Alloy Digest (1973) 22 (8): Al-23.
Published: 01 August 1973
... ALUMINUM 2024 is a high-strength wrought alloy that responds readily to an age-hardening heat treatment. It is recommended for applications requiring highly favorable strength-weight ratios. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1999) 48 (1): Al-357.
Published: 01 January 1999
... Kaiser Aluminum Alloy 2024 has good machinability and good mechanical properties. The alloy is typically used in aircraft structures, rivets, connectors, hydraulic valve bodies, and miscellaneous structural applications. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2008) 57 (9): Al-417.
Published: 01 September 2008
... joinability machinability physical properties tensile properties workability ALCAN 2024-T3, T351X (Aluminum-Copper-Magnesium Alloy Extruded Bar) This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. Chemical Composition, wt (Typical) Silicon 0.50 max...
Journal Articles
Alloy Digest (2010) 59 (6): Al-429.
Published: 01 June 2010
... datasheet covers Alcan 2024 alloy in T3 and T351x tempers for drawn tubes. The alloy possesses good damage tolerance. See also Alloy Digest Al-417. ALCAN 2024 T3, T351X TUBES (Aluminum-Copper- Magnesium Alloy) ALCAN 2024 T3, T351X TUBES Chemical Composition, wt (Typical) Silicon 0.50 max Iron 0.50 max...
Journal Articles
Alloy Digest (2000) 49 (9): Al-372.
Published: 01 September 2000
... toughness at moderately high strength levels. Approxi- mate bands for axial stress notch fatigue data are shown in Fig. 1 for 2024 T351 and T851 products. Heat Treatment: The recommended practices for heat-treating and aging alloy 2024 sheet and plate are described in MIL-H-6088, Heat Treatment of Aluminum...
Journal Articles
Alloy Digest (1998) 47 (3): Al-346.
Published: 01 March 1998
.... Anodizing: Alcoa 2024 accepts all types of anodic coatings. General Characteristics: A cold finished aluminum wrought product, Alcoa 2024 is a high strength aluminum screw machine stock alloy with tensile Table 1 Typical Mechanical Properties Ta?.sik~ Yid sue* -in TV MPa ksi MF-a ksi Zin T351.T4 469 68 324...
Journal Articles
Alloy Digest (1998) 47 (10): Al-354.
Published: 01 October 1998
.... Corrosion resistance is only fair. Weldability is good with arc and resistance methods. In many applications, this ahoy can be substituted for 2024. Tennalum and Kaiser are registered trademarks of Kaiser Aluminum Corporation. Chemical Composition, wt Silicon Iron Copper Manganese Magnesium Chromium zinc...
Journal Articles
Alloy Digest (2008) 57 (5): Al-413.
Published: 01 May 2008
... Kaiser aluminum alloy 2124 is a high-purity version of 2024 with tighter controls on the iron and silicon for an increase in strength and toughness. It is primarily used as plate in the aircraft industry. This data sheet applies to sheet, coil, and plate in the T851 temper. This datasheet provides...
Journal Articles
Alloy Digest (2006) 55 (10): Al-401.
Published: 01 October 2006
... corrosion-resistant alloys fatigue resistance manufacturability tensile properties workability wrought aluminum alloys Chemical Composition, wt Alloy 2026 Alloy 2024 Alloy 2224 Zinc 0.10 max 0.25 max 0.25 max Magnesium 1.00 1.60 1.2 1.8 1.2 1.8 Copper 3.60 4.30 3.4 4.9 3.8 4.4 Zirconium 0.05 0.25...
Journal Articles
Alloy Digest (2009) 58 (8): Al-424.
Published: 01 August 2009
... Alcan 2027 is an Al-Cu-Mg-Mn-Zr alloy, developed to provide higher strength and damage tolerance than the incumbent 2024 alloy. Alcan 2027 T3511 possesses good damage tolerance. This datasheet covers Alcan 2027 T3511 in both thin and the heavier cross sections. This datasheet provides information...
