are blanking dies, burnishing tools, beading rolls, lathe centers, plug gages, spinning tools, slitters and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also...
Journal Articles
Alloy Digest (1969) 18 (8): TS-222.
Published: 01 August 1969
... VAN LOM is a molybdenum type high-speed steel having excellent wear and cutting properties. It is recommended for cutting tools, punches, shear blades, blanking dies, etc. where improved toughness is desired. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1963) 12 (4): TS-132.
Published: 01 April 1963
... HYCC is a high-carbon high-chromium tool steel having high wear and abrasion resistance combined with non-deforming characteristics. It is particularly adaptable for blanking dies and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity...
Journal Articles
Alloy Digest (1966) 15 (1): TS-174.
Published: 01 January 1966
... BOFORS RT-1733 is an oil hardening, non-deforming tool and die steel. It has a good combination of toughness, wear and abrasion resistance. It is recommended for punches, forming rolls, master tools, blanking dies and cutters. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1979) 28 (5): TS-348.
Published: 01 May 1979
... Slag Remelted) high-speed steel. Its many uses include blanking dies, drills, lathe tools, punches and shearing blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface...
Journal Articles
Alloy Digest (1979) 28 (7): TS-351.
Published: 01 July 1979
... practical use in the field of cutting tools. Its many uses include drills, milling cutters, lathe tools, blanking dies and special shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1980) 29 (12): TS-374.
Published: 01 December 1980
... for fine-edged tools and for tools that must be ground with sharp angles where danger of edge crumbling or chipping is pronounced. Typical applications comprise blanking dies, drills, milling cutters and punches. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1983) 32 (2): TS-411.
Published: 01 February 1983
... structure, and is unusually tough. Its many applications include blanking dies, master tools, milling and form cutters, paper knives, punches and taps. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
... applications. Among its many uses are blanking dies, shear blades, punches and chisels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating...
Journal Articles
Alloy Digest (1984) 33 (11): TS-432.
Published: 01 November 1984
... REX TMO molybdenum-tungsten high-speed steel is a tough, general-purpose high-speed steel with high cutting efficiency and excellent finishing properties. It is adapted to fast light cuts on soft or medium hard materials. Among its many applications are blanking dies, twist drills, circular saws...
Journal Articles
Alloy Digest (1969) 18 (6): TS-220.
Published: 01 June 1969
... AISI Type A10 is a high-carbon graphitic tool steel capable of developing high hardness and wear resistance. It is recommended for shear blades, blanking and forming dies, drawing dies and wear plates. This datasheet provides information on composition and hardness as well as fracture toughness...
Journal Articles
Alloy Digest (1968) 17 (5): TS-205.
Published: 01 May 1968
... Double Six Super is a high-carbon high-chromium air hardening tool steel having excellent non-deforming characteristics. It is recommended for blanking and thread rolling dies, drawing and coining dies, gauges and mandrels. This datasheet provides information on composition, hardness, tensile...