Alloy Digest (1974) 23 (11): Cu-287.
Published: 01 November 1974
... Copper Alloy No. 674 is a non-heat-treatable, high-strength bearing alloy for applications requiring good bearing properties, especially in conjunction with hardened steel mating surfaces, and the ability to stand up under moderately high loads. It has outstanding resistance to wear along...
Journal Articles
Alloy Digest (1984) 33 (8): Cu-481.
Published: 01 August 1984
... MUELLER Alloy 6732 is a free-machining high-leaded copper-base alloy that is especially well suited for screw machine work. It can be used with hard or soft mating members. It can be joined readily by soft or silver soldering. It possesses excellent bearing properties, high mechanical properties...
Journal Articles
Alloy Digest (1954) 3 (1): Al-12.
Published: 01 January 1954
... BOHNALITE J is a high-copper aluminum alloy suitable for permanent mold and sand casting. It responds to heat treatment to produce high mechanical properties. It retains its strength well and has other excellent properties at elevated temperatures. Its bearing properties are also good...
Journal Articles
Alloy Digest (2006) 55 (2): Cu-740.
Published: 01 February 2006
... Hidurax 1 is a complex nickel-aluminum bronze possessing good mechanical strength and hardness. Advantages and benefits to be obtained with this alloy include ductility, corrosion resistance, wear resistance, superior bearing properties, and fatigue strength. The excellent properties of Hidurax 1...
Journal Articles
Alloy Digest (1973) 22 (7): Zn-16.
Published: 01 July 1973
... KORLOY 2570 and 2573 are zinc-base alloys possessing superior strength and good low-temperature impact properties down to -60 F. They are easily forged, extruded and machined for wrought applications and alloy 2570 can be used in the cast condition. They have excellent bearing properties and can...
Journal Articles
Alloy Digest (2022) 71 (1): CI-89.
Published: 01 January 2022
... are not the crucial properties in service. The high carbon content of this material also imparts good lubricated bearing properties. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on heat treating...
Journal Articles
Alloy Digest (2022) 71 (3): CI-91.
Published: 01 March 2022
..., and machinability are important, but where tensile strength and hardness are not the crucial properties in service. The high carbon content of this material also imparts good lubricated bearing properties, provided that the environment does not include abrasive debris that can score and wear the soft matrix...
Journal Articles
Alloy Digest (2020) 69 (3): CI-67.
Published: 01 March 2020
..., but where tensile strength and hardness are not the crucial properties in service. The high carbon content of this material also imparts good lubricated bearing properties. This datasheet provides information on composition, physical properties, tensile properties, shear and bend strength as well as fatigue...
Journal Articles
Alloy Digest (2008) 57 (8): Cu-757.
Published: 01 August 2008
... Ansonia alloy C54400, a leaded phosphor bronze alloy, combines machinability with bearing properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (1978) 27 (10): Cu-361.
Published: 01 October 1978
... MUELLER Alloy No. 6300 (formerly MBCo. Alloy 224K and sometimes called Tuf-Stuf Alloy) is a heat-treatable aluminum bronze containing 5% nickel. It is intended for those applications requiring combinations of corrosion resistance, excellent bearing properties at considerable loads, and extremely...
Journal Articles
Alloy Digest (1965) 14 (10): Cu-156.
Published: 01 October 1965
... recommended for the toughest applications as wear strips, slides and bearings in tools and dies, machine tools and industrial equipment. It is generally used for sliding contact applications in which a high strength bearing surface is required. This alloy has excellent bearing properties when used against...
Journal Articles
Alloy Digest (1963) 12 (3): Al-123.
Published: 01 March 1963
... NORAL 162 is an age-hardenable aluminum casting alloy. It has low thermal expansion, good high temperature strength and bearing (frictional) properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear...
Journal Articles
Alloy Digest (1971) 20 (6): Cu-235.
Published: 01 June 1971
... MUELLER ALLOY No. 6741 (formerly 600 Alloy) is a high-strength bearing alloy intended for use in applications requiring a combination of outstanding wear characteristics and high bearing strength. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1961) 10 (10): Cu-108.
Published: 01 October 1961
... physical properties tensile properties workability MUELLER 604 Filing Code: Cu-108 Copper Alloy OCTOBER 1961 -DATA ON WORLD WIDE METALS AND ALLOYS MUELLER 604 (High-Leaded Bearing Alloy) Psblisbd by h&aing Alloys Digest, Inc. Upper Moatdair. New Jasq MUELLER 604 is a high leaded copper alloy...
Journal Articles
Alloy Digest (1968) 17 (10): Cu-192.
Published: 01 October 1968
... PROMET No. 3 is a leaded tin bronze possessing a good combination of physical properties and corrosion resistance. It is recommended for bearings, gears, pump bodies and impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (2005) 54 (10): Cu-737.
Published: 01 October 2005
... Marinel 230 is an ultrahigh-strength alloy with improved bearing and hardness properties compared to Marinel (see Alloy Digest Cu-602, December 1995). It is a copper alloy with 18% nickel and high manganese and aluminum. It develops high strength with excellent corrosion resistance in seawater...
Journal Articles
Alloy Digest (2009) 58 (4): Cu-769.
Published: 01 April 2009
... of cold work to the material before precipitation-hardening. The alloy provides: High strength Excellent bearing properties/wear resistance Good electrical and thermal conductivity Very low magnetic permeability <1.001 Spark resistance Full retention of impact properties to 196 °C ( 321 °F...
Journal Articles
Alloy Digest (1966) 15 (4): Cu-163.
Published: 01 April 1966
... PROMET BRONZE No. 100 is a manganese bronze containing alpha and beta phases and offering an excellent combination of mechanical properties. It is recommended for cast gears, bearings, propellers and marine hardware. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1956) 5 (7): Sn-2.
Published: 01 July 1956
... FEDRATED NO. 3 is a tin-base bearing alloy recommended for moderate to high speeds and loads. It has low frictional resistance, low wear, good running-in properties, good emergency behavior upon failing of lubrication, and lower coefficient of expension than the lead-base alloys. This datasheet...
Journal Articles
Alloy Digest (1986) 35 (9): Cu-514.
Published: 01 September 1986
... many applications are bearings, bushings, connecting rods, pump parts, gears, cams and seal rings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...