Journal Articles
Alloy Digest (1980) 29 (3): CS-82.
Published: 01 March 1980
... AISI 1139 is a carbon steel containing 1.35-1.65% manganese and 0.13-0.20% sulfur to furnish free-machining characteristics. It is recommended especially for high-production machined products. Among its many applications are splined shafts, screws, arbors, tool holders and propeller shafts. This...
Journal Articles
Alloy Digest (1984) 33 (7): TS-424.
Published: 01 July 1984
... JESSOP TRUGLIDE is a free-machining, oil-hardening too steel designed primarily for cold-work die applications. Free graphite in this steel gives it excellent machinability and outstanding resistance to galling and seizing in operation. Among its many uses are dies, gages, punches, arbors and...
Journal Articles
Alloy Digest (1981) 30 (1): TS-375.
Published: 01 January 1981
... hardness, wear resistance, compressive strength and toughness. Typical applications include dies of various types, arbors, punches, pinions, shear blades and clutch parts. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on...
Journal Articles
Alloy Digest (1999) 48 (3): Ni-549.
Published: 01 March 1999
... is well suited for the preparation of special compositions in a timely and cost effective manner. Products Available: Coil sizes up to 200 lb/in. of width with no weld. Standard arbor diameters are as follows: 3.25, 4.25, 6, 9, 12, and 16 in. AMETEK 820 alloy is normally furnished in the annealed...
Journal Articles
Alloy Digest (1956) 5 (11): TS-52.
Published: 01 November 1956
... toughness is desired and ex- treme hardness unnecessary. Where higher hardnesses are re- quired, one of the series with higher carbon content should be selected. Forms Available: Bars, rods, plate, sheer, scrip, wire, and forgings. Applications: Grinding machine spindles, milling machine arbors, larhe...
Journal Articles
Alloy Digest (1990) 39 (12): Ni-389.
Published: 01 December 1990
... raise a straight horizontal wire of the indicated gage to the stated temperamre. B&S Gage 15 16 17 18 19 20 ;; 23 26 27 28 ;z Table 4 - CURRJ%T CHARACTERISTICS OF COILED WIRE* Diam. in. 0.057 0.05 1 0.045 0.040 0.036 0.032 0.0285 0.0253 0.0226 0.0201 0.0179 0.0159 0.0142 0.0126 0.0113 0.010 Arbor...
Journal Articles
Alloy Digest (1991) 40 (1): Ni-390.
Published: 01 January 1991
... indicated gage to the stated temperatme. B&S Gage 15 16 17 18 ii 21 22 ;: 25 E 28 ii Diam. in. 0.057 0.05 1 0.045 0.040 0.036 0.032 0.0285 0.0253 0.0226 0.0201 0.0179 0.0159 0.0142 0.0126 0.0113 0.010 Table 4 - CURFENT CHARACTERISTICS OF COILED !VIRE* Arbor Temperature, OF 572 752 932 1112 - - - 6.0 8.0...
Journal Articles
Alloy Digest (1985) 34 (11): CS-2.
Published: 01 November 1985
... (0.25-2 in Applications: STRESSPROOF is an economical material for use in automatic screw machines. It is widely used for keyed shafts, arbors. gears. pinions. pins and lead screws. Manufacturer: La Salle Steel Company Chicago. Illinois 60680. ...
Journal Articles
Alloy Digest (1969) 18 (4): SA-238.
Published: 01 April 1969
... recommended. It is a general purpose tool room steel. Forms Available: Bars, rods and flats. Applications: Dies, shafting, machine parts, tool shanks, clutch parts, chisels, shear blades, punches, arbors, gears, collets, cams. Manufacturer: North American Steel Co. Warrensvilla Heights, Ohio ...
Journal Articles
Alloy Digest (1966) 15 (2): SA-191.
Published: 01 February 1966
... steel has air hardening properties, especially in small sections, and is especially free of temper-brittleness. Forms Available: Forgings, seamless forged and rolled rings, mandreled forgings, discs and shafts. Applications: Gears, pinions, shafts, machine tool arbors, mill bearing bushings, bearing...
