Journal Articles
Alloy Digest (1977) 26 (11): CS-70.
Published: 01 November 1977
... for agricultural machinery and tools, hand tools, shafts, springs and heavy-machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1980) 29 (2): CS-80.
Published: 01 February 1980
... workability. Its many uses include hand tools, machinery parts, springs and agricultural machinery. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1983) 32 (2): CS-92.
Published: 01 February 1983
... if precautions are taken to prevent cracking. Its many uses include springs, hand tools, heavy machinery parts, shafts and agricultural machinery. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1987) 36 (12): CS-116.
Published: 01 December 1987
... if precautions are taken to prevent cracking. Its many uses include springs, hand tools, heavy machinery parts, shafts and agricultural machinery. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2011) 60 (11): SA-636.
Published: 01 November 2011
... Dillidur 400V is a wear-resistant steel with surface hardness at room temperature of 370–430 HB. The steel is easy to weld, bend, and machine. Because of its high wear resistance and good welding performance, 400V is used in the production of agricultural machinery and industrial truck systems...
Journal Articles
Alloy Digest (1984) 33 (2): CS-100.
Published: 01 February 1984
... or liquid-quenched-and-tempered condition for a wide range of applications. It has good machinability and good workability. Its many uses include springs, shafts, hand tools, railway parts and agricultural machinery. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1973) 22 (1): CS-49.
Published: 01 January 1973
... AISI 1055 is a high-carbon oil or water-hardening tool and machinery steel recommended for hand tools, agricultural tools and machinery, shafts, springs and heavy-machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1988) 37 (1): CS-117.
Published: 01 January 1988
... SAE 1055 is a high-carbon oil or water-hardening tool and machinery steel recommended for hand tools, agricultural tools and machinery, shafts, springs and heavy-machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1980) 29 (5): CS-83.
Published: 01 May 1980
... lightly. It has good wear resistance. Its many uses include agricultural equipment, tools, springs and machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1985) 34 (5): CS-105.
Published: 01 May 1985
... hardness and a soft core on quenching and tempering lightly. It has good wear resistance. Its many uses include agricultural equipment, tools, springs, and machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2018) 67 (1): SA-808.
Published: 01 January 2018
... applied in an unquenched condition where moderate wear requirements are present, e.g., concrete mixers. This steel grade has been tried and tested in various applications in agricultural machinery, for example in harrows, balers, and ploughs, and also in construction machinery. Product Forms Available...
Journal Articles
Alloy Digest (2018) 67 (2): SA-811.
Published: 01 February 2018
... resistance is required. The TBL grade is also applied in an unquenched condition where moderate wear requirements are present, e.g., concrete mixers. This steel grade has been tried and tested in various applications in agricultural machinery; for example, in harrows, balers, and ploughs and also...
Journal Articles
Alloy Digest (2016) 65 (6): SA-758.
Published: 01 June 2016
... components, tow hooks, industrial silos, and lifting and excavating and agricultural machinery. Producer: Tata Steel 1970 CA IJmuiden The Netherlands Tel: +31 (0) 251 496126 www.tatasteeleurope.com ISSN: 002-614X SA-758BFig. 1 Available dimensions of Ympress Laser S420MC ...
Journal Articles
Alloy Digest (1976) 25 (10): CS-63.
Published: 01 October 1976
..., sheet and billets. Applications: Braces, shafts, hand tools, wrenches, hammers, pliers, screw drivers, axes, hatchets, agricultural machinery, heavy machinery parts and various types of springs. Manufacturers: Carbon steel mills. ...
Journal Articles
Alloy Digest (1988) 37 (1): CS-118.
Published: 01 January 1988
..., hand tools, wrenches, hammers, pliers, screw drivers, axes, hatchets, agricultural machinery, heavy machinery parts and various types of springs. Manufacturers: Carbon steel mills. ...
Journal Articles
Alloy Digest (2003) 52 (5): SA-512.
Published: 01 May 2003
... reduce production costs, lower overall weight, and increase payload. Examples include cranes; the car, truck, and the rail industries; and contractor and agricultural machinery. Producer: SSAB Swedish Steel, Inc. 4700 Grand Ave. Pittsburgh, PA 15225 (800) 8536639 (412) 269-2120 (412) 269-2124 (fax...
Journal Articles
Alloy Digest (1975) 24 (9): CS-57.
Published: 01 September 1975
..., hatchets, axes, agricultural machinery, cold-formed flat springs, large hot-formed flat springs, hot-coiled helical springs, lawn mower blades, and mine bits. Manufacturer: Practically all carbon steel mills. ...
Journal Articles
Alloy Digest (1988) 37 (6): CS-121.
Published: 01 June 1988
... strip, cold-rolled strip, wire. and heavy rolled and forged shapes such as rails. Applications: Heavy machinery parts, shafts, braces, control rods, hand tools, wrenches, hammers, pliers, screwdrivers, hatchets, axes, agricultural machinery, cold-formed flat springs, large hot-formed flat springs, hot...
Journal Articles
Alloy Digest (1986) 35 (8): CS-112.
Published: 01 August 1986
.... wire and heavy rolled and forged shapes. Applications: Hand tools, music wire. control rods, braces. shafts, heavy machinery parts, wrenches. hammers. pliers, screwdrivers, hatchets. axes, agricultural machinery. cold-formed flat springs. large hot- formed flat springs. hot-coiled helical springs, lawn...
Journal Articles
Alloy Digest (1980) 29 (3): CS-81.
Published: 01 March 1980
... and equipment, agricultural machinery, gears, pins, rods, trusses, forgings, chain pins, track Iinks and various types of tools. Manufacturer: Carbon steel milLs. ...