Skip Nav Destination
Close Modal
Search Results for
airborne assemblies
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3 Search Results for
airborne assemblies
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (6): Ti-44.
Published: 01 June 1965
... Ti-6A1-6V-2Sn is an alpha-beta titanium alloy capable of heat treatment to very high strength levels. It provides effective weight saving when extruded shapes, thick plate sections, or forged parts are required for airborne assemblies operating at long times to temperatures up to 700 F...
Abstract
View article
PDF
Ti-6A1-6V-2Sn is an alpha-beta titanium alloy capable of heat treatment to very high strength levels. It provides effective weight saving when extruded shapes, thick plate sections, or forged parts are required for airborne assemblies operating at long times to temperatures up to 700 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-44. Producer or source: Titanium Metals Corporation of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (10): Ti-27.
Published: 01 October 1960
... assemblies is 60 hours at WOOF plus 30 minutes at 105OoF, air cooled. Corrosion Resistance: In either the solution-treated or aged condition the marerio is inert to sea water, salt and ocher natural environments, oxidizing media, inhibited reducing acids, alkalis and metallic chlorides at ambient...
Abstract
View article
PDF
Ti-13V-11Cr-3Al is a high strength, meta-stable beta titanium-base alloy recommended for service in the temperature range of -65 to plus 600 F. It responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-27. Producer or source: Titanium Metals Corporation of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (6): Cu-356.
Published: 01 June 1978
...: Beryllium-containing materials, like many other industrial materials, are potentially harmful if proper precautions are not taken. The hazards can usually be controlled easily and economically. Care must be taken in the fabrication and processing of these materials to avoid inhalation of airborne beryllium...
Abstract
View article
PDF
BRUSH Alloy 25 attains the highest strength and hardness of any copper-base alloy. In the age-hardened condition, its tensile strength can exceed 200,000 psi and its Rockwell C hardness can reach 45. Its many applications include springs, deep-drawing parts, current-carrying springs connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-356. Producer or source: Brush Wellman Inc..