1-15 of 15 Search Results for

air conditioners

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (4): Cu-495.
Published: 01 April 1985
... characteristics and can be joined by several methods. Among its many applications are air conditioners, gas lines, heater lines, oil-burner and plumbing tubes, dairy tubes and oil lines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1986) 35 (6): Cu-511.
Published: 01 June 1986
... applications are cooling fins for automotive and heavy-duty radiators, anneal-resistant electrical uses and air conditioners. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1999) 48 (11): Fe-121.
Published: 01 November 1999
..., active convertors in air conditioners and refrigerators, high-speed motors, and automotive parts such as actuators Inverter insulation transformers for UPS and fuel battery power systems; distribution transformers; current transformers (CT) for power transmission (a) A 6.5% silicon content is optimum...
Journal Articles
Alloy Digest (1992) 41 (4): Cu-570.
Published: 01 April 1992
..., brazing, coated metal-arc welding and butt resistance welding characteristics. Its machinability rating is 20% that of free cutting brass. Forms Available Sheet and strip, light annealed (050) and cold worked tempers (HO0 through HlO). Applications: Air conditioners, cooling fins for heavy duty and auto...
Journal Articles
Alloy Digest (2001) 50 (7): Cu-669.
Published: 01 July 2001
..., and contour-milled strip. Strip thicknesses are 0.08 mm and greater. Strip widths are 3 mm and greater, but must be a minimum of 10× the strip thickness. Applications: The most important application is in the manufacture of power transistors. Other applications include air conditioner and heat exchanger...
Journal Articles
Alloy Digest (2021) 70 (8): Cu-923.
Published: 01 August 2021
... for equalization of the tem- Consumer Downspouts, flashing, gutters, roofing. perature. Do not finish below 750 °C (1380 °F). Electrical Industrial Condenser sheets, heater units. Heat Treatment Marine Air conditioners, refrigerators. Annealing temperature Stress relieving temperature Heater elements, wire...
Journal Articles
Alloy Digest (1971) 20 (2): SS-250.
Published: 01 February 1971
.... The fabrication of this new stainless steel is similar to Type 410. However, unlike Type 410. Armco 400 is non-hardenable by heat treatment because of its low carbon content. The low level of carbon also minimizes hardening during welding. Forms Available: Sheet and strip. Applications: Air conditioner panels...
Journal Articles
Alloy Digest (2022) 71 (1): Cu-928.
Published: 01 January 2022
... Table 3 for ratings of fabrication characteristics. Product Forms Plate; sheet; strip. Applications Air conditioners; air, hydraulic, and oil pipes; engineering apparatus; architecture; cladding band; components of electrical engineering; heat exchangers; roofing; transistors; wire. Supplier Aurubis AG...
Journal Articles
Alloy Digest (1972) 21 (3): Cu-253.
Published: 01 March 1972
... as industrial condensers, refrigerators, heat exchangers and evaporators. Forms Available: Bar, rod, wire, plate, sheet, strip, pipe, tube, extrusions. Applications: Air conditioners, brewery tubes, condensers. evaporators, heat exchangers, dairy tubes, distiller tubes, kettles, pulp and paper lines, steam...
Journal Articles
Alloy Digest (1973) 22 (12): Cu-273.
Published: 01 December 1973
... are available from major mills throughout the world. Applications: Refrigerator and air conditioner tubing and components, commutators, clad products, gas and burner lines and units, oil burner tubes, condenser and heat exchanger tubes, pulp and paper lines, steam and water lines, tank gage lines, plumbing pipe...
Journal Articles
Alloy Digest (1980) 29 (8): Cu-400.
Published: 01 August 1980
..., hydraulic and gas lines, air conditioners, chemical and industrial heat exchangers, refrigerators, radiant-heating lines, sugar house refinery lines and heaters and calandria pans, brewery tubs and kettles, brewery lines, pulp and paper lines and tanks, instrument piping, heater elements. wire connectors...
Journal Articles
Alloy Digest (2021) 70 (8): Al-479.
Published: 01 August 2021
... London SW1Y 4AD, United Kingdom Automotive turbo chargers; impellers and scrolls for auto- Tel: +44 20 7781 2000 / Web: www.riotinto.com motive air conditioners. All data from Primary Aluminum Foundry Alloys, 4th ed., Rio Tinto, 2019, except where noted. ISSN: 002-614X Al 479B ...
Journal Articles
Alloy Digest (2018) 67 (1): SA-808.
Published: 01 January 2018
... mm (0.6 in.) plate thickness. The values are valid for the delivery condition. Delivery condition: normalized or normalized rolled. Heat Treatment Normalizing. 840 890 °C (1544 1634 °F), subsequent to temperature equalization and cooling in still air. Hardening. 870 920 °C (1598 1688 °F) and quenched...
Journal Articles
Alloy Digest (2018) 67 (2): SA-811.
Published: 01 February 2018
... Properties typical of 15 mm (0.6 in.) plate thickness. Yield strength values are valid for the delivery condition (normalized or normalized rolled). Heat Treatment Normalizing is done at 840 890 °C (1544 1634 °F) subsequent to temperature equalization and cooling in still air. Hardening is done at 870 920 °C...
Journal Articles
Alloy Digest (1965) 14 (5): SS-168.
Published: 01 May 1965
... OF SPRINGS (Initial room temperature stress for 96 hours) Test % Loss in Load Temperature Initial Stress 40000 psi Initial Stress 80000 psi oF 0.040 Rd.* 0.080 Rd.* 0.040 Rd.* 0.080 Rd 350 0.0 0.0 450 1.1 0.9 550 a:; 2.0 1.26 3.7 650 3.7 5.55 4.0 750 15.6 10.7 20.7 13.2 l Aged 9000F for 1 hr., air cooled...