Alloy Digest (1995) 44 (6): Al-335.
Published: 01 June 1995
... ALUMINUM ALLOY(S) 206.0 and A206.0 are structural castings in the heat treated temper for applications requiring high tensile and yield strengths with moderate elongation. This datasheet provides information on composition, physical properties, tensile properties, and compressive, shear, and...
Journal Articles
Alloy Digest (2020) 69 (1): Al-460.
Published: 01 January 2020
... Rio Tinto Alloys 206.2, A206.2, and B206.2 are heat-treatable, aluminum-copper-magnesium casting alloys in ingot form for remelting. These alloys are primarily intended for producing sand and permanent mold castings for aerospace and automotive applications. This datasheet provides information on...
Journal Articles
Alloy Digest (1992) 41 (7): SA-463.
Published: 01 July 1992
... ultimate Yield Red. of Temp. Temp. StR.tlgth StiIlgth Elong. Area F OF (ksi) @xi) % % 185Oair 1150 209.0 206.0 13.3 45.5 185Oair 1175 194.7 193.5 13.5 48.4 17cOair 1150 184.3 179.2 14.4 50.1 17OQair 1175 177.4 176.2 15.0 50.1 Table 2 - COEFFICIENT OF THERMAL EXPANSION Temperature hperh Temperature Cm. per...