Skip Nav Destination
Close Modal
Search Results for
automobile applications
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 157
Search Results for automobile applications
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
REMANIT 4512: Ferritic Stainless Steel with Titanium
Available to Purchase
Alloy Digest (1997) 46 (7): SS-691.
Published: 01 July 1997
... Remanit 4512 is a ferritic stainless steel with titanium added to improve high-temperature corrosion resistance. Applications include silencers and exhaust emission-control systems in automobiles. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Abstract
View articletitled, REMANIT 4512: Ferritic Stainless Steel with Titanium
View
PDF
for article titled, REMANIT 4512: Ferritic Stainless Steel with Titanium
Remanit 4512 is a ferritic stainless steel with titanium added to improve high-temperature corrosion resistance. Applications include silencers and exhaust emission-control systems in automobiles. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: SS-691. Producer or source: Thyssen Stahl AG.
Journal Articles
CARPENTER STAINLESS TYPE 430: Corrosion and Heat Resistant Ferritic Stainless Steel
Available to Purchase
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... 1995. Producer or Source: Carpenter Copyright © ASM International® 1996 1996 ASM International automobile applications builders hardware CARPENTER STAINLESS TYPE 430 chemical composition corrosion-resistant alloys decorative trim deformation properties ductility elasticity...
Abstract
View articletitled, CARPENTER STAINLESS TYPE 430: Corrosion and Heat Resistant Ferritic Stainless Steel
View
PDF
for article titled, CARPENTER STAINLESS TYPE 430: Corrosion and Heat Resistant Ferritic Stainless Steel
CARPENTER STAINLESS TYPE 430 is a chromium stainless steel that is especially useful for all types of decorative trim. This steel is suitable for trim on automobiles, cameras, vending machines, counters and showcases, electrical appliances and finished hardware in the building trade. The alloy also has many applications in both the petrochemical and chemical area. Type 430 has moderate strength and good ductility. It can be cold worked readily for producing trim and can be joined successfully by several methods. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, and deformation. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-384. Producer or source: Carpenter. Originally published March 1981, revised April 1995.
Journal Articles
A-L 42: Controlled Expansion Alloy
Available to Purchase
Alloy Digest (1981) 30 (4): Fe-62.
Published: 01 April 1981
... in 100-ton heats to insure high quality and uniformity. Its applications include semi-conductor lead frames, sealed-beam automobile headlamps and industrial lamps. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion...
Abstract
View articletitled, A-L 42: Controlled Expansion Alloy
View
PDF
for article titled, A-L 42: Controlled Expansion Alloy
A-L 42 is intended as a controlled-expansion alloy for applications in the electronics and electrical industries. It is used in conjunction with certain glass (0120, 0010, 1075, etc.) and other nonmetallic materials in sealing applications. A-L 42 is AOD (Argon Oxygen Decarburization) refined in 100-ton heats to insure high quality and uniformity. Its applications include semi-conductor lead frames, sealed-beam automobile headlamps and industrial lamps. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-62. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
CARPENTER 21-55N: Valve Steel
Available to Purchase
Alloy Digest (1966) 15 (1): SS-176.
Published: 01 January 1966
... temperature strength and corrosion resistance for exhaust valve applications. It is widely used as the head material in two-piece valves for internal combustion engines. It is also finding increasing use for one-piece valves in automobile engines. Composition: Carbon Manganese Silicon Chromium Nickel Nitrogen...
Abstract
View articletitled, CARPENTER 21-55N: Valve Steel
View
PDF
for article titled, CARPENTER 21-55N: Valve Steel
Carpenter 21-55N Valve Steel is an austenitic nitrogen-bearing chromium-nickel-manganese alloy which offers an excellent combination of high temperature strength and corrosion resistance for exhaust valve applications. It is widely used as the head material in two-piece valves for internal combustion engines. It is also finding increasing use for one-piece valves in automobile engines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-176. Producer or source: Carpenter.
Journal Articles
42 NICKEL-IRON ALLOY: Controlled Expansion Alloy
Available to Purchase
Alloy Digest (1982) 31 (8): Fe-66.
Published: 01 August 1982
..., joining of glass sealing. Forms Available: Bar, sheet, strip and wire. Applications: The 42 Nickel-Iron Alloy is used for sealed-beam automobile headlamps, semi-conductor head frames, glass-to-metal seals in electronic tubes, industrial lamps, ceramic-to-glass seals, and transformer and capacitor bushings...
Abstract
View articletitled, 42 NICKEL-IRON ALLOY: Controlled Expansion Alloy
View
PDF
for article titled, 42 NICKEL-IRON ALLOY: Controlled Expansion Alloy
The 42 Nickel-Iron alloy has the lowest expansivity of the Iron-Nickel alloys that are commonly used for glass-sealing applications. Its thermal expansion closely matches the 1075 glass and it is sometimes used for sealing action with the 0120 and 0010 glasses. It is made close metallurgical control to provide uniformity of performance. Its many uses include industrial lamps, ceramic-to-glass seals, and sealed-beam automobile headlamps. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-66. Producer or source: Iron-nickel alloy mills.