Journal Articles
Alloy Digest (1967) 16 (12): TS-200.
Published: 01 December 1967
... softening at elevated temperatures. Forms Available: Billers, forgings, bars Applications: Gauges, knife edges, knurls, caps, dies, arbors, rolls, bearings. Manufacturer: Universal-Cyclops Specialry Steel Division Cyclops Corporarion Pittsburgh, Pennsylvania ...
Journal Articles
Alloy Digest (1960) 9 (6): CS-13.
Published: 01 June 1960
... direction of rolling. Forms Available: Hot rolled and cold drawn bars. Applications: Mine car axles and shafts, spindles, screws, U-bolts, tie-rods, armature shafts, propeller shafts, arbors, ba.U ~;t;~lts~tsbu.shings, clutches, gears, Iead screws, feed Manufacturer: Practically all carbon steel mills. ...
Journal Articles
Alloy Digest (1962) 11 (5): SA-128.
Published: 01 May 1962
... centers, pushers, dowel pins, straightening rolls, swaging rolls, screw drivers, nail sets, arbors, mandrels, ratchets, cams, conveyor pins, hammers, vise jaws, chuck jaws, etc. Forming inch up to 1 1 to 2 in./rev. sfpm - - 0.0015 70-80 0.00125 70-80 Circular or dovetail Cutoff Camfering and facir.g 2 co...
Journal Articles
Alloy Digest (1962) 11 (8): TS-121.
Published: 01 August 1962
... fully, leaving the flutes softer. This is sometimes desirable for added toughness. Forms Available: Rods and bars. Taps, reamers, broaches, small blanking dies, punches. Arbors, threading dies, drills, thread gauges, and drill bushings. Manufacturer: Vanadium Alloys Steel Corporation Latrobe...
Journal Articles
Alloy Digest (1963) 12 (3): TS-130.
Published: 01 March 1963
... normal heat treatments and is a satisfactory steel for many purposes. Io the hardened condition, it has a hard case sup- ported by a tough core which imparts rhe desired wear-resistance and toughness characteristics of carbon tool steel. Forms Available: Bars and rods. Applications: Arbors, axes, bending...
Journal Articles
Alloy Digest (1964) 13 (2): TS-143.
Published: 01 February 1964
..., arbors, milling cutter bodies, reamer bodies, spindles. Manufacturer: Vanadium Alloys Sreel Corporation Latrobe, Pennsylvania ...
Journal Articles
Alloy Digest (1958) 7 (6): SA-69.
Published: 01 June 1958
... high hardenability, good fatigue properties, and good wear and impact resistance. It is not subject to temper-brittleness after tempering. Forms Available: Bars. Applications: Gears, axles, spindles, adapters, sleeves, nuts, set screws, heavy duty shafting, hydraulic fittings, arbors, pinions, studs...
Journal Articles
Alloy Digest (1959) 8 (3): TS-80.
Published: 01 March 1959
...: Taps, reamers, broaches, smaII blanking dies, punches, drill bushing, wearing parts, arbors. Vanadium Alloys Steel Corporation Latrobe, Pennsylvania ...
Journal Articles
Alloy Digest (1959) 8 (4): CS-9.
Published: 01 April 1959
... induction methods; high wear resistance; excellent mechanical properties. Forms Available: Hot rolled and cold finished bars. Applications: Gears, pinions, lead screws, worm shafts, motor and generator shafts, studs, arbors, bolts, tie rods, drill collars, spindles, mine car axles, anchor pins, clutches...
Journal Articles
Alloy Digest (1955) 4 (12): CS-4.
Published: 01 December 1955
..., arbors, spike shafts, feed and lead screws, mine car axles and shaft+ screws, gears, feed and rack bars, bolts, bushings, anchor pms, tool holders, tie-rods, propeller shafts, armature shafts, pump shafts, cokts. turret index gear sets, clutches. Manufacturer: Jones & Laughlin Steel Corporation...