Alloy Digest (1957) 6 (7): Al-53.
Published: 01 July 1957
... also includes information on high temperature performance as well as machining. Filing Code: Al-53. Producer or source: Aluminum Company of America. Producer or Source: Aluminum Company of America Copyright Ā© ASM InternationalĀ® 1996 1996 ASM International Aluminum A750 anti-scuffing...
Journal Articles
Alloy Digest (1977) 26 (10): Al-229.
Published: 01 October 1977
... anti-scuffing properties, low friction and high resistance to wear under conditions of boundary and thin-film lubrication, it is used extensively for large rolling mill bearings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue...
Journal Articles
Alloy Digest (1982) 31 (9): Al-240.
Published: 01 September 1982
... extensively in the T5 temper for heavy-duty applications, such as large rolling-mill bearings. It is particularly suitable for this application because of its anti-scuffing characteristics, low friction and high resistance to wear under conditions of boundary and thin-film lubrication. Composition: Tin 5.5...
Journal Articles
Alloy Digest (1984) 33 (3): Al-250.
Published: 01 March 1984
... application because of its anti-scuffing characteristics, low friction and high resistance to wear under conditions of boundary and thin-film lubrication. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue...
Journal Articles
Alloy Digest (1976) 25 (6): Mo-12.
Published: 01 June 1976
... forks, synchro rings, gear cones, Wankel Engine end plates, button seals, rebuilding worn or damaged cylinder walls, bumper crankshafts for punch presses, sugar cane grinding-roll journals. anti-galling sleeves, rudder bearings, impeller shafts and pinion-gear journals. For resisting wear by abrasive...
Journal Articles
Alloy Digest (1969) 18 (3): TS-216.
Published: 01 March 1969
... resistance. It has good resistance to decarburization and very good nondeforming properties during hardening. It has good anti-friction characteristics and high impact resistance. It is an oil hardening steel suitable for use as tools, dies, gauges and parts requiring maximum hardness and freedom from...