Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (4): Al-234.
Published: 01 April 1979
... ALUMINUM A201 offers high strength, high impact resistance, a good combination of room and elevated-temperature performance, and good ballistic properties. Its ballistic properties are comparable to those of the standard wrought aluminum alloys. Among its many application are components...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (3): SA-674.
Published: 01 March 2013
... Armox 370T Class 1 combines good ballistic properties with excellent toughness. Hardness for Class 1 is 380–430 HBW for thicknesses up to 20 mm (0.78 in.). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (5): SA-677.
Published: 01 May 2013
... Armox 370T Class 2 combines good ballistic properties with excellent toughness. Hardness for Class 2 is 280-330 HBW for thicknesses up to 150 mm (6 in.). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (7): SA-679.
Published: 01 July 2013
... Armox 440T combines good ballistic properties with excellent toughness. Hardness is 420-480 HBW. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-679...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (8): SA-680.
Published: 01 August 2013
... Armox 500T combines good ballistic properties with excellent toughness. Hardness is 480–540 HBW. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming and joining. Filing Code: SA-680...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (10): SA-683.
Published: 01 October 2013
... Armox 600T combines good ballistic properties with excellent toughness. Hardness for 600T is 570–640 HBW. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as forming, heat...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (11): SA-686.
Published: 01 November 2013
... Armox Advance combines good ballistic properties with excellent toughness. Hardness for Advance is 58-63 HRC. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-686...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (11): SA-685.
Published: 01 November 2013
... MARS 300 is a super high-hardness (620 HB) steel for ballistic protection. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (4): SA-870.
Published: 01 April 2021
... SSAB Armox 500T is a low-carbon, nickel-chromium-molybdenum-boron, alloy protection steel that is used in the quenched and tempered condition (typical hardness = 500 HBW) for ballistic protection. This datasheet provides information on composition, hardness, and tensile properties. It also...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (9): SA-682.
Published: 01 September 2013
... MARS 270 is a high hardness (510/550 HB) steel for ballistic protection. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-682...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (12): SA-668.
Published: 01 December 2012
... Mars 240 is a high hardness (500 HB) steel for ballistic protection. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-668...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (8): SA-875.
Published: 01 August 2021
... SSAB Ramor 500 is a nickel-chromium-molybdenum-boron, alloy protection steel that is used in the quenched condition (hardness = 490–560 HBW) for ballistic protection. This datasheet provides information on composition, hardness, tensile properties, and bend strength. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (3): SA-869.
Published: 01 March 2021
... in the quenched and tempered condition (typical hardness = 380 HBW). It is used as rolled homogeneous armor for ballistic protection and evaluation of armor-defeating ammunition. Chemical Composition Ballistic Properties Element Composition, wt%(a)(b) See Tables 2 and 3. Carbon 0.30 Silicon 0.4 Delivery Condition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (10): SA-664.
Published: 01 October 2012
... specification. Physical Properties: Density, kg/m3 (lb/in.3) 8100 (0.29) Mechanical Properties: Tensile properties for flat products of different thicknesses are shown in Table 1. Ballistic properties are shown in Table 2. Heat Treatment: Mars 190 is a quenched and high tempered armor steel. Formability: Hot...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (2): SA-560.
Published: 01 February 2007
... hardness armor plate routinely exhibits superior ballistic performance compared with conventional homogeneous armor plate. Microstructure. Proper heat treatment is crucial in developing the optimum microstructure for good ballistics properties. Structural Characteristics. K12 plate is a refined steel...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (10): SA-610.
Published: 01 October 2009
.../°F) 11.6 (6.5) Ballistic properties are shown in Fig. 1 and 2. Mechanical Properties: Typical mechanical property data for this alloy are included below. These data represent an average of results for 0.275 and 0.199 in. (7 and 5 mm) plate. Fig. 1 Typical ballistic results .30 AP M2 at 30° UHHS...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (11): SA-667.
Published: 01 November 2012
... for flat products are shown in Table 1. Ballistic Properties. MARS 220 steel grade has been defined for high ballistic blast resistance against mines (shock effects). Against kinetic projectiles, MARS 220 steel has a ballistic comportment between MARS 19 (< 400 HB) and MARS 240 (500 HB). Heat Treatment...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (9): SA-606.
Published: 01 September 2009
... expansion, at 20 100 °C (68 212 °F), 10 6/K (10 6/°F) 11.6 (6.5) Ballistic properties are shown in Table 1. Table 1 Average tensile properties of annealed K12 plate Size MIL-DTP- 46100EBL(P) mm in. Threat level mps fps BL(P) 5.06 0.199 .30 cal AP 579.4 1901 Exceeds spec 6.35 0.25 .30 cal AP 681.8 2237...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (2): Al-244.
Published: 01 February 1983
.... The T7 condition meets all of the stress- corrosion standards established for high-strength aluminum alloys. Ballistic Properties: Actual firing tests. made in accordance with MIL-A46027. show that the ballistic merit ra1ing of Aluminum A206.0 compares favorably with that of other high-strength aluminum...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (8): Ti-146.
Published: 01 August 2008
... is an alpha-beta alloy with superior machinability and strength comparable to that of Ti -6Al-4V. Timetal 54M can provide cost savings over Ti-6Al-4V parts that require extensive machining operations by extending tool life. Mechanical properties including tensile, fatigue, fracture toughness, and ballistic...