Skip Nav Destination
Close Modal
Search Results for
blades
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 829 Search Results for
blades
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1993) 42 (1): Ni-420.
Published: 01 January 1993
... CMSX-3@ Nickel Alloy - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JANUARY 1993 ~lnn3.AlbyD@St.kM@h!S-. Pabhadby: AbyDipm,IncI201%?7%161 gg 27 Canlid Stmet Ofan~% NJ. 07050 I U.SA CMSX-3@ (Single Crystal TurtMe Blade Alloy) CM!SX-3 is a pqrietary single crystal alloy development of Cannon-Muskegon...
Abstract
View article
PDF
CMSX-3 is a single crystal alloy development of Cannon-Muskegon Corporation designed to achieve a balance in properties at high temperatures. This datasheet provides information on composition and physical properties as well as creep. It also includes information on corrosion resistance. Filing Code: Ni-420. Producer or source: Cannon-Muskegon Corporation.
Journal Articles
Alloy Digest (1992) 41 (10): Ni-415.
Published: 01 October 1992
... CM 247 LC alloy is a derivative of the MAR M 247 composition, specifically designed for directionally solidified (DS) turbine blade and vane applications. This datasheet provides information on composition and physical properties. It also includes information on casting and heat treating. Filing...
Abstract
View article
PDF
CM 247 LC alloy is a derivative of the MAR M 247 composition, specifically designed for directionally solidified (DS) turbine blade and vane applications. This datasheet provides information on composition and physical properties. It also includes information on casting and heat treating. Filing Code: Ni-415. Producer or source: Cannon-Muskegon Corporation.
Journal Articles
Alloy Digest (1992) 41 (12): Ni-418.
Published: 01 December 1992
... -ah1 1992. Alloy Digsst inc. All riqhfs rclbewed PMMby: Ailoy Di9-W. Inc 1201677-9161 Dalashowllam~,norrobelJs6dlof 27 Canliild SlreeI. Orange. NJ. 07060 I U.S.A s&xdkaltiorlmal~ign. CMSX-6@ (Low Density Single Crystal Nickel-Base Turbine Blade Alloy) CMSX-6 is a proprietaq low density, single crystal...
Abstract
View article
PDF
CMSX-6 is a low density, single crystal alloy development to retrofit existing turbine designs. This datasheet provides information on composition and physical properties as well as creep. It also includes information on casting. Filing Code: Ni-418. Producer or source: Cannon-Muskegon Corporation.
Journal Articles
Alloy Digest (2007) 56 (1): SA-559.
Published: 01 January 2007
... Boehler T552 Extra is a hardened and tempered steel with a combination of properties for stressed turbine blades. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on high...
Abstract
View article
PDF
Boehler T552 Extra is a hardened and tempered steel with a combination of properties for stressed turbine blades. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: SA-559. Producer or source: Böhler-Uddeholm North America.
Journal Articles
Alloy Digest (2007) 56 (2): SS-987.
Published: 01 February 2007
.... BOEHLER M314 EXTRA Filing Code: SS-987 Stainless Steel February 2007 BOEHLER M314 EXTRA (Tempered Turbine Blade Steel) Böhler M314 Extra is free machining with high sulfur, prehardened, and corrosion resistant with 16% Cr. It is used as holder frames for plastic mold tooling. Hardening. The tool must...
Abstract
View article
PDF
Böhler M314 Extra is free machining with high sulfur, prehardened, and corrosion resistant with 16% Cr. It is used as holder frames for plastic mold tooling. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: SS-987. Producer or source: Böhler-Uddeholm North America.
Journal Articles
Alloy Digest (1962) 11 (9): TS-124.
Published: 01 September 1962
... DOUBLE SEVEN is an air hardening high-carbon high-chromium tool and die steel having high hardness and wear resistance. It is recommended for shear blades, cold working tools, and heavy duty dies. This datasheet provides information on composition, physical properties, hardness, and elasticity...
Abstract
View article
PDF
DOUBLE SEVEN is an air hardening high-carbon high-chromium tool and die steel having high hardness and wear resistance. It is recommended for shear blades, cold working tools, and heavy duty dies. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-124. Producer or source: Edgar Allen & Company Ltd, Imperial Steel Works.
