Journal Articles
Alloy Digest (1991) 40 (4): Fe-95.
Published: 01 April 1991
... ALCHROME ALLOY DK is a heating element alloy for use up to 2300 F (1260 C). This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Fe-95. Producer or source: Carpenter Technology Corporation. Producer or Source: Carpenter Technology...
Journal Articles
Alloy Digest (2024) 73 (3): SS-1366.
Published: 01 March 2024
... VDM 40 B is an austenitic iron-nickel-chromium-silicon-lanthanum alloy that is suitable for heating elements. It is characterized by excellent oxidation resistance, high resistivity, good sag resistance, and superior mechanical properties at high temperatures in comparison to other heating element...
Journal Articles
Alloy Digest (1971) 20 (2): Ni-162.
Published: 01 February 1971
... TOPHET H is a heating-element alloy specifically designed for use in duct heaters and clothes dryers where hot strength and long life are of most importance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2005) 54 (6): SS-932.
Published: 01 June 2005
... June 2005 ALUCHROM Eco (Heating Element Alloy) Aluchrom Eco is an improved heating element material with extended life, especially in high-oxygen environments. Table 1 Typical Mechanical Properties of Wire at Room Temperature Wire diameter Yield strength, 0.2% Tensile strength Elongation, mm in. MPa...
Journal Articles
Alloy Digest (1981) 30 (2): Ni-265.
Published: 01 February 1981
... NIKROTHAL 6 is a nickel-chromium-iron electrical-resistance alloy for use in appliances and industrial furnaces. Its maximum recommended operating temperature is 1125 C (2055 F). It is highly suitable for heating elements in domestic appliances. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1981) 30 (5): Ni-268.
Published: 01 May 1981
... NIKROTHAL 8 is a nickel-chromium electrical-resistance alloy for use in appliances and industrial furnaces. Its maximum recommended element temperature in continuous use is 1200 C (2190 F). Nikrothal 8 is non-magnetic, highly resistant to corrosion, and has a lower temperature coefficient...
Journal Articles
Alloy Digest (1958) 7 (8): Ni-43.
Published: 01 August 1958
..., watts/cm/X. at 1OOOC. carbon 0.05 Chromium 20.0 Ahlminum 5.0 SiliCOl3 Nickel 1.5 Remainder Psblisbed by Engineering Alloys Digest, Inc Upper Montclair, New Jersey D-H No. 245 (Heating Element Alloy) 7.9 0.2854 0.125 Thermal coef. expansion, in/in/X. (20-500┬░C.) x 1O-6 Thermal coef. resistance, ohms/ohm...
Journal Articles
Alloy Digest (1959) 8 (12): SS-98.
Published: 01 December 1959
... CHROMEL-D is a special 35-20 nickel-chromium alloy developed primarily for use as heating elements in industrial furnaces designed to operate in the critical temperature range between 1500 and 1800 F. with controlled atmospheres. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1997) 46 (4): SS-677.
Published: 01 April 1997
... AND ALLOYS Filing Code: S-677 m Stainless Steel - u vm- -, April 1997 ALFA-Iv ALLOY (Ferritic Stainless Steel Containing Aluminum and Rare Earth Elements) ALFA-Iv alloy is a 20% Cr. 5% AI stainless steel enhanced in oxidation resistance for high-temperature use by the addition of the rare earth metals cerium...
Journal Articles
Alloy Digest (2001) 50 (10): SS-833.
Published: 01 October 2001
... Allegheny Ludlum Type 334 is an austenitic stainless steel with alloying elements of aluminum and titanium. These additions, along with its higher chromium and nickel levels, give the alloy excellent strength and oxidation resistance, especially when compared to Type 304 stainless steel...
Journal Articles
Alloy Digest (1990) 39 (5): Al-304.
Published: 01 May 1990
... AA 2014 is a precipitation hardenable aluminum alloy in which copper is the principal alloying element. In the heat treated condition the alloy's properties are similar to those of mild steel. Corrosion resistance of AA 2014 is inferior to that of most other aluminum alloys. Sheet and plate may...
Journal Articles
Alloy Digest (2021) 70 (2): TS-809.
Published: 01 February 2021
... Deutsche Edelstahlwerke Cryodur 2002 is a high-carbon, alloy cold-work tool steel in which the principal alloying element is chromium. It is among the least expensive of the tool steels and requires strict control of processing and heat treatment to achieve good properties and performance. The low...
Journal Articles
Alloy Digest (1992) 41 (12): Cu-537.
Published: 01 December 1992
... BRUSH CASTING ALLOYS 275C AND 275CT are beryllium copper alloys of very high strength with cobalt and silicon as the secondary alloying elements. Use is in the age-hardened temper. Brush casting alloy 275CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2005) 54 (6): SS-923.
Published: 01 June 2005
... The AL-6XN PLUS alloy is an enhanced version of the AL-6XN alloy (see Alloy Digest SS-494, May 1988). Both satisfy the composition requirements of UNS N08367, but AL-6XN PLUS contains a greater concentration of the alloying elements (Cr, Mo, and N) which promote corrosion resistance...
Journal Articles
Alloy Digest (2010) 59 (6): SS-1067.
Published: 01 June 2010
... ZECOR ALLOY (UNS S38815) was developed as a lower cost alternative to other austenitic stainless steels for use in environments containing concentrated sulfuric acid. The alloy has the leanest alloying element content of any of the high silicon austenitic stainless steels designed for concentrated...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-581.
Published: 01 January 1993
... BRUSH CASTING ALLOYS 20C AND 20CT are beryllium copper alloys (1.90-2.15% Be) of very high strength with cobalt as the second alloying element (0.35 to 0.70% Co). Use is in the age-hardened temper. Brush casting alloy 20CT is the fine-grained version. This datasheet provides information...
Journal Articles
Alloy Digest (1992) 41 (9): Cu-576.
Published: 01 September 1992
... BRUSH CASTING ALLOYS 165C AND 165CT are beryllium copper alloys of high strength with cobalt as the second alloying element (0.20 to 0.65% Co). Use is in the age-hardened temper. Brush casting alloy 165CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1992) 41 (10): Cu-577.
Published: 01 October 1992
... BRUSH CASTING ALLOYS 245C AND 245CT are beryllium copper (2.25-2.55% Be) alloys of high strength with cobalt as the second alloying element (0.35-0.70% Co). Use is in the age-hardened temper. Brush casting alloy 245CT is the fine-grained version. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2001) 50 (12): Ti-123.
Published: 01 December 2001
... TIMETAL 367 is a Ti-6Al-7Nb medium-strength alpha-beta alloy for surgical implants. The alloy is analogous to TIMETAL 367 6-4 (revised as Ti-6Al-4V, Alloy Digest Ti-66, September 1992), but with niobium as the more biocompatible alloying element. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1963) 12 (6): Ti-35.
Published: 01 June 1963
... Republic RS-110A is a titanium alloy containing manganese as its principle alloying element. The alloy is a medium strength, highly formable sheet alloy which has been used extensively as an aircraft structural material. This datasheet provides information on composition, physical properties...