Journal Articles
ALUMINUM A413.0: Die Casting Alloy
Available to Purchase
Alloy Digest (1984) 33 (5): Al-251.
Published: 01 May 1984
... ductility; and increasing silicon content may lead to machining problems. Forms Available: Die castings and ingots. Applications: Aluminum A413.0 is used for miscellaneous thin- walled and intricately designed die castings, motor housings. meter cases, switch boxes, manifolds and automobile fittings...
Abstract
View articletitled, ALUMINUM A413.0: Die Casting Alloy
View
PDF
for article titled, ALUMINUM A413.0: Die Casting Alloy
ALUMINUM A413.0 is a high-silicon (nominally 12%), aluminum-base alloy. It is recommended for applications where excellent castability and resistance to corrosion are required. Typical uses comprise miscellaneous thin-walled and intricately designed castings for such items as meter cases and automobile fittings. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-251. Producer or source: Various aluminum companies.
Journal Articles
AISI 1010: Low Carbon Steel
Available to Purchase
Alloy Digest (1985) 34 (5): CS-106.
Published: 01 May 1985
... for structural shapes and carburized parts. Among its many applications are bushings. clutch discs, flanges, thrust washers. tinplate. nails. rivets. automobile bodies and fenders. pans and transmission covers. Composition: Carbon Manganese Phosphorus Sulfur Silicon Iron 0.08-o. I3 0.30-0.60 0.040 max. 0.050 max...
Abstract
View articletitled, AISI 1010: Low Carbon Steel
View
PDF
for article titled, AISI 1010: Low Carbon Steel
AISI 1010 is a low-carbon steel having good formability and weldability. It is recommended for sheet stock for deep-drawing operations and in sheet and stock for structural shapes and carburized parts. Among its many applications are bushings, clutch discs, flanges, thrust washers, tinplate, nails, rivets, automobile bodies and fenders, pans and transmission covers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-106. Producer or source: Carbon steel mills.
Journal Articles
ALUCHROM I SE: Oxidation Resistant Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2001) 50 (5): SS-823.
Published: 01 May 2001
... Aluchrom I SE is an oxidation resistant ferritic stainless steel alloyed with aluminum and rare earth elements. Applications include framework for catalytic automobile muffler systems. This datasheet provides information on composition, physical properties, and tensile properties as well as creep...
Abstract
View articletitled, ALUCHROM I SE: Oxidation Resistant Ferritic Stainless Steel
View
PDF
for article titled, ALUCHROM I SE: Oxidation Resistant Ferritic Stainless Steel
Aluchrom I SE is an oxidation resistant ferritic stainless steel alloyed with aluminum and rare earth elements. Applications include framework for catalytic automobile muffler systems. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-823. Producer or source: Krupp VDM.
Journal Articles
TECHALLOY GLASSEAL 42: Controlled Expansion Alloy
Available to Purchase
Alloy Digest (1979) 28 (10): Fe-59.
Published: 01 October 1979
... used for sealing action for the 0120 and 0010 glasses. It has the lowest expansivity of the iron-nickel alloys that are commonly used for glass-sealing applications. It is made under strict metallurgical control to provide uniformity of performance. Among its uses are sealed-beam automobile headlamps...
Abstract
View articletitled, TECHALLOY GLASSEAL 42: Controlled Expansion Alloy
View
PDF
for article titled, TECHALLOY GLASSEAL 42: Controlled Expansion Alloy
TECHALLOY GLASSEAL 42 is an iron-nickel alloy with thermal expansion that closely matches the 1075 glass. Also, it is sometimes used for sealing action for the 0120 and 0010 glasses. It has the lowest expansivity of the iron-nickel alloys that are commonly used for glass-sealing applications. It is made under strict metallurgical control to provide uniformity of performance. Among its uses are sealed-beam automobile headlamps, ceramic-to-glass seals and industrial lamps. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-59. Producer or source: Techalloy Company Inc..
Journal Articles
WIELAND-S12: Tin Brass
Available to Purchase
Alloy Digest (2004) 53 (9): Cu-723.
Published: 01 September 2004
... Wieland-S12 has good cold working properties. Spring properties are higher than phosphor bronzes and stress-corrosion cracking (SCC) sensitivity is lower than that of copper-zinc alloys. Applications include connectors in the automobile industry. This datasheet provides information on composition...
