1-20 of 85 Search Results for

ball bearings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (2): SA-406.
Published: 01 February 1985
... STROLOY 503-A is a hypereutectoid steel of bearing quality. It has through-hardening characteristics similar to those of AISI 52100 steel. Stroloy 503-A is made in accordance with ASTM A 295-84. It is used principally in ball bearing applications. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2013) 62 (11): SS-1160.
Published: 01 November 2013
... and has been used for cutlery, ball bearings, and small machinery parts subjected to high wear conditions. This datasheet provides information on composition and physical properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1979) 28 (8): SA-363.
Published: 01 August 1979
... TIMKEN TBS-9 is a high-carbon, chromium-molybdenum ball-bearing steel that combines high hardenability and low cost. It was designed with metallurgical properties virtually equivalent to those of AISI 52100. TBS-9 is less expensive than the 52100 grade because annealing is simplified...
Journal Articles
Alloy Digest (1969) 18 (4): SS-223.
Published: 01 April 1969
... AISI Type 440B is a hardenable high-carbon high-chromium steel recommended stainless for cutlery, valve parts, ball bearings, pivot pins, etc. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1984) 33 (1): CS-99.
Published: 01 January 1984
...) but it may be quenched in oil if a less drastic quench meets requirements. Its many uses include springs, bushings, drills, hay-rake teeth, pins and ball bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1963) 12 (1): TS-128.
Published: 01 January 1963
..., fine ball bearings, special rolls, rollers for ball bearings, arbors, bearing races. Manufacturer: Width of Cut inch Forming Circular or dovetail Cutoff upto 1 1 co 2 2 co 2% 2% co 3 3adup l/16 l/8 Feed in/rev 0.0015 0.00125 0.001 0.00075 0.0005 0.0008 0.0011 Speed Efpm 70-80 70-80 70-80 70-80 65-75...
Journal Articles
Alloy Digest (1978) 27 (10): SS-356.
Published: 01 October 1978
... Remelted) to consistently assure good cleanliness and superior properties. It is used for bearings, gears, ball screws and other aerospace applications. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (1968) 17 (10): Co-56.
Published: 01 October 1968
... hard- ness after exposure to temperature as high as 20000F. It s resistance to oxidation, corrosion and erosion is excellent. Forms Available: Castings Applications: Cutting tools, ball bearing rolls, bearing balls, sleeves, bushings, wear strips, valve seat inserts, knives, scraper blades, cutters...
Journal Articles
Alloy Digest (1992) 41 (2): SS-179.
Published: 01 February 1992
... to that of AISI type 440C stainless. Rolling contact fatigue properties are shown in Fig. 2, the results of tests on three heats of the alloy. Applications: Ball bearings in aircraft pneumatic actuator motor rotors, pneumatic valves, gear box and ball screw support bear- ings. Producer: Latrobe Steel Company...
Journal Articles
Alloy Digest (1966) 15 (2): SA-192.
Published: 01 February 1966
... and roughness is required. Forms Available: Billets, bars and forgings. Applications: Ball bearings, bearing races, pivot bearings, rollers for roller bearings, special rolls, precision gauges, special arbors, special dies. Manufacturer: \ anadium Alloys Steel Company Division of \ asco hletals Corporation...
Journal Articles
Alloy Digest (1999) 48 (2): SS-737.
Published: 01 February 1999
... Crucible 154 CM is a hardenable chromium stainless steel with molybdenum to improve hot hardness and corrosion resistance. Typical applications include bushings and bearings where high hardness is needed. This datasheet provides information on composition, physical properties, and hardness...
Journal Articles
Alloy Digest (2007) 56 (2): Fe-140.
Published: 01 February 2007
...: The alloy is supplied in a wide variety of strip dimensions. Applications: Application include springs for clock motors, springs for rough watch movements, form springs for analog quartz watches, springs for miscellaneous applications, weighing machines, precision bearing balls, ball bearing cages...
Journal Articles
Alloy Digest (2007) 56 (3): Fe-141.
Published: 01 March 2007
.... Applications: Applications include springs for clock motors, springs for rough watch movements, form springs for analogue quartz watches, springs for miscellaneous applications, weighing machines, precision bearing balls, ball-bearing cages, electrical and electronic apparatus, plastics industry, defense...
Journal Articles
Alloy Digest (1963) 12 (5): Cu-128.
Published: 01 May 1963
... bearings, valve guides, valve seat inserts, ball bearings, pump and marine shafting, machine tool parts, sleeves, valve stems. Manufacturer: Ampco hletal Inc. h!ilwaukee. Risconsin Satisfactorily welded with any of the arc welding processes available. Oxy-acetylene welding is not recommended. Filler metal...
Journal Articles
Alloy Digest (1963) 12 (6): Co-16.
Published: 01 June 1963
.... Round wire requires a cold reduc- cion of 4548% in cross-sectional area Forms Available: Strip and wire. Applications: Watch springs, main springs, power springs, pen nibs, corrosion resistanr ball bearings, flapper valves, textile thread guides, drawing instruments, sewing machine parts, cutlery, valve...
Journal Articles
Alloy Digest (1997) 46 (11): SS-700.
Published: 01 November 1997
.... The better the i%ish of the hardened and temper& part, the better will be its corrosion resistance. Crucible 44OC scales at approximately 760 C (1400 F). This temperamre will vary with the type of atmosphere, type of con- st~~ctiou and cycle of operation. Typical Applications: Ball bearings. bushings...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... Solphuric acid 2 R.T. O.WOl lSo°F 0.023 z ET: o.OOi.l2 0.0003 Hydrochloric acid 2 R.T. 0.009 IsoOF 0.169 20 R.T. 0.026 Sodium hydroxide S Boiling o.ows Applications: Cutting toois, ball bearing rolls, bearing balls, sleeves, bushings, wear amps, valve seat mseru, ksives, scraper blades, caters, valve psrts...
Journal Articles
Alloy Digest (2020) 69 (7): SS-1321.
Published: 01 July 2020
...; magnetic in both the annealed and hardened conditions. Product Forms Billet; flat, hexagonal, round, and square bars; strip; wire rod; wire Applications CarTech 420 is used for ball bearings, ball check valves, cams, cutlery, gauges, gears, magnets, needle valves, pivots, scissors, shafts, surgical...
Journal Articles
Alloy Digest (1988) 37 (6): SS-101.
Published: 01 June 1988
..., ground bars. wire and wire rods. annealed strip. Applications: Pivot pins. dental and surgical instruments. cutlery. valve pans, ball bearings. nozzles, hardened steel balls and seats for oil well pumps, wear-resistant textile machlne pans. Manufacturer: Stamless steel mills. ...
Journal Articles
Alloy Digest (2001) 50 (7): SS-826.
Published: 01 July 2001
..., plastic extru- sion dies, cutlery, surgical and dental instruments, gages, valves, shafts, cams, and ball bearings. Producer: Timken Latrobe Steel A Timken Company Subsidiary Latrobe, PA (724) 537-7711 (724) 532-6316 (fax) ISSN: 002-614X SS-826B Fig. 1 Tempering temperature with resulting hardness...