Journal Articles
Alloy Digest (1963) 12 (4): Ti-34.
Published: 01 April 1963
... HYLITE 40 is a titanium-aluminum-manganese alloy of high strength with excellent properties as forgings and bar stock. It is recommended for compressor dises and blades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Abstract
View article
PDF
HYLITE 40 is a titanium-aluminum-manganese alloy of high strength with excellent properties as forgings and bar stock. It is recommended for compressor dises and blades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-34. Producer or source: Jessop-Saville Ltd, Brightside Works.
Journal Articles
Alloy Digest (1964) 13 (2): Ni-88.
Published: 01 February 1964
... SM-200 is a nickel-base alloy designed primarily as a cast turbine blade material which retains useful strength up to 1900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance...
Abstract
View article
PDF
SM-200 is a nickel-base alloy designed primarily as a cast turbine blade material which retains useful strength up to 1900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Ni-88. Producer or source: Martin Metals Company.
Journal Articles
Alloy Digest (1964) 13 (6): Co-37.
Published: 01 June 1964
... Nivco 10 is a cobalt-base turbine alloy having a combination of high damping capacity, high strength and high ductility. It is a precipitation hardening alloy recommended for use at temperatures up to 1200 F, such as turbine blades. This datasheet provides information on composition, physical...
Abstract
View article
PDF
Nivco 10 is a cobalt-base turbine alloy having a combination of high damping capacity, high strength and high ductility. It is a precipitation hardening alloy recommended for use at temperatures up to 1200 F, such as turbine blades. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Co-37. Producer or source: Westinghouse Electric Corporation.
Journal Articles
Alloy Digest (1964) 13 (7): Co-38.
Published: 01 July 1964
... SM322 is a cobalt-base casting alloy characterized by exceptional high temperature strength, good ductility, and oxidation resistance throughout its operating range of 1400-2000 F. It is recommended for turbine vanes and blades. This datasheet provides information on composition, physical...
Abstract
View article
PDF
SM322 is a cobalt-base casting alloy characterized by exceptional high temperature strength, good ductility, and oxidation resistance throughout its operating range of 1400-2000 F. It is recommended for turbine vanes and blades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Co-38. Producer or source: Martin Metals Division, Martin Marietta Corporation.
Journal Articles
Alloy Digest (1964) 13 (11): Ni-95.
Published: 01 November 1964
... Udimet N-115 is a vacuum-induction melted nickel-base alloy that responds to precipitation hardening. It is a superalloy for extended service to 1850 F. It has been thus far limited to barstock for turbine blading applications and may be suitable for existing or future large forging applications...
Abstract
View article
PDF
Udimet N-115 is a vacuum-induction melted nickel-base alloy that responds to precipitation hardening. It is a superalloy for extended service to 1850 F. It has been thus far limited to barstock for turbine blading applications and may be suitable for existing or future large forging applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-95. Producer or source: Special Metals Inc..
Journal Articles
Alloy Digest (1965) 14 (3): SS-166.
Published: 01 March 1965
... F.V.520B is an improved martensitic stainless steel which has good corrosion resistance, weldability, and capacity of being hardened by low temperature heat treatment. It is recommended for steam turbine blades and aircraft components. This datasheet provides information on composition, physical...
Abstract
View article
PDF
F.V.520B is an improved martensitic stainless steel which has good corrosion resistance, weldability, and capacity of being hardened by low temperature heat treatment. It is recommended for steam turbine blades and aircraft components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-166. Producer or source: Firth-Vickers Stainless Steels Ltd.
Journal Articles
Alloy Digest (1965) 14 (5): Co-44.
Published: 01 May 1965
... Deloro-Stellite-7 is a cobalt base casting alloy possessing excellent corrosion resistance and high temperature strength together with good ductility and excellent resistance to thermal shock. It is recommended for gas turbine blades, brass casting dies and extrusion dies. This datasheet provides...
Abstract
View article
PDF
Deloro-Stellite-7 is a cobalt base casting alloy possessing excellent corrosion resistance and high temperature strength together with good ductility and excellent resistance to thermal shock. It is recommended for gas turbine blades, brass casting dies and extrusion dies. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Co-44. Producer or source: Deloro Stellite Ltd.