Abstract
View articletitled, WIELAND-S12: Tin Brass
View
PDF
for article titled, WIELAND-S12: Tin Brass
Wieland-S12 has good cold working properties. Spring properties are higher than phosphor bronzes and stress-corrosion cracking (SCC) sensitivity is lower than that of copper-zinc alloys. Applications include connectors in the automobile industry. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-723. Producer or source: Wieland Metals Inc., Wieland-Werke AG.
Journal Articles
JLX - 50CC: High Strength Low Alloy Construction Steel
Available to Purchase
Alloy Digest (1968) 17 (5): SA-226.
Published: 01 May 1968
... or Source: Jones & Laughlin Steel Corporation Copyright © ASM International® 1996 1996 ASM International automobile applications chemical composition corrosion-resistant alloys elasticity fatigue properties formability fracture toughness hardness heat treatability JLX-50CC...
Abstract
View articletitled, JLX - 50CC: High Strength Low Alloy Construction Steel
View
PDF
for article titled, JLX - 50CC: High Strength Low Alloy Construction Steel
JLX-50CC is a high-strength columbium steel designed for ease of fabrication. It has good formability, weldability, and toughness. It is recommended for mining equipment, automobile and truck bodies, trailers and similar construction. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-226. Producer or source: Jones & Laughlin Steel Corporation.
Journal Articles
USS DUAL PHASE 80: Specially Heat Treated High-Strength Steel
Available to Purchase
Alloy Digest (1978) 27 (12): SA-352.
Published: 01 December 1978
... Corporation Copyright © ASM International® 1996 1996 ASM International automobile applications chemical composition corrosion-resistant alloys ductility farm equipment hardness heat treatability joinability machinability microstructure tensile properties USS DUAL PHASE 80 weldability...
Abstract
View articletitled, USS DUAL PHASE 80: Specially Heat Treated High-Strength Steel
View
PDF
for article titled, USS DUAL PHASE 80: Specially Heat Treated High-Strength Steel
USS Dual Phase 80 is a high-strength steel sheet which has a dual phase structure of martensite and ferrite. It provides all the benefits of higher strength with little sacrifice in ductility, formability or weldability. Dual Phase 80 gains strength as it is formed through rapid work hardening of its unique microstructure; in fact, it increases from its delivered yield strength of 50,000 psi up to 80,000 psi (or more) in forming. Its final strength depends on the amount of forming. Its many applications include automotive vehicles, farm equipment and heavy construction equipment. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-352. Producer or source: United States Steel Corporation.
Journal Articles
TIMETAL 550: Forgeable Alpha Beta Alloy
Available to Purchase
Alloy Digest (1998) 47 (7): Ti-112.
Published: 01 July 1998
... automobile applications chemical composition creep properties fatigue properties fracture toughness heat treatability high-temperature alloys joinability physical properties tensile properties TIMETAL 550 thermal properties DATA ON WORLD WIDE METALS AND ALLOYS TIMETAL 550 (Forgeable Alpha Beta...
Abstract
View articletitled, TIMETAL 550: Forgeable Alpha Beta Alloy
View
PDF
for article titled, TIMETAL 550: Forgeable Alpha Beta Alloy
TIMETAL 550 is a medium strength forgeable alpha beta alloy for applications in the aerospace and automotive industries. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance as well as heat treating and joining. Filing Code: TI-112. Producer or source: Titanium Metals Corporation (Timet).
Journal Articles
BRUSHFORM 65: Beryllium-Nickel-Copper Alloy
Available to Purchase
Alloy Digest (2013) 62 (6): Cu-821.
Published: 01 June 2013
.... Producer or Source: Materion Brush Performance Alloys Copyright © ASM International® 2013 2013 ASM International appliances automobile applications BRUSHFORM 65 chemical composition computer power applications elasticity fatigue properties hardness physical properties reliability...
Abstract
View articletitled, BRUSHFORM 65: Beryllium-Nickel-Copper Alloy
View
PDF
for article titled, BRUSHFORM 65: Beryllium-Nickel-Copper Alloy
BrushForm 65 is designed for both superior performance and high reliability in appliance, automotive, and computer power applications. Alloy BF-65’s combination of properties limits power loss at the contact interface, controls temperature rise from resistive heating, and provides stable contact force at temperatures to 200 C (390 F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on forming. Filing Code: Cu-821. Producer or source: Materion Brush Performance Alloys.
Journal Articles
DOCOL 1800 BOR: Hardenable Boron Steel
Available to Purchase
Alloy Digest (2014) 63 (2): SA-692.
Published: 01 February 2014
... Steel Inc.. Producer or Source: SSAB Swedish Steel Inc. Copyright © ASM International® 2014 2014 ASM International automobile applications chemical composition DOCOL 1800 BOR joinability physical properties tensile properties workability DATA ON WORLDWIDE METALS AND ALLOYS...