Journal Articles
Alloy Digest (2006) 55 (7): Al-399.
Published: 01 July 2006
... Alloy 2124 is a heat treatable plate alloy that was developed for elevated-temperature application. Copper is the main alloying addition. 2124-T851 plate is an improvement in fracture toughness compared to 2024-T851. This datasheet provides information on composition, physical properties, and...
Journal Articles
Alloy Digest (2007) 56 (6): Al-404.
Published: 01 June 2007
...: 2056 is delivered in O or T3 temper depending on customer requirements. Corrosion Resistance: The cladding consumption of 2056 clad sheet is lower than that of 2024 clad sheet (typically 3.2 mm). See Fig. 2. Specification Equivalents: AMS 4298 MMPDS pending ALCAN 2056 T3 Filing Code: Al-404 Aluminum...
Journal Articles
Alloy Digest (2007) 56 (8): Al-405.
Published: 01 August 2007
... workability Chemical Composition, wt (Typical for alloy 2098) Silicon 0.12 max Iron 0.15 max Copper 3.2-3.8 Manganese 0.35 max Magnesium 0.25-0.8 Silver 0.25-0.6 Lithium 0.8-1.3 Zirconium 0.04-0.18 Aluminum bal Physical Properties: Density, kg/m3 (lb/in.3) 2098 2700 (0.097) 2024 2780 (0.100) Mechanical...
Journal Articles
Alloy Digest (2007) 56 (12): Al-408.
Published: 01 December 2007
... fatigue properties heat treatability joinability physical properties tensile properties weldability workability Chemical Composition, wt (Aluminum Association (AA) registered limits) AA 6156 AA 2024 AA 2024A Silicon 0.7 1.3 0.50 max 0.15 max Iron 0.20 max 0.50 max 0.20 max Copper 0.7 1.1 3.8 4.9...
Journal Articles
Alloy Digest (1988) 37 (7): Al-282.
Published: 01 July 1988
... Alcoa Aluminum Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy. It is available in five tempers. It is crossing many market areas of applications in aerospace, defense, automotive and general structural use. This datasheet provides information on composition, physical properties, elasticity, and...
Journal Articles
Alloy Digest (1974) 23 (8): Al-58.
Published: 01 August 1974
... 2024-O. In the T4 temper condition it forms as readily as 2024T3 or 2024-T4. Weldability: Aluminum 2017 can be welded with proper equipment and procedure. However, because of the effect of heating on corrosion resistance, welding is rarely recommended except where heat treatment after welding is...
Journal Articles
Alloy Digest (1958) 7 (2): Al-63.
Published: 01 February 1958
... dloy has the suength characteristics approaching Aluminum 2024 aIloy and fabricating characteristics equaling Aluminum 6061 alloy. It com- bines low cost, excellent mechanical properties, weight savings and workabiby. It is a general purpose aIu- minum alloy with high strength, high corrosion resist...
Journal Articles
Alloy Digest (1979) 28 (11): Al-158.
Published: 01 November 1979
.... Rivets of this alloy are widely used in aircraft and are also used successfully in other types of structures where the parts to be joined are Ahuninum 2014, Aluminum 2017 or Aluminum 2024. Forms Available: Rod, wire and rivets. Application: Rivets and other fasteners. Manufacturers: Aluminum alloy mills. ...
Journal Articles
Alloy Digest (1960) 9 (10): Al-96.
Published: 01 October 1960
... treated and artificially aged, T42 Temper - Material in any form. purchased in any temper then resolution created by user. T62 Temper - Material in any form, purchased in any temper then resolurion created and aged by the user, The workability of Aluminum 2219 is comparable to that of Aluminum 2024...
Journal Articles
Alloy Digest (1998) 47 (11): Al-355.
Published: 01 November 1998
... Kaiser Aluminum alloy 2017 has good machinability and good mechanical properties. It is used in rivets. General structural applications, and transportation. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue...