Alloy Digest (1971) 20 (12): Cu-246.
Published: 01 December 1971
... COMPO H is an oil-impregnated sintered bronze, produced by powder metallurgy techniques, which is widely used in automotive, applicance, farm equipment, and aircraft industry applications. This datasheet provides information on composition, physical properties, tensile properties, and compressive...
Journal Articles
Alloy Digest (2021) 70 (11): Cu-926.
Published: 01 November 2021
... the strength, and improve the softening characteristics. Wieland B31 possesses the right combination of formability, conductivity, strength, and stress relaxation resistance to be used for automotive applications at relatively high ambient temperatures. In addition, its strength is similar to that of a 4% tin...
Journal Articles
Alloy Digest (1976) 25 (2): Al-222.
Published: 01 February 1976
... ALUMINUM 295.0 is an aluminum sand casting alloy suitable for uses requiring high strength with ductility and toughness. It has fair castability, good machinability, and is used for a number of aerospace and automotive applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1981) 30 (9): Ni-270.
Published: 01 September 1981
... electrical device across a fluctuating voltage source. Kanthal 70 has a maximum recommended operating temperature of 600 C and is used widely in resistance thermometers and in various appliance and automotive applications. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (1989) 38 (7): Al-297.
Published: 01 July 1989
... UNS A02950 is an aluminum casting alloy suitable where high strength with ductility and toughness is required. It has fair castablility and good machinability. It is used for aerospace and automotive applications. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1991) 40 (10): Cp-18.
Published: 01 October 1991
... ZYMAXX provides outstanding compressive creep resistance, toughness and chemical inertness at high temperatures and pressures and under adverse conditions. They have a wide range of uses beyond chemical processing, including aerospace and automotive applications, general industrial equipment, home...
Journal Articles
Alloy Digest (1983) 32 (2): Al-244.
Published: 01 February 1983
... is a new high-strength aluminum castingalloy. It providesan optimum combination of strength. light weight and economy. Its performance approaches that of forged steel. yet it may be less expensive to use because its lower tooling costs often offset the price difference. In automotive applications...
Journal Articles
Alloy Digest (2020) 69 (1): Al-460.
Published: 01 January 2020
... Rio Tinto Alloys 206.2, A206.2, and B206.2 are heat-treatable, aluminum-copper-magnesium casting alloys in ingot form for remelting. These alloys are primarily intended for producing sand and permanent mold castings for aerospace and automotive applications. This datasheet provides information...
Journal Articles
Alloy Digest (2020) 69 (2): Al-461.
Published: 01 February 2020
... Alcoa EZCast 370 is a heat-treatable, aluminum-silicon-magnesium-manganese high-pressure die casting (HPDC) alloy which is widely used for thin-walled, crash-resistant, structural components for automotive applications. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2004) 53 (3): SA-532.
Published: 01 March 2004
... DUAL-TEN 590 (UTS 590 MPa, or 86 ksi) is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional HSLA steels. They offer a great opportunity for part weight reduction. The improved formability...
Journal Articles
Alloy Digest (2004) 53 (2): SA-530.
Published: 01 February 2004
... DUAL-TEN 500 (UTS 500 MPa, or 73 ksi) is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional HSLA steels. They offer a great opportunity for part weight reduction. The improved formability...
Journal Articles
Alloy Digest (2004) 53 (4): SA-533.
Published: 01 April 2004
... DUAL-TEN 600 is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional high-strength low-alloy (HSLA) steels. Applications include front and rear rails, crush cans, rocker reinforcements, pillar...
Journal Articles
Alloy Digest (2004) 53 (5): SA-535.
Published: 01 May 2004
... DUAL-TEN 780 (UTS 780 MPa, or 113 ksi) is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional high-strength low-alloy (HSLA) steels. Applications include front and rear rails, crush cans...
Journal Articles
Alloy Digest (2010) 59 (8): Cu-786.
Published: 01 August 2010
... PMX alloy C15100 is a high performance alloy with improved stress relaxation so it can be used reliably at 65 deg C (150 deg F) for automotive and electrical applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend...
Journal Articles
Alloy Digest (1980) 29 (5): SA-372.
Published: 01 May 1980
...: Republic Steel Corporation. Producer or Source: Republic Steel Corporation Copyright © ASM International® 1996 1996 ASM International automotive applications bend strength chemical composition corrosion-resistant alloys elasticity heat treatability joinability machinability physical...
Journal Articles
Alloy Digest (2011) 60 (10): Mg-78.
Published: 01 October 2011
... ELEKTRON AZ31B is a wrought magnesium alloy developed to offer good properties maintaining corrosion resistance and weldability. The alloy is used in aerospace, automotive, and military applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1974) 23 (11): Al-210.
Published: 01 November 1974
... FEDERATED F410 is a heat-treatable aluminum sand casting alloy recommended for uses requiring high strength along with toughness and ductility. It has good machinability, fair castability, and is suitable for a number of automotive and aerospace applications. This datasheet provides information...
Journal Articles
Alloy Digest (2009) 58 (6): Fe-148.
Published: 01 June 2009
... Carpenter AerMet 340 Alloy possesses high hardness and strength while exhibiting exceptional toughness and ductility, and can be considered for a variety of automotive, racing, aerospace, and defense applications. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1988) 37 (7): Al-282.
Published: 01 July 1988
... Alcoa Aluminum Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy. It is available in five tempers. It is crossing many market areas of applications in aerospace, defense, automotive and general structural use. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1980) 29 (5): Cu-395.
Published: 01 May 1980
... for artillery and small-arms cartridge cases. It offers excellent-to-good resistance to corrosion in most environments. Its many uses include architectural, automotive, electrical, hardware, industrial, munitions, plumbing and wire applications. This datasheet provides information on composition, physical...