Abstract
View articletitled, DOCOL 1800 BOR: Hardenable Boron Steel
View
PDF
for article titled, DOCOL 1800 BOR: Hardenable Boron Steel
Docol 1800 Bor is a hardenable boron steel for the automotive industry. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, joining, and surface treatment. Filing Code: SA-692. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
DOCOL 1500 BOR: Hardenable Boron Steel
Available to Purchase
Alloy Digest (2014) 63 (11): SA-713.
Published: 01 November 2014
... Steel Inc.. Producer or Source: SSAB Swedish Steel Inc. Copyright © ASM International® 2014 2014 ASM International automobile applications chemical composition Docol 1500 Bor joinability physical properties tensile properties workability DATA ON WORLDWIDE METALS AND ALLOYS...
Abstract
View articletitled, DOCOL 1500 BOR: Hardenable Boron Steel
View
PDF
for article titled, DOCOL 1500 BOR: Hardenable Boron Steel
Docol 1500 Bor is a hardenable boron steel for the automotive industry. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, joining, and surface treatment. Filing Code: SA-713. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
KANTHAL 70: Nickel Iron Alloy
Available to Purchase
Alloy Digest (1981) 30 (9): Ni-270.
Published: 01 September 1981
... automobile applications chemical composition corrosion-resistant alloys electrical resistance electrical resistivity heat treatability joinability KANTHAL 70 physical properties resistance thermometers tensile properties workability 1 Filing Code: Ni-270 KANTHAL 70 Nickel Alloy 08 SEPTEMBER...
Abstract
View articletitled, KANTHAL 70: Nickel Iron Alloy
View
PDF
for article titled, KANTHAL 70: Nickel Iron Alloy
KANTHAL 70 alloy was designed to provide a high positive temperature coefficient to electrical resistance comparable with that of pure nickel; however, it has much higher electrical resistivity than pure nickel. This makes it useful as a voltage regulator when placed in series with another electrical device across a fluctuating voltage source. Kanthal 70 has a maximum recommended operating temperature of 600 C and is used widely in resistance thermometers and in various appliance and automotive applications. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-270. Producer or source: The Kanthal Corporation.
Journal Articles
SAE 4032: Molybdenum Alloy Steel
Available to Purchase
Alloy Digest (1975) 24 (9): SA-319.
Published: 01 September 1975
...: Alloy steel mills and foundries Copyright © ASM International® 1996 1996 ASM International automobile applications chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability physical properties SAE 4032 tensile properties...
Abstract
View articletitled, SAE 4032: Molybdenum Alloy Steel
View
PDF
for article titled, SAE 4032: Molybdenum Alloy Steel
SAE 4032 is an alloy steel used extensively in the automobile industry. It combines moderate strength with good toughness in the quenched and tempered condition because it is relatively free from temper embrittlement when tempered in the range 850-1100 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-319. Producer or source: Alloy steel mills and foundries.
Journal Articles
ALUMINUM 5657: Bright, Corrosion Resistant Wrought Alloy
Available to Purchase
Alloy Digest (1980) 29 (8): Al-178.
Published: 01 August 1980
... published August 1968, revised August 1980. Producer or Source: Various aluminum companies Copyright © ASM International® 1996 1996 ASM International ALUMINUM 5657 appliance trim automobile applications chemical composition corrosion-resistant alloys elasticity hardness heat treatability...
Abstract
View articletitled, ALUMINUM 5657: Bright, Corrosion Resistant Wrought Alloy
View
PDF
for article titled, ALUMINUM 5657: Bright, Corrosion Resistant Wrought Alloy
ALUMINUM 5657 is an aluminum-base, wrought, non-heat-treatable alloy of high purity and bright appearance. It has high resistance to general corrosion and to stress-corrosion cracking. It is used widely in the anodized condition for automotive and appliance trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-178. Producer or source: Various aluminum companies. Originally published August 1968, revised August 1980.
Journal Articles
ALUMINUM 5252: Non Heat Treatable Wrought Alloy
Available to Purchase
Alloy Digest (1980) 29 (1): Al-161.
Published: 01 January 1980
... or source: Various aluminum companies. Originally published December 1966, revised January 1980. Producer or Source: Various aluminum companies Copyright © ASM International® 1996 1996 ASM International ALUMINUM 5252 automobile applications chemical composition corrosion-resistant alloys...
Abstract
View articletitled, ALUMINUM 5252: Non Heat Treatable Wrought Alloy
View
PDF
for article titled, ALUMINUM 5252: Non Heat Treatable Wrought Alloy
ALUMINUM 5252 is a high-purity aluminum-magnesium alloy of moderate strength, good fabricating characteristics and excellent resistance to corrosion. It is highly resistant to denting and is used widely as trim in the automotive industry and for a wide variety of other industrial products. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-161. Producer or source: Various aluminum companies. Originally published December 1966, revised January 1980.