Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (1): SS-1314.
Published: 01 January 2020
... AK Steel Types 430, 434, 435 Mod, and 436 are ferritic stainless steels that provide a combination of corrosion resistance, functionality, and beauty that make them suitable for many roll-formed and stamped automotive trim applications. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (4): Al-121.
Published: 01 April 1978
... ALUMINUM 5457 is an aluminum sheet alloy that offers a lustrous, mirror-like appearance when polished, brightened and anodized. The brightness of the specially treated sheet makes it particularly desirable for decorative trim applications in the appliance and automotive industries. This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (5): Al-189.
Published: 01 May 1981
... ALUMINUM 6463 is an aluminum-magnesium-silicon alloy used widely for extrusions. It can be hardened and strengthened by a precipitation-hardening heat treatment. Its many applications comprise extrusions for trim and archtectural use in the automotive, appliance and building industries...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (3): SS-422.
Published: 01 March 1983
...) shows improved resistance to pitting attack from various de-icing chemicals. In addition, the color of Uniloy 434, when buffed, closely resembles that of bright chromium plate. Hence a popular application for Uniloy 434 is automotive trim. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (9): Zn-22.
Published: 01 September 1975
... NJZ ALLOY No. 25 is a zinc-copper-titanium alloy that offers outstanding high creep resistance and a low coefficient of expansion. It can be severely work hardened. Its applications include architectural building products, sporting equipment components, hardware and automotive trim. This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (1): SS-266.
Published: 01 January 1972
... ALLEGHENY TYPE 211 is a copper-bearing, austenitic, chromium-nickel-manganese stainless steel with a low work-hardening rate. It is used for many deep-drawing applications, such as automotive trim, and broiler pans, mixing bowls, sinks, and door hardware. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (2): SS-292.
Published: 01 February 1974
... or heat tint on these alloys. These discolorations must be completely removed to realize maximum corrosion resistance. Corrosion Resistance: Allegheny Stainless Type 434 is resistant to attack in a wide variety of corrosive media. It has exrensive use for automotive trim applications where it shows...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (8): Al-178.
Published: 01 August 1980
... ALUMINUM 5657 is an aluminum-base, wrought, non-heat-treatable alloy of high purity and bright appearance. It has high resistance to general corrosion and to stress-corrosion cracking. It is used widely in the anodized condition for automotive and appliance trim. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (6): SS-792.
Published: 01 June 2000
... as sheet with thicknesses of 0.20 3.68 mm (0.008 0.145 in.) and widths up to and including 1219 mm (48 in Applications: Typical consumer product applications include automotive trim and molding, furnace combustion chambers, dishwashers, range hoods, gas burners and heating units, gutters and down spouts...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (8): SS-828.
Published: 01 August 2001
.../pattern, polished, or brushed. Applications: Typical applications include domestic appliances, trim work, catering surfaces, decorative tubes, window fittings, strapping, decorative and coated panels, automotive components and pressings, and cutlery. Producer: AvestaPolarit, Inc. 425 N. Martingale Rd...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (6): Al-176.
Published: 01 June 1968
..., brightened and anodized, offers a lustrous mirror-like appearance. Brightness of the specially treated sheet makes it of particular importance for decorative trim applications in the automotive and appliance industries. Forms Available: Flat and coiled sheet, plate. Applications: Automotive and appliance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (1): Al-161.
Published: 01 January 1980
... ALUMINUM 5252 is a high-purity aluminum-magnesium alloy of moderate strength, good fabricating characteristics and excellent resistance to corrosion. It is highly resistant to denting and is used widely as trim in the automotive industry and for a wide variety of other industrial products...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (7): Zn-16.
Published: 01 July 1973
....; control consoles; shelf fronts; thin decorative trim strips. Automotive: radiator grilles, grille components, rocker panels, side trim, windshield molding, luggage and ski racks. Hardware: door handles and pulls, bathroom towel bars, drawer pulls, latches, brackets, etc. Office furniture, vending machine...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (5): SS-408.
Published: 01 May 1982
..., sheet and strip. Applications: Typical uses for Uniloy 430 are architectural trim, oil refining equipment, automotive trim or molding, nitric acid storage tanks and tank cars, fasteners, combustion-chamber liners for diesel engines, oil-burner parts, television cones. and household and kitchen...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (6): SA-848.
Published: 01 June 2019
... CP-K 570Y780T is one of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (5): Zn-15.
Published: 01 May 1973
... bending, forming or other fabricating operations. Forms Available: Bar, rod, forgings and extruded forms. Applications: Architectural uses. Appliances: handles for refrigerators, ranges, washers, etc.; control consoles; shelf fronts; thin decorative trim strips. Automotive: radiator grilles, grille...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (9): Zn-1.
Published: 01 September 1991
...: Ingot, die castings. Applications: Automotive components (housings, heat sinks, trim, handles), electronics, household faucets, hand tools and a wide variety of general purpose applications where net shape, precision and physical properties are important. Producer: Noranda Sales Corporation Toronto...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (7): SA-849.
Published: 01 July 2019
... CP-K 900Y 1180T is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (4): P-2.
Published: 01 April 1989
... thermoplastic resins are alloys of acryloniaile butadiene styrene (ABS) and polycarbonate (PC) engineered initially for automotive applications but capable of being adapted to other uses to meet specific customer needs. Types 13 10.1350 and 1370 described here have proprietary formulations. PROPERTIES Table 1...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (3): SA-841.
Published: 01 March 2019
... CP-W 660 is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles...