1-20 of 26

Search Results for armatures

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1986) 35 (12): Fe-74.
Published: 01 December 1986
... such as solenoid switches, armatures, pole pieces, relays and cores. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-74...
Journal Articles
Alloy Digest (1968) 17 (11): Fe-36.
Published: 01 November 1968
... Silicon Core Iron is a low carbon silicon electric furnace melted iron recommended for direct current and alternating current magnetic applications in solenoids, armatures and other flux carrying parts operating at high saturations. It is furnished in five grades: A, A-FM, B, B-FM, and C...
Journal Articles
Alloy Digest (1992) 41 (4): Fe-97.
Published: 01 April 1992
... in the part. In an actual relay, a low value of coercive force and a high permeability will enable an air gap to lower the effective residual magnetism to the very low levels de- sired to avoid sticking of the relay armature in the closed position when the magnetizing current is reduced to a low value...
Journal Articles
Alloy Digest (1969) 18 (10): Fe-39.
Published: 01 October 1969
... and permeability at high flux level. Forms Available: Bar, wire, strip and ribbon. Applications: Terminal bands in vitreous enameled resistors, cores and armatures for relays, motors, inductors, transformers. Manufacturer: Wilbur B. Driver Co. Newark. New Jersey ...
Journal Articles
Alloy Digest (2010) 59 (10): CS-158.
Published: 01 October 2010
... are ventilation, lightning, armatures and pressed details in the automotive industry. Table 2 Coating thickness with spot tests Weight determination on two sides, min Weight class Coating thickness per side, µm Triple spot test, g/m2 Single test, g/m2 Z100 7 100 85 Z120 8 120 100 Z140 10 140 120 Z200 14 200 170...
Journal Articles
Alloy Digest (1971) 20 (7): Cu-236.
Published: 01 July 1971
... and product applications. It has exccllcnt cold-forming characteristics and can bc brazed in a reducing atmosphere without danger of cmbrittlement. Forms Available: Sheet and strip. Applications: Vacuum tube anodes, busbars, connectors. armature windings, transformer windings, hollow conductors, coasial...
Journal Articles
Alloy Digest (1957) 6 (4): Fe-13.
Published: 01 April 1957
... cumulative reductions in weight and consequent savings in copper and insulation when used at ffux densities over 20,000 gaussa. Forms Available: Sheet, strip, solid sections and special shapes. Applications: Core material for motors, generators, and transformers in whi& low weight is necessary, armature...
Journal Articles
Alloy Digest (1963) 12 (4): Ni-81.
Published: 01 April 1963
... Available: Strip, rod, wire, billet forgings. Applications: Glass to metal seals both matched and com- pression types, magnetic relay armatures. Differential expansion temperature controls. Manufacturea Driver-Harris Company Harrison, New Jersey ...
Journal Articles
Alloy Digest (1991) 40 (1): Fe-94.
Published: 01 January 1991
.... Applications: Solenoid switches, armatures, pole pieces, relays and others where a combination of high initial permeability, low hysteresis loss and medium electrical resistivity are desired. Manufacturer: Carpenter Technology Corporation, Carpenter Steel Division Reading, Pennsylvania 19612 ...
Journal Articles
Alloy Digest (1958) 7 (9): Cu-67.
Published: 01 September 1958
..., armature con- ductors, soldering iron tips. Manufacturer: Nippert Electric Products Company Columbus. Ohio ...
Journal Articles
Alloy Digest (1961) 10 (4): CS-15.
Published: 01 April 1961
... or chlorinated cutting oils containing sulphur for the high speed steel cutting tools, but no cutting oil for the carbide-tipped tools. The following feeds, depths of cut and surface cutting speeds are recommended: Hot rolled bars, cold drawn or ground bars. Applications: Armature shafts, drill press spindles...
Journal Articles
Alloy Digest (2014) 63 (12): Cu-834.
Published: 01 December 2014
... applications such as coaxial cables, computer hook-up wire, heat sinks for diodes, rectifiers, and their components, lead wire for circuit breakers and modules, microwave equipment, radar components, solderless connectors, and wave guides. Electrical applications include armature windings, bus bars, and cold...
Journal Articles
Alloy Digest (1969) 18 (5): Cu-199.
Published: 01 May 1969
..., rod, wire, bar, tube and extruded shapes. Applications: Workability: Electronic devices, magnetrons. synchrotrons, klystrons, coaxial cables, electron tubes, vacuum and conventional switch-gear. transistor and diode bases. commutator bars, armature and transformer windings. Manufacturer: Excellent...
Journal Articles
Alloy Digest (1990) 39 (4): Fe-90.
Published: 01 April 1990
...: Bar in various forms and conditions (requests for cold drawn finish should be refemzd to the mill s technical department for acceptan Saip. billet. Applications: Solenoid switches, armatures, pole pieces, relays, etc. Producer: Carpenter Technology Corporstion Carpenter Steel Division Reading...
Journal Articles
Alloy Digest (1973) 22 (12): CS-53.
Published: 01 December 1973
...: Hot roiled and cold-drawn bars and rods. Applications: Spindles, arbors. spline shafts, feed and lead screws, mine car axles and shafts, screws, gears, feed and rack bars, bolts, bushings, anchor pins, tool holders, tie-rods, propeller shafts, armature shafts, pump shafts, collets, turret index gear...
Journal Articles
Alloy Digest (1960) 9 (6): CS-13.
Published: 01 June 1960
... to the direction of rolling. Forms Available: Hot rolled and cold drawn bars. Applications: Mine car axles and shafts, spindles, screws, U-bolts, tie-rods, armature shafts, propeller shafts, arbors, ba.U ~;t;~lts~tsbu.shings, clutches, gears, Iead screws, feed Manufacturer: Practically all carbon steel mills. ...
Journal Articles
Alloy Digest (1957) 6 (6): CS-6.
Published: 01 June 1957
.... Applications: Mine ear axles and shafts, spindles, screws, U-bola, tietods, armature shafts, propeller shafts, arbors, ball joints, bolts, bushings, clutches, gears, lead saews, feed and rack bars. Manufacturer: Bethlehem Steel Company, Bethlehem? Pennsylvania And practically all carbon steel mills under thecr...
Journal Articles
Alloy Digest (1985) 34 (1): CS-103.
Published: 01 January 1985
... to the direction of rolling (transverse direction). Forms Available: Blooms, billets. slabs, hot-rolled bars and rods, and cold-drawn bars and rods. Applications: Typical applications are screws, spindles, mine car axles and shafts, U-bolts, tie rods, armature shafts, arbors, ball joints, bolts, bushings, clutches...
Journal Articles
Alloy Digest (1997) 46 (10): SS-640.
Published: 01 October 1997
..., nonmagnetic cables, vac- uum chambers for atomic energy equipmen& armature winding wire, and high voltage transformer cases. Producer: Allegheny Ludlum Corp. 1000 Six PPG Place Pittsburgh, PA 15222-5479 (412) 294-2800 SS-64OB ...
Journal Articles
Alloy Digest (1955) 4 (12): CS-4.
Published: 01 December 1955
..., arbors, spike shafts, feed and lead screws, mine car axles and shaft+ screws, gears, feed and rack bars, bolts, bushings, anchor pms, tool holders, tie-rods, propeller shafts, armature shafts, pump shafts, cokts. turret index gear sets, clutches. Manufacturer: Jones & Laughlin Steel Corporation...