1-7 of 7 Search Results for

aircraft heaters

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1982) 31 (4): SS-405.
Published: 01 April 1982
... CRUCIBLE 309 is a non-hardenable austenitic chromium-nickel steel that has high heat-resisting characteristics. In the annealed condition it is non-magnetic or magnetic, depending on the composition. When cold worked it is very slightly magnetic. Typical applications include aircraft heaters and...
Journal Articles
Alloy Digest (1965) 14 (12): Ni-108.
Published: 01 December 1965
... cold drawn tubes, welded or welded and cold drawn cubes and strip. Applications: Aircraft exhaust manifolds, cabin heaters, locking wire, parts in turbo-jet engines. Nuclear power reacror heat exchanger tubes, equipment for the plastic, paper and pulp, textile and chemical industries. Furnace parts...
Journal Articles
Alloy Digest (1981) 30 (11): SS-396.
Published: 01 November 1981
... this sensitizing (damaging) temperature range; however, its carbon combines preferentially with titanium leaving chromium in solution to maintain full corrosion resistance. Among its applications are high-temperature steam service, chemical plants and heavy-duty aircraft exhaust manifolds. This...
Journal Articles
Alloy Digest (1962) 11 (12): Ni-77.
Published: 01 December 1962
..., bubble- towers, manifolds, collector rings, heaters, lock wires, gaskets, jet blankets and combustion liners, cbermo- couple coverings, domes and transition units in jer- propelled aircraft. Used in the chemical, petroleum and paper pulp industries. Manufacturer: Rolled Alloys, Inc. Decroir 11, Michigan ...
Journal Articles
Alloy Digest (2003) 52 (12): SS-896.
Published: 01 December 2003
... in. maximum. Inquire to the manufacturer about slit coils for Gauer bar. Hot-rolled annealed and pickled sheet is available as a standard grade with thickness 0.095 0.300 in. and width 24 60 in. Applications: Typical applications are aircraft heaters, chemical processing equipment, dryers, dyehouse...
Journal Articles
Alloy Digest (2017) 66 (7): Ni-731.
Published: 01 July 2017
... pipes, afterburners, nozzle vein, cabin heaters, and other aircraft components. Producer: Hitachi Metals MMC Superalloy, Ltd. Saitama 363-8510, Japan Tel: +81-48786-3709 Fax: +81-48-786-3416 www.hitachi-metals-sa.co.jp ISSN: 002-614X Ni-731B Table 2 Average stress-rupture data for mill-annealed bar...
Journal Articles
Alloy Digest (1956) 5 (1): Ni-22.
Published: 01 January 1956
... turbines, aircraft engine components, flame tubes, slator blades, dies and cores for die-casting aluminum and bronze and brass, furnace tubes, thermocouple sheaths, precision molds for glass, first-stage blading for steam turbines, com- bustion components of aircraft, cabin heaters, gas tur- bine tubes...