Alloy Digest (1977) 26 (8): Al-228.
Published: 01 August 1977
... BELMONT ALLOY 1918 is a general-purpose aluminum casting alloy that can be sand cast and permanent-mold cast. It is used widely for bearings and is particularly suited for heavy-duty bearings such as those used for diesel engine crankshafts. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1980) 29 (6): SA-374.
Published: 01 June 1980
... LESCALLOY 52100 VAC ARC is a deep-hardening alloy steel used in high-performance aircraft bearings and other high-load applications where premium-quality steel is required. This grade is produced by the vacuum consumable electrode melting process and offers greatly improved cleanliness...
Journal Articles
Alloy Digest (1982) 31 (9): Al-240.
Published: 01 September 1982
... ALUMINUM A850.0 is an aluminum bearing alloy containing nominally 2.5% silicon for improved casting characteristics. It is used extensively in the T5 temper for heavy-duty applications, such as large rolling-mill bearings. It is particularly suitable for this application because of its anti...
Journal Articles
Alloy Digest (1983) 32 (11): Al-248.
Published: 01 November 1983
... ALUMINUM 852.0 contains higher concentrations of copper and nickel than either Aluminum 850.0 or Aluminum 851.0 alloy. The higher copper and nickel percentages and an addition of magnesium give Aluminum 852.0 higher strength and make it suitable for bearing applications requiring improved...
Journal Articles
Alloy Digest (1988) 37 (9): Al-290.
Published: 01 September 1988
... 850.0 ALUMINUM Alloy can be considered the general purpose light metal bearing alloy. Its good thermal conductivity keeps operating temperatures low. It has high ductility. In many applications it has been found to be superior to steel backed bearings. 852.0 ALUMINUM Alloy has higher mechanical...
Journal Articles
Alloy Digest (1991) 40 (7): TS-360.
Published: 01 July 1991
... CARPENTER VIM-VAR M-50 Bearing Steel is produced by vacuum induction melting and vacuum arc remelting. The alloy's high degree of cleanliness enables it to be finished to a high luster. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1956) 5 (7): Sn-2.
Published: 01 July 1956
... FEDRATED NO. 3 is a tin-base bearing alloy recommended for moderate to high speeds and loads. It has low frictional resistance, low wear, good running-in properties, good emergency behavior upon failing of lubrication, and lower coefficient of expension than the lead-base alloys. This datasheet...
Journal Articles
Alloy Digest (1956) 5 (8): Pb-3.
Published: 01 August 1956
... FEDERATED No. 8 is a lead-base bearing alloy recommended for moderate to high speeds and moderate loads. It has very good frictional properties, reasonably good corrosion resistance and low price. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1956) 5 (9): Al-43.
Published: 01 September 1956
... Alloy 750 is an aluminum-tin-nickel-copper alloy used for bearings. This material is intended for, and has been used principally in the form of permanent mold castings, which by virtue of their rapid solidification are typified by a fine, dense, fatigue resistant structure. Solid aluminum bearings...
Journal Articles
Alloy Digest (1956) 5 (11): Cu-44.
Published: 01 November 1956
... NI-VEE TYPE E is a precipitation hardening leaded-nickel bearing bronze suitable for bearings and acid-resisting castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as deformation. It also...
Journal Articles
Alloy Digest (1953) 2 (4): Cu-7.
Published: 01 April 1953
... HY-TEN-SL No. 1 Copper Alloy APRIL, 1953 DATA ON WORLD WIDE METALS AND ALLOYS Published by Engineering Alloys Digest. Inc. Upper Montclair, New Jersey HY-TEN-SL No. 1 (ALUMINUM-MANGANESE BEARING BRONZE) I-W-TEN-SL No. 1 is a dose-grained, tough, homogeneous metal, having the non-corrosive properties...
Journal Articles
Alloy Digest (1954) 3 (4): SA-16.
Published: 01 April 1954
... machinability physical properties tensile properties workability All Or DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: SA-16 Steel Alloy APRIL, 1954 AISI ES2 100 (Bearing Steel) AISI E52100 is a high-carbon, chromium alloy steel of the water hardening type. It has great depth hardenability...
Journal Articles
Alloy Digest (1954) 3 (8): Cu-19.
Published: 01 August 1954
... Federaloy F-1 is a copper tin-zinc bearing bronze whose strength suits it for applications where loads are heavy. It should be used only where lubrication is exceptionally good or motion is of a rocking nature. It is also a good gear bronze. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1954) 3 (9): Pb-1.
Published: 01 September 1954
... Federated No. 7 is a lead-base white Babbitt metal used for bearings where speeds, loads and stresses are moderate. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1954) 3 (10): Sn-1.
Published: 01 October 1954
... Federated No. 2 is a tin-base white Babbitt metal used for bearings where speeds, loads and stresses are moderate to high. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also...
Journal Articles
Alloy Digest (1977) 26 (3): Cu-328.
Published: 01 March 1977
... BUNTING Alloy 907 is a cast copper-tin alloy (tin bronze) recommended for severe service requirements. It is used widely for bearings and gears. It is a standard alloy for the manufacture of cast gear blanks and has long been known as Phosphor Gear Bronze. This datasheet provides information...
Journal Articles
Alloy Digest (1978) 27 (5): SA-346.
Published: 01 May 1978
... INLAND HI-FORM Steels are a low-carbon, low or intermediate-manganese, low-sulfur, aluminum-killed, fine-grain, columbium and/or phosphorus-bearing series of high-strength steels providing greatly enhanced forming and bending properties. These steels are furnished in minimum yield strength levels...
Journal Articles
Alloy Digest (1979) 28 (4): Cu-370.
Published: 01 April 1979
... Copper APRIL 1979 - DATA ON WORLD WIDE MnALS AND ALLOYS - wJiIC~~ hf2 Upper Mootdair, New Jagr Copper No. 803 (High-Conductivity Silver-Bearing Casting Copper) Copper No. 803 is cast copper containing silver to raise its softening temperature and improve its elevated-temperature prop- erties. It has low...
Journal Articles
Alloy Digest (1979) 28 (8): SA-363.
Published: 01 August 1979
... TIMKEN TBS-9 is a high-carbon, chromium-molybdenum ball-bearing steel that combines high hardenability and low cost. It was designed with metallurgical properties virtually equivalent to those of AISI 52100. TBS-9 is less expensive than the 52100 grade because annealing is simplified...
Journal Articles
Alloy Digest (1979) 28 (11): SS-370.
Published: 01 November 1979
... CARPENTER CRB-7 is a corrosion-resistant, wear-resistant and secondary-hardening steel for high-temperature bearings. It has high quenched-and-tempered hardness and maintains high hardness at elevated temperatures. CRB-7 is a martensitic type of stainless steel. This datasheet provides information...