1-20 of 43 Search Results for

automotive exhaust systems

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1998) 47 (2): SS-708.
Published: 01 February 1998
... Incoloy Alloy 864 is a high performance alloy developed specifically for automotive exhaust system flexible couplings and other exhaust applications. The alloy has a good combination of oxidation and corrosion resistance, with good mechanical strength, stability, and fatigue properties...
Journal Articles
Alloy Digest (2013) 62 (2): SS-1135.
Published: 01 February 2013
... ATI 409HP (UNS S40900) ferritic stainless steel was introduced by ATI Allegheny Ludlum to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon steel. The alloy was designated "MF-1", indicating its end use: automotive mufflers. The good...
Journal Articles
Alloy Digest (2021) 70 (11): SS-1341.
Published: 01 November 2021
..., Outokumpu Moda 439/4510 can be welded in all dimensions without becoming susceptible to intergranular corrosion. It is possible to use Outokumpu Moda 439/4510 at elevated temperatures, for example the cold end of automotive exhaust systems. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2021) 70 (12): SS-1342.
Published: 01 December 2021
.... It is possible to use Outokumpu Moda 409/4512 at elevated temperatures, for example in automotive exhaust systems, where it is often used to replace aluminum-coated carbon steel. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2004) 53 (4): SS-902.
Published: 01 April 2004
... J and L Type 409NI is a ferritic stainless steel with 11% Cr. It exhibits an excellent combination of good formability, economy, and resistance to oxidation and corrosion. It is typically used in automotive exhaust systems or where more forming is required. This datasheet provides information...
Journal Articles
Alloy Digest (1971) 20 (11): SS-263.
Published: 01 November 1971
... ALLEGHENY LUDLUM MF-1 is a chromium-titanium corrosion resisting steel that was developed originally for automotive exhaust system applications. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature...
Journal Articles
Alloy Digest (1997) 46 (7): SS-690.
Published: 01 July 1997
... Armco 11 Cr-Cb stainless steel has higher silicon content and is dual stabilized with titanium and columbium (niobium). The alloy is designed for use in automotive exhaust systems and should be considered where the performance of AISI Type 409 stainless steel is marginal. This datasheet provides...
Journal Articles
Alloy Digest (1999) 48 (5): SS-743.
Published: 01 May 1999
... J and L Types 409 HP are ferritic stainless steels with 11% chromium. They exhibit an excellent combination of good formability, economy, and resistance to oxidation and corrosion. It is typically used in automotive exhaust systems. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1987) 36 (6): SS-486.
Published: 01 June 1987
... ARMCO 439 HIGH PERFORMANCE-10 is a ferritic stainless steel sheet and strip alloy suited to automotive-exhaust system applications where oxidatin resistance is needed at temperatures beyond the capability of AISI Type 409 to withstand. The alloy also has good resistance to wet chloride...
Journal Articles
Alloy Digest (1972) 21 (4): SS-270.
Published: 01 April 1972
... and can be welded by conventional methods. It has excellent oxidation resistance and is highly resistant to corrosives of the type found in automotive exhaust systems. It can be hardened only by cold work. Since it does not air harden, welding problems are minimized. In general, it can be fabricated...
Journal Articles
Alloy Digest (2005) 54 (9): SS-939.
Published: 01 September 2005
... in comparison to AL409 HP base metal, in acid environments such as automotive exhaust system condensates. Austenitic stainless steel filler metals also are appropriate for joining the 409 ALMZ product to itself, carbon steel, or austenitic stainless steels. Because of its balance chem- istry and proper...
Journal Articles
Alloy Digest (2010) 59 (5): SS-1062.
Published: 01 May 2010
... International AK STEEL 436L ULTRA FORM automotive exhaust systems chemical composition corrosion-resistant alloys hardness high-temperature alloys joinability tensile properties workability DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2010, ASM International®. All rights reserved. Data shown...
Journal Articles
Alloy Digest (2014) 63 (6): Ti-156.
Published: 01 June 2014
... temperature performance and corrosion resistance as well as forming. Filing Code: Ti-156. Producer or source: Timet. Producer or Source: Timet Copyright © ASM International® 2014 2014 ASM International automotive exhaust systems bend strength chemical composition corrosion-resistant alloys...
Journal Articles
Alloy Digest (2013) 62 (9): SS-1157.
Published: 01 September 2013
... for applications like automotive exhaust system components. Ferritic steels are not inherently strong at elevated temperatures, but columbium additions coupled with appropriate solution annealing markedly improve long-time creep rupture strength properties. ATI 441 HP alloy is dual stabilized with columbium...
Journal Articles
Alloy Digest (2001) 50 (9): SS-829.
Published: 01 September 2001
... oxidation resistance for many automotive exhaust system components that are too hot for Type 409. Since oxidation rates are greatly affected by service conditions such as atmo- spheres, thermal cycling, and structural design, laboratory test results should only be used as a guide for estimating service...
Journal Articles
Alloy Digest (1996) 45 (10): SS-658.
Published: 01 October 1996
... stainless has been used extensively in automotive exhaust systems. Producer: Carpenter Technology Corporation Carpenter Steel Division Reading, PA 196124662 (610) 208-2000 SS-658B F-1 EffeuofcoMworkontypialmsilepqxnk ...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1229.
Published: 01 October 2015
... tests DOI: 10.31399/asm.ad.ss1229 Applications: The alloy is used as automotive exhaust systems for boilers burning S-containing fuels, etc., sulfur production equipment, exhaust gas desulfurizers, and smokestack/ flue lining. Producer: Nippon Steel and Sumitomo Metal Chicago, IL 60611, USA Tel: (312...
Journal Articles
Alloy Digest (2003) 52 (10): Ni-615.
Published: 01 October 2003
... is a bare solid wire for metal inert gas (MIG) or gas metal arc welding (GMAW) and for tungsten inert gas (TIG) or gas tungsten arc welding (GTAW). The alloy was developed, following the success of NI-ROD Filler Metal 44, for use in automotive exhaust systems, principally in joining catalytic converters...
Journal Articles
Alloy Digest (2016) 65 (4): SS-1244.
Published: 01 April 2016
.... These characteristics make the ATI 436S alloy an excellent candidate for use in automotive exhaust systems as well as other applications where resistance to chlorides and mild corrosives, combined with fabricability, are needed. Product Forms Available: Plates, sheets, and strip Applications: Applications include...
Journal Articles
Alloy Digest (2015) 64 (7): SS-1216.
Published: 01 July 2015
.... See Fig. 3 for available size. Applications: The alloy is used as automotive exhaust systems, high- temperature heated locations, and hot water supply parts. Producer: Nippon Steel and Sumitomo Metal Chicago, IL 60611, USA Tel: (312) 751-0800 Fax: (312) 751-0345 In Japan: Chiyoda-ku, Tokyo 100-871...