Journal Articles
Alloy Digest (1956) 5 (8): TS-49.
Published: 01 August 1956
... AIRDI-150 is an air-hardening high-carbon high-chromium tool and die steel having high resistance to abrasion. It corresponds to AISI Type D2 and ASM Class II D-2. This datasheet provides information on composition, hardness, tensile properties, and compressive strength as well as fracture...
Journal Articles
Alloy Digest (2020) 69 (4): TS-790.
Published: 01 April 2020
... Crucible Airdi 150 is an air-hardening, high-carbon (1.5%), high-chromium (12%), alloy cold work tool steel that also contains molybdenum and vanadium. It is suitable for applications that require very good abrasive wear resistance. This datasheet provides information on composition, physical...