1-20 of 221 Search Results for

automotive engines

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1974) 23 (2): SS-291.
Published: 01 February 1974
... MANIFLEX-FM is a free-machining chromium-nickel austenitic stainless steel which offers excellent high-temperature strength and hardness with good corrosion resistance to combustion products. It is widely used exhaust components in automotive engines. This datasheet provides information...
Journal Articles
Alloy Digest (1972) 21 (2): SS-268.
Published: 01 February 1972
... CARPENTER C-XB is a hardenable high-carbon high-silicon high-chromium stainless steel offering good high-temperature strength and corrosion resistance to combustion products of automotive gas engines. It is also available in aircraft quality. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2003) 52 (5): SA-512.
Published: 01 May 2003
... Domex 110XF is a very-high-strength steel that is used for automotive and civil engineering structural components. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1980) 29 (10): SA-377.
Published: 01 October 1980
... Inland INX Steels are a series of balanced composition steels with columbium or vanadium additions; they were developed to provide a choice of mechanical properties and engineering features. They are furnished to minimum yield point levels ranging from 42,000 psi (290 MPa) to 70,000 psi (485 MPa...
Journal Articles
Alloy Digest (1991) 40 (3): Al-313.
Published: 01 March 1991
... transmission components, automotive engine blocks. Producer: Aluminum Smelting and Refining Company, Inc. Certified Alloys Company Maple Heights, Ohio 44 137 ...
Journal Articles
Alloy Digest (2018) 67 (6): SS-1288.
Published: 01 June 2018
... mm (0.16 0.8 in solution annealed; pickled; drawn; straightened; peeled; ground. Applications Typical applications include construction of high temperature components; automotive engineering; chains, screens and mesh; mechanical engineering and furnace engineering. Producer Deutsche Edelstahlwerke...
Journal Articles
Alloy Digest (2007) 56 (7): SS-993.
Published: 01 July 2007
... 500 2000 mm. Applications: The typical fields of application are aeronautical engineering (compressor valves, exhaust components, fasteners), automotive engineering (turbine components, exhaust manifolds), power engineering (turbine components), and the oil and gas industries. The alloy is also used...
Journal Articles
Alloy Digest (2018) 67 (3): SS-1282.
Published: 01 March 2018
... construction of high- temperature components; automotive engineering; chains, screens, and mesh; mechanical engineering; and furnace engineering. Producer Deutsche Edelstahlwerke 58452 Witten, Germany Tel: + 49 (0) 2302 29 0 Fax: +49 (0) 2302 29 4000 www.dew-stahl.com ISSN: 002-614X SS-128B Fig. 2 Temperature...
Journal Articles
Alloy Digest (1971) 20 (8): Al-203.
Published: 01 August 1971
... should be treated with phosphorus to refine the primary silicon phase. Care must be taken to properly control the pouring temperature and rate to minimize primary silicon growth and segregation. Forms Available: 390 Die castings. A390 Sand and permanent mold castings. Applications: Automotive engine...
Journal Articles
Alloy Digest (1979) 28 (5): Al-130.
Published: 01 May 1979
... growth. In general, strength and elongation remain unchanged or improved at low temperatures. The presence of any lead, cadmium or bismuth impairs forgeability. Forms Available: Forgings and forging stock. Applications: Aircraft engine cylinders, heads and pistons. Automotive engine pistons, cylinder...
Journal Articles
Alloy Digest (2006) 55 (6): Ni-638.
Published: 01 June 2006
... application. In all conditions, alloy X-750 is resistant to oxidation up to 980 °C (1800 °F). The most often used heat treatments have been incorporated by the Society of Automotive Engineers in their AMS specifications for various product forms. See Tables 1 and 2. Heat Treatment: See Table 1. Fabricability...
Journal Articles
Alloy Digest (1960) 9 (10): Al-96.
Published: 01 October 1960
... 5,500 p.s.i. at 6OOoF and 11,000 p.s.i. at 4000F. Forms Available: Forgings - T4 and T6 tempers Extrusions - T31 and T81 tempers Sheet and Plate - T31, T81, T37 and T87 tempers Applications: Aircraft and automotive engine parts, special appli- cations in missiles, space vehicles, and ground support...
Journal Articles
Alloy Digest (1977) 26 (1): Ni-239.
Published: 01 January 1977
...- ing. Cast-iron parts with large blow holes or other flaws are easily salvaged through the application of Colmonoy No. 23A. Such repair work is done extensively by found- ries producing automotive engine blocks and other cast- iron parts. These two powders can be applied very quickly by a relatively...
Journal Articles
Alloy Digest (1973) 22 (7): Pb-10.
Published: 01 July 1973
... machinery, car journals; used with all kinds of shafting. Alloy 13: Used for light loads and speeds, car journal bearings. AUoy 15: Used for high loads and speeds, diesel engines, automotive engines, steamships, steel mills and all kinds of machinery. Manufacturer: White metal bearing alloy producers. ...
Journal Articles
Alloy Digest (1999) 48 (2): Al-358.
Published: 01 February 1999
... applications such as space boost- ers and fuel tanks. The alloy is readily weldable. It is useful over a temperature range of 269 to 316 °C ( 452 to 600 °F). The al- loy also has good fracture toughness. The T8 temper is resistant to SCC. Applications: Typical uses include aircraft and automotive engine parts...
Journal Articles
Alloy Digest (2006) 55 (9): SA-556.
Published: 01 September 2006
... Mittal Di-Form T500 is a dual-phase steel intended primarily for exposed outer automotive body panels (door, hoods, and fenders). Dual-phase steels are one of the important advanced high-strength steel products developed for the automotive industry. Their microstructure typically consists...
Journal Articles
Alloy Digest (2020) 69 (2): Al-461.
Published: 01 February 2020
... Alcoa EZCast 370 is a heat-treatable, aluminum-silicon-magnesium-manganese high-pressure die casting (HPDC) alloy which is widely used for thin-walled, crash-resistant, structural components for automotive applications. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1980) 29 (5): SA-372.
Published: 01 May 1980
... REPUBLIC X-80-W is a high-strength, low-alloy steel developed to achieve a minimum yield strength of 80,000 psi in the as-hot-rolled condition. It also exhibits good fatigue performance, good bendability, and good weldability. It is available as bars and can be used in various automotive...
Journal Articles
Alloy Digest (2019) 68 (5): SA-845.
Published: 01 May 2019
... CP-W 1000 is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...
Journal Articles
Alloy Digest (2019) 68 (6): SA-848.
Published: 01 June 2019
... CP-K 570Y780T is one of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...