Alloy Digest (2021) 70 (4): SA-870.
Published: 01 April 2021
... SSAB Armox 500T is a low-carbon, nickel-chromium-molybdenum-boron, alloy protection steel that is used in the quenched and tempered condition (typical hardness = 500 HBW) for ballistic protection. This datasheet provides information on composition, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (2021) 70 (8): SA-875.
Published: 01 August 2021
... SSAB Ramor 500 is a nickel-chromium-molybdenum-boron, alloy protection steel that is used in the quenched condition (hardness = 490–560 HBW) for ballistic protection. This datasheet provides information on composition, hardness, tensile properties, and bend strength. It also includes information...
Journal Articles
Alloy Digest (2021) 70 (3): SA-869.
Published: 01 March 2021
... Industeel Mars 380 (earlier known as Industeel Mars 190) is a low-carbon, Ni-Cr-Mo-V-B, alloy protection steel that is used in the quenched and tempered condition (typical hardness = 380 HBW). It is used as rolled homogeneous armor for ballistic protection and evaluation of armor-defeating...
Journal Articles
Alloy Digest (2004) 53 (7): Ti-133.
Published: 01 July 2004
... ATI 425 was originally developed for hot-rolled armor plate to provide ballistic protection comparable to Ti-6Al-4V and has been evaluated against a variety of projectile threats for use as armor. While processing the alloy for armor plate applications, it was observed that the material exhibited...
Journal Articles
Alloy Digest (2013) 62 (9): SA-682.
Published: 01 September 2013
... MARS 270 is a high hardness (510/550 HB) steel for ballistic protection. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-682...
Journal Articles
Alloy Digest (2013) 62 (11): SA-685.
Published: 01 November 2013
... MARS 300 is a super high-hardness (620 HB) steel for ballistic protection. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (2012) 61 (12): SA-668.
Published: 01 December 2012
... Mars 240 is a high hardness (500 HB) steel for ballistic protection. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-668...
Journal Articles
Alloy Digest (2007) 56 (2): SA-560.
Published: 01 February 2007
... K12 has a Ni-Mo-Cr alloy steel composition and possesses an appropriate combination of hardness and toughness mandatory for proper ballistics performance. K12 plate is normally supplied in the annealed condition so that it may be more easily cut and formed into the desired configuration. It may...
Journal Articles
Alloy Digest (2013) 62 (11): SA-686.
Published: 01 November 2013
...: Steel Alloy November 2013 SA-686 Armox Advance combines good ballistic properties with excellent toughness. Hardness for Advance is 58 63 HRC. ARMOX® ADVANCE (High Strength Protection Steel Plate) ARMOX® ADVANCE Chemical Composition, wt (Ladle analysis, maximum) Carbon 0.47 Silicon 0.7 Manganese 1.0...
Journal Articles
Alloy Digest (2012) 61 (11): SA-667.
Published: 01 November 2012
... MARS 220 is a medium hardness steel (440 HB) for blast protection. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing...
Journal Articles
Alloy Digest (2013) 62 (10): SA-683.
Published: 01 October 2013
...@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Steel Alloy October 2013 SA-683 Armox® 600T combines good ballistic properties with excellent toughness. Hardness for 600T is 570 640 HBW. ARMOX® 600T (High Strength Protection Steel Plate) ARMOX® 600T Chemical Composition, wt (Ladle analysis...
Journal Articles
Alloy Digest (2013) 62 (3): SA-674.
Published: 01 March 2013
...@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Steel Alloy March 2013 SA-674 Armox® 370T Class 1 combines good ballistic properties with excellent toughness. ARMOX® 370T Class 1 (High Strength Protection Steel Plate) ARMOX® 370T Class 1 Chemical Composition, wt (Ladle Analysis, maximum...
Journal Articles
Alloy Digest (2013) 62 (5): SA-677.
Published: 01 May 2013
... www.asminternational.org Filing Code: Steel Alloy May 2013 SA-677 Armox 370T Class 2 combines good ballistic properties with excellent toughness. Hardness for Class 2 is 380 430 HBW. ARMOX® 370T Class 2 (High Strength Protection Steel Plate) ARMOX® 370T Class 2 Chemical Composition, wt (Ladle analysis, maximum) Carbon...
Journal Articles
Alloy Digest (1979) 28 (4): Al-234.
Published: 01 April 1979
... ALUMINUM A201 offers high strength, high impact resistance, a good combination of room and elevated-temperature performance, and good ballistic properties. Its ballistic properties are comparable to those of the standard wrought aluminum alloys. Among its many application are components...
Journal Articles
Alloy Digest (2013) 62 (8): SA-680.
Published: 01 August 2013
...: Steel Alloy August 2013 SA-680 Armox 500T combines good ballistic properties with excellent toughness. Hardness is 480 540 HBW. ARMOX® 500T (High-Strength Protection Steel Plate) ARMOX® 500T Chemical Composition, wt (Ladle analysis, maximum) Carbon 0.32 Silicon 0.4 Manganese 1.2 Phosphorus 0.015 Sulfur...
Journal Articles
Alloy Digest (2012) 61 (10): SA-664.
Published: 01 October 2012
...-3000 Fax: (610) 383-3007 In France Usinor Industeel France 71201 Le Creusot Cedex, France Tel: +33 3 85 80 55 35 Fax: +33 3 85 80 56 99 www.industeel.info ISSN: 002-614X SA-664B Table 2 Ballistic properties Threat Vo, m/s (ft/s) Distance, m (ft) Obliquity, degrees Thickness for protection, mm...
Journal Articles
Alloy Digest (2009) 58 (9): SA-606.
Published: 01 September 2009
... is designed to meet or exceed the ballistic requirements of MIL- DTL-46100E. AP, armor piercing; cal, caliber; fps, feet per second; mps, meters per second; BL(P), V50 protection ballistic limit Mechanical Properties: Typical mechanical property data for this alloy are included. These data represent...
Journal Articles
Alloy Digest (2013) 62 (7): SA-679.
Published: 01 July 2013
...: Alloy Steel July 2013 SA-679 Armox 440T combines good ballistic properties with excellent toughness. ARMOX® 440T (High-Strength Protection Steel Plate) ARMOX® 440T Chemical Composition, wt (Ladle analysis, maximum) Carbon 0.21 Silicon 0.5 Manganese 1.2 Phosphorus 0.010 Sulfur 0.010 Chromium 1.0 Nickel...
Journal Articles
Alloy Digest (1969) 18 (4): Ni-144.
Published: 01 April 1969
... drawn shields, consideration should be given to the use of the more ductile alloy, such as Mumetal). The use of protective atmosphere, preferably commercial hydrogen, will obviate the necessity for removing scale which might be detrimental to subsequent drawing operations. It is to be noted...
Journal Articles
Alloy Digest (1966) 15 (6): SA-197.
Published: 01 June 1966
... shielded arc welding is done with filler wires of Type MIL-B88 for butt, seam, and fillet welds. To ensure dry steel and prevent cracking of weld metal and heat-affected zones and in cases of heavy restraint or rigidity, particularly with fillet welds, preheating should be applied to 3000F. To protect...