Alloy Digest (1997) 46 (1): SS-667.
Published: 01 January 1997
... AL Tech 416 EZR is one variation of AISI Type 416, the free-machining martensitic stainless steel that has been one of the staples of the automatic machining industry. It offers higher machinability than Type 416 EZ (Alloy Digest SS-665, December 1996), but is not recommended for bright hardening...
Journal Articles
Alloy Digest (1996) 45 (12): SS-665.
Published: 01 December 1996
... Al Tech 416 EZ is one variation of AISI Type 416, the free-machining martensitic stainless steel that has been one of the staples of the automatic machining industry. It offers higher hardenability than other AL Tech variations, but does not machine as readily as them. This datasheet provides...
Journal Articles
Alloy Digest (2021) 70 (7): SS-1337.
Published: 01 July 2021
... on automatic screw machines at about 70% of the speed of SAE 1212. This sulfur modification has led to widespread acceptance and use of this grade in the screw machine industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1990) 39 (12): Cu-556.
Published: 01 December 1990
... Copper alloy C32000 is a leaded red brass applicable to automatic screw machine production of parts for hardware and industrial applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue...
Journal Articles
Alloy Digest (1997) 46 (2): SS-670.
Published: 01 February 1997
... of the automatic machining industry. This specialty steel, available since the 1930s has been used to manufacture an almost countless variety of consumer, automotive, industrial, and militaq hardware. The technology of stainless steels and espe- cially knowledge about the factors that influence machinability have...
Journal Articles
Alloy Digest (1996) 45 (4): Ni-507.
Published: 01 April 1996
...- mum. The preheating temperature should be above 600°F (3 WC). General Characteristics: NI-Rod Filler Metal 99 is a solid wire of commercially pure (99.6 nickel developed for the cast iron industry for the purpose of making easily machined weld deposits on cast iron products, as well as repair welds...
Journal Articles
Alloy Digest (1953) 2 (6): Cu-9.
Published: 01 June 1953
... REVERE No. 240 is a highly leaded brass combining free-machining characteristics with good mechanical and corrosion resistant properties suited to high-speed production in automatic screw machines. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1963) 12 (2): Ni-79.
Published: 01 February 1963
... MONEL alloy R-405 is a machining grade of nickel-copper alloy that combines toughness, strength and corrosion resistance of MONEL alloy 400 with excellent machinability. The alloy is designed especially for use in automatic screw machines. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2005) 54 (6): SA-544.
Published: 01 June 2005
..., machining, and joining. Filing Code: SA-544. Producer or source: Ovako Steel Inc. Producer or Source: Ovako Steel Inc. Copyright © ASM International® 2005 2005 ASM International chemical composition hardness hydraulic industry joinability machinability Ovahyd 450 tensile properties...
Journal Articles
Alloy Digest (2005) 54 (11): SS-946.
Published: 01 November 2005
... surgical needles. It is also used within the automotive industry for critical applications. Producer: Sandvik Steel Co. Scranton, PA 18501-1220 (570) 585-7511 (570) 585-7513 (fax) In Sweden: Sandvik AB Sandviken 46 26 26 30 00 46 26 25 17 10 (fax) www.sandvik.com ISSN: 002-614X SS-946B Table 3 Machining...
Journal Articles
Alloy Digest (1982) 31 (11): Cu-447.
Published: 01 November 1982
... such as gears and pinions where excellent machinability is a prime factor as well as for all types of automatic high-speed screw-machine products for every use. Manufacturer: Anaconda Industries American Brass/Magnet Wire Rolling Meadows. Illinois 60008. ...
Journal Articles
Alloy Digest (1966) 15 (7): Ni-114.
Published: 01 July 1966
... re- sistance from room temperature to operating temperatures of 1000oF. As a casting alloy, easily cast to size and machined by cooveational methods, Brush M220C is of interest to the tool designer and engineer, particularly in the glass industry. In glass forming operation an oxide surface film...
Journal Articles
Alloy Digest (2002) 51 (6): Cu-683.
Published: 01 June 2002
..., and automatic screw machine parts that need more severe cold working than can be tolerated with free-cutting brass processes such as knurling, crimping, and thread rolling. Producer: Swissmetal Metalworks Ltd, Plant Boillat CH-2732 Reconvilier, Switzerland +41-32 482 0 482 +41-32 482 0 116 (fax...
Journal Articles
Alloy Digest (1977) 26 (4): Cu-330.
Published: 01 April 1977
... properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-330. Producer or source: NL Industries Inc., Bearing Division. Producer or Source: NL Industries Inc., Bearing...
Journal Articles
Alloy Digest (1983) 32 (8): SA-392.
Published: 01 August 1983
... TRI-MARK TM-115 is a gas-shielded flux-cored welding electrode for continuous high deposition are welding. It is designed specifically for semiautomatic and automatic arc welding of high-strength low-alloy steels and quenched-and-tempered steels. This gas-sheilded tubular wire can be used...
Journal Articles
Alloy Digest (1973) 22 (8): Cu-269.
Published: 01 August 1973
... in a wide variety of automotive and industrial equipment. The Bunting Brass and Brow Company A subsidiary of National Lead Industries, Inc. Toledo, Ohio 43601. A light mineral oil, frequently called paraffin oil, is used in large quantities on automatic and hand screw machines and is directed...
Journal Articles
Alloy Digest (1978) 27 (3): Cu-350.
Published: 01 March 1978
... paraffin oil, is used in large quantities on automatic and hand screw machines and is directed at the cutting edge of the tools. A cutting compound with good cooling properties, consisting of 20 parts water to 1 part soluble oil, may also be used. Do not use cutting compound when hand reaming. Castability...
Journal Articles
Alloy Digest (2005) 54 (7): Ti-136.
Published: 01 July 2005
... Allvac Ti-15Mo is a metastable beta alloy melted in a vacuum arc remelting (VAR) furnace to minimize segregation. The alloy has a unique combination of properties and is used in the medical, chemical, and aerospace industries. This datasheet provides information on composition. Filing Code: TI-136...
Journal Articles
Alloy Digest (2020) 69 (3): TS-788.
Published: 01 March 2020
... abrasive ceramic materials, liner plates for the brick industry and for making refractories, press tools for the pharmaceutical industry, automatic lathe guide sleeves, guide bars in centerless grinding machines, cone pulleys and rings for wire drawing machines, sandblast nozzles, and tools for the powder...
Journal Articles
Alloy Digest (2012) 61 (2): SA-644.
Published: 01 February 2012
... characteristics), this alloy is easy to machine, to bend, and to weld, which simplifies production and maintenance. Available Products: Quarter plate to 125 mm (4.9 in See Table 3. Applications: Applications include cranes, mobile cranes, trailers, bulldozers, loaders, industrial trucks, buckets, pipes, bridges...