1-20 of 66 Search Results for

automobile industry

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2004) 53 (9): Cu-723.
Published: 01 September 2004
... Wieland-S12 has good cold working properties. Spring properties are higher than phosphor bronzes and stress-corrosion cracking (SCC) sensitivity is lower than that of copper-zinc alloys. Applications include connectors in the automobile industry. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2006) 55 (4): SS-959.
Published: 01 April 2006
... Nirosta H400 is an ultrahigh-strength stainless steel that has an unstable austenitic microstructure which work hardens to martensite. The alloy was developed for volume production in the automobile industry primarily for weight reduction. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1975) 24 (9): SA-319.
Published: 01 September 1975
... SAE 4032 is an alloy steel used extensively in the automobile industry. It combines moderate strength with good toughness in the quenched and tempered condition because it is relatively free from temper embrittlement when tempered in the range 850-1100 F. This datasheet provides information...
Journal Articles
Alloy Digest (1981) 30 (4): Fe-62.
Published: 01 April 1981
... in 100-ton heats to insure high quality and uniformity. Its applications include semi-conductor lead frames, sealed-beam automobile headlamps and industrial lamps. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion...
Journal Articles
Alloy Digest (1979) 28 (10): Fe-59.
Published: 01 October 1979
.... It is made under strict metallurgical control to provide uniformity of performance. Among its uses are sealed-beam automobile headlamps, ceramic-to-glass seals and industrial lamps. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1982) 31 (8): Fe-66.
Published: 01 August 1982
... control to provide uniformity of performance. Its many uses include industrial lamps, ceramic-to-glass seals, and sealed-beam automobile headlamps. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1984) 33 (7): Cu-480.
Published: 01 July 1984
... popular in the electronics industry. This alloy, in contrast to the beryllium copper alloys, costs less and causes less environmental problems. Its uses include electronic switch terminals, television remote controls and automobile telephones. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1996) 45 (1): SS-631.
Published: 01 January 1996
.... sinks. washing machines and kitchen appliances. in inte- rior decorating. in the automobile industry and for non-welded parts in industrial canteens. spip Sbrcr l5mimamwidul max.* -Lnslb - - - mm 20.40 1ooll ml0 Moo 2050 1250 1250 4ooo 20.60 1250 12% 4ooo 20.70 1524 1.524 6ooo >I.MS.CO 1524 1524 13.ooo...
Journal Articles
Alloy Digest (1996) 45 (4): SS-642.
Published: 01 April 1996
...-6.00 1524 1.524 13.aa so.70 I524 1.524 6.MN Applications: Due to its good resistance to corrosion. good cold workability, and good weldability. this steel is widely used for household goods. dishwashers, cutlery, in the consumer goods industry, in architecture, in the automobile industry. etc...
Journal Articles
Alloy Digest (2013) 62 (10): SS-1159.
Published: 01 October 2013
.... Characterization of magnetic steels is performed through permeameters and coercimeters. MG1 is the best known and most widely used in the automobile industry as well as household appliances. Machinability is reduced when compared to unannealed bars after cold drawing. However, there is no wide gap between the two...
Journal Articles
Alloy Digest (2021) 70 (4): Ni-769.
Published: 01 April 2021
... 31.9 610 88.5 55 1000 1832 65 180 26.1 530 76.9 165 23.9 470 68.2 protection facilities, in the automobile industry, and in power plants. Typical applications include: (a) Trays, baskets 110 16.0 270 39.2 and fixtures for heat treatment plants, e. g., in carburizing or carbonitriding environments; (b...
Journal Articles
Alloy Digest (1975) 24 (1): SA-312.
Published: 01 January 1975
... to 0.312~in. thick. Applications: Component parts for automobiles, industrial equipment. farm machinery. material handling equipment. trucks. buses. and construction equipment. Any parts requiring high strength which must be bent or formed in more than one direction can use the advantages of Maxi-Form 80...
Journal Articles
Alloy Digest (1998) 47 (5): SS-718.
Published: 01 May 1998
.... and the automobile industry. UGIMA 4301 is also used for the construction of apparatus and contain- ers in the dairy, beer. wine, and food indusrries. and in the Production of niungen compounds. Producer: Producer in France: Distribumr in USA: Ugine-Savoie ugitte stainless & Alloys 73403 Ugine Cedex Cohar. PA 18915...
Journal Articles
Alloy Digest (1972) 21 (4): SS-270.
Published: 01 April 1972
... ALLEGHENY LUDLUM MF-2 is a 12% chromium steel that was developed initially for use in automobile exhaust systems. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance...
Journal Articles
Alloy Digest (1971) 20 (11): SS-263.
Published: 01 November 1971
... was developed to withstand the strong acid concentrates that form in automobile mufflers and tailpipes and has proved much superior to carbon steel in this service. It is also resistant to hard natural waters and polhrted river waters. It is superficially stained and may be pitted in urban and industrial...
Journal Articles
Alloy Digest (1980) 29 (1): Al-161.
Published: 01 January 1980
... for automobiles, trucks, appliances and other industrial products. This alloy can be bright dipped or anodized to give a bright, clear finish. Manufacturers: Aluminwn alloy mins. ...
Journal Articles
Alloy Digest (1978) 27 (12): SA-352.
Published: 01 December 1978
... Corporation Copyright ┬ę ASM International┬« 1996 1996 ASM International automobile applications chemical composition corrosion-resistant alloys ductility farm equipment hardness heat treatability joinability machinability microstructure tensile properties USS DUAL PHASE 80 weldability...
Journal Articles
Alloy Digest (1996) 45 (10): SS-658.
Published: 01 October 1996
... Carpenter Type 409Cb stainless steel is a 11% Cr steel stabilized with columbium (niobium). The alloy is used extensively in automobile exhast systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1966) 15 (8): SA-199.
Published: 01 August 1966
... AW-TEN is a high-strength structural steel offering 50,000 psi minimum yield strength, good formability and weldability, and superior corrosion resistance. It is intended primarily for weight reduction and longer service life. It is recommended for automobile and truck bodies, buildings, bridges...
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... range of sizes-l/2 through 60 . Applications: Bright trim for automobiles, cameras, vending machines, wunters and showcases, electrical appliances, finiShed hard- ware and moldings for architectural use and a host of other industrial and household equipment. Because of its excellent resistance...