Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (9): Zn-22.
Published: 01 September 1975
... NJZ ALLOY No. 25 is a zinc-copper-titanium alloy that offers outstanding high creep resistance and a low coefficient of expansion. It can be severely work hardened. Its applications include architectural building products, sporting equipment components, hardware and automotive trim. This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (11): Al-482.
Published: 01 November 2021
.... The architectural products produced from this alloy are used on many high-end building projects to meet customer specifications for uniformity and color match. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (12): Al-109.
Published: 01 December 1961
... ALCAN A320 is an aluminum casting alloy suitable for architectural, ornamental and marine uses. It has good finishing characteristics and excellent corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (4): Al-392.
Published: 01 April 2005
.... Contact the producer for information on custom solid shapes and heat sinks. Applications: Typical applications include architectural and building products; electri- cal components; conduit, pipe, and tube for irrigation systems; door and window frames; railings; and furniture. Alloy 6063 is often used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (11): Cu-222.
Published: 01 November 1970
...-bars and commutators and in forms such as sheet, strip, and plate for many architectural and industrial applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (2): Cu-411.
Published: 01 February 1981
... formability and good resistance to dezincification and stress- corrosion cracking. Among the binary brasses it holds a favored position where product appearance is an important factor; it possesses a rich and pleasing bronze color. Among its many applications are architectural trim, cosmetics containers...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (9): Cu-402.
Published: 01 September 1980
... for use in a wide range of electrical, architectural and hardware applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (11): Al-38.
Published: 01 November 1978
..., utensils and architectural components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-38...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (4): SA-264.
Published: 01 April 1971
...: 10.31399/asm.ad.sa0264 Copyright © ASM International® 1996 Heat Treatment: Yoloy-T Steel is furnished in the hot-rolled condition. The hot-rolled products are intended for cold forming without any subsequent heat treatment. Machinability: Yoloy-T Steel can be machined readily using the procedures employed...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (5): Al-189.
Published: 01 May 1981
... ALUMINUM 6463 is an aluminum-magnesium-silicon alloy used widely for extrusions. It can be hardened and strengthened by a precipitation-hardening heat treatment. Its many applications comprise extrusions for trim and archtectural use in the automotive, appliance and building industries...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
... CARPENTER STAINLESS TYPE 430 is a chromium stainless steel that is especially useful for all types of decorative trim. This steel is suitable for trim on automobiles, cameras, vending machines, counters and showcases, electrical appliances and finished hardware in the building trade. The alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (12): Cu-263.
Published: 01 December 1972
...: Electrical components such as bus bar, contacts, switches, terminals; hardware applications such as ball floats, cotter pins, nails, rivets, soldering copper, tacks; architectural uses for downspouts, flashings, building fronts, gutters, screening; chemical process equipment, anodes, printing rolls, vats...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (4): SS-642.
Published: 01 April 1996
.... In addition, it is used for the construction of apparatus and containers in the dairy. beer. wine, and food industries as well as in the production of nitrogen compounds. Remanit 4301 is also used as wall ties in the building industry. Producer: THYSSEN STAHL AC Krefeld Getmany (02151) 83-01 In USA: Thyssen...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (6): Cu-771.
Published: 01 June 2009
.... For other forms, contact the producer. Applications: The high resistance of this alloy to stress-corrosion cracking and dezincification makes it especially suitable for use as an engineering alloy. Because of its remarkable durability, C22000 is used extensively in architectural, marine, and building...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (10): SS-805.
Published: 01 October 2000
... equipment in con- tact with fresh water also utilize these alloys. Building facades and other architectural and structural applications exposed to nonmarine atmospheres, as well as a large variety of applica- tions involving household and industrial chemicals, heavily utilize the 18-8 alloys. DOI: 10.31399...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (8): Cu-923.
Published: 01 August 2021
... suitable Excellent Excellent Fig. 2. Softening resistance Product Forms Plate, sheet, strip. acids; and alkalis, with the exception of ammonia and cya- Applications nide-containing compounds. Application area Hot Forming Architecture Typical applications Building Heat to 950 °C (1740 °F). Wait...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (5): Cu-931.
Published: 01 May 2022
.... Product Forms Bar; rod; profiles. Applications Category Architecture Automotive Builder s hardware Electrical Industrial Applications Downspouts, flashing, roofing, gutters, building fronts, skylight frames, kitchen counter tops. Gaskets, radiators. Ball floats, butts, rivets, nails, cotter pines...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (11): Cu-554.
Published: 01 November 1990
.... Resistance butt welding is satisfactory; spot and seam methods not recommended. Forms Available: Strip, sheet, plate, rod, wire and shapes. Applications: Architectural; Building fronts, downspouts, flashing, gut- ters, roofing, screening, spouting. Automotive; Gaskets, radiators. Electrical; bus bars...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (11): Al-470.
Published: 01 November 2020
... International, 2019, p 352. Product Forms Plate, flat sheet, coiled sheet. Applications Cabinets, food processing equipment, small marine craft, and in tread plate form for industrial and marine flooring, trailers, and tool boxes. Stucco finish sheet is used in build- ing paneling and similar applications...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (10): Al-57.
Published: 01 October 1957
... in the soft tempers, and tend to build up burrs on the tool. In generai tipped-carbide tools can be ground to approxi- mately the same rake angles used on high speed steel tools for similar work Primary clearance (relief angles) should be 6-9 for most jobs. Secondary clear- ances should be enough so...