Journal Articles
Alloy Digest (1965) 14 (7): Co-45.
Published: 01 July 1965
... MAR-M Alloy 322 is a cobalt-base casting alloy characterized by exceptional high temperature strength, good ductility, and oxidation resistance throughout its operating range of 1400-2000 F. It is recommended for turbine vanes and blades. This datasheet provides information on composition...
Abstract
View article
PDF
MAR-M Alloy 322 is a cobalt-base casting alloy characterized by exceptional high temperature strength, good ductility, and oxidation resistance throughout its operating range of 1400-2000 F. It is recommended for turbine vanes and blades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, and machining. Filing Code: Co-45. Producer or source: Martin Metals Division, Martin Marietta Corporation.
Journal Articles
Alloy Digest (1965) 14 (11): Ni-107.
Published: 01 November 1965
... MAR-M Alloy 200 is a nickel-base alloy designed primarily as a cast turbine blade material which retains useful strength up to 1900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature...
Abstract
View article
PDF
MAR-M Alloy 200 is a nickel-base alloy designed primarily as a cast turbine blade material which retains useful strength up to 1900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as heat treating and joining. Filing Code: Ni-107. Producer or source: Martin Metals Company.
Journal Articles
Alloy Digest (1965) 14 (12): SS-175.
Published: 01 December 1965
... AISI No. 615 is a hardenable chromium-nickel-tungsten martensitic corrosion resistant steel used primarily at temperatures up to 1050 F. It is used for compressor blades, vanes, discs, and other gas turbine engine components. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
AISI No. 615 is a hardenable chromium-nickel-tungsten martensitic corrosion resistant steel used primarily at temperatures up to 1050 F. It is used for compressor blades, vanes, discs, and other gas turbine engine components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-175. Producer or source: Alloy steel mills and foundries.
Journal Articles
Alloy Digest (2019) 68 (2): SS-1303.
Published: 01 February 2019
... Sandvik 13C26 Medical Strip is martensitic stainless strip steel that has very good wear resistance. One important use is surgical blades. This datasheet provides information on composition, physical properties, and hardness as well as fatigue. It also includes information on wear resistance...
Abstract
View article
PDF
Sandvik 13C26 Medical Strip is martensitic stainless strip steel that has very good wear resistance. One important use is surgical blades. This datasheet provides information on composition, physical properties, and hardness as well as fatigue. It also includes information on wear resistance as well as heat treating. Filing Code: SS-1303. Producer or source: Sandvik Steel Company.
Journal Articles
Alloy Digest (2000) 49 (1): CS-134.
Published: 01 January 2000
... SANDVIK 15N2 is strip steel for stonecutting saws and especially designed for the manufacture of diamond saw blades. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: CS-134. Producer or source: Sandvik. Producer or Source...
Abstract
View article
PDF
SANDVIK 15N2 is strip steel for stonecutting saws and especially designed for the manufacture of diamond saw blades. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: CS-134. Producer or source: Sandvik.
Journal Articles
Alloy Digest (2001) 50 (8): TS-589.
Published: 01 August 2001
... Mazeman is a cold-work die steel with a combination of toughness, wear resistance, and hardenability. Applications include shear blades, punches and die inserts. This datasheet provides information on composition, physical properties, and hardness as well as creep. It also includes information...
Abstract
View article
PDF
Mazeman is a cold-work die steel with a combination of toughness, wear resistance, and hardenability. Applications include shear blades, punches and die inserts. This datasheet provides information on composition, physical properties, and hardness as well as creep. It also includes information on high temperature performance as well as heat treating and machining. Filing Code: TS-589. Producer or source: Timken Latrobe Steel.
Journal Articles
Alloy Digest (2001) 50 (9): TS-590.
Published: 01 September 2001
... Lanark is a silicon-manganese shock resistant tool steel with highest impact strength of the AISI S type tool steels. It is used for pneumatic tools, shear blades, and mandrels. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Abstract
View article
PDF
Lanark is a silicon-manganese shock resistant tool steel with highest impact strength of the AISI S type tool steels. It is used for pneumatic tools, shear blades, and mandrels. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-590. Producer or source: Timken Latrobe Steel.