Alloy Digest (2006) 55 (10): Al-401.
Published: 01 October 2006
... Alcoa extrusion alloy 2026 was developed as an improvement over 2024 and 2224 extrusions in aerospace structural applications where the governing selection criteria are high damage tolerance, good fatigue resistance, and a high degree of manufacturability. In addition to improved damage tolerance...
Journal Articles
Alloy Digest (2006) 55 (8): Al-400.
Published: 01 August 2006
... Aluminum 7xxx series alloys contain zinc as the main alloying element, usually in combination with magnesium and copper. High-strength 7020 alloy is widely used in aerospace structures and is approved by the world’s leading airframe builders. For engineering applications this alloy is generally...
Journal Articles
Alloy Digest (2008) 57 (10): Al-418.
Published: 01 October 2008
... Alcan 7040 is an Al-Mg-Zn-Cu-Zr alloy, developed to provide an improved strength-toughness balance versus incumbent 7010 and 7050 alloys. This datasheet covers Alcan 7040 alloy in T7651 temper. The alloy is used in aerospace structures. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2008) 57 (12): SS-1003.
Published: 01 December 2008
... Carpenter Ferrium S53 is both corrosion resistant and ultrahigh-strength for aerospace structural applications. Please see updated designation and information on this alloy in Alloy Digest SA-589, December 2008. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2000) 49 (9): Al-372.
Published: 01 September 2000
... Alcoa 2024 was introduced by Alcoa in 1931 as the first alloy to have a yield strength approaching 345 MPa (50 ksi). With relatively good fatigue resistance in plate forms, alloy 2024 continues in many aerospace structural applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1971) 20 (9): Be-1.
Published: 01 September 1971
... LOCKALLOY is a beryllium-aluminum alloy that was developed for aerospace structural applications where high modulus and low density are design criteria. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive, shear, and bearing...
Journal Articles
Alloy Digest (1982) 31 (10): SA-387.
Published: 01 October 1982
..., the new grade provides higher ductility and toughness. VascoMax T-250 is recommended for aerospace structures, pressure vessels, shafting, bolts, and fasteners. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1987) 36 (1): Be-3.
Published: 01 January 1987
... components and aerospace structural applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface...
Journal Articles
Alloy Digest (2001) 50 (7): Al-374.
Published: 01 July 2001
... direction. Source: Aerospace Structural Metals Handbook, Nonferrous Alloy, AIWT on AL-6069 Table 2 Tensile Properties of Hot Hollow Extrusions Tensile strength Yield strength Elongation, Direction MPa ksi MPa ksi % Longitudinal 396 57.4 345 50.1 20 Transverse 451 65.4 407 59 9.6 45° 412 59.7 361 52.4 21.5...
Journal Articles
Alloy Digest (2010) 59 (8): SA-618.
Published: 01 August 2010
...-sensitive aerospace structural applications. It is double vacuum melted variety (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superior cleanliness, ingot homogeneity, and to enhance mechanical properties. Product Availability: Lescalloy AF1410 VIM-VAR steel is available...
Journal Articles
Alloy Digest (2007) 56 (12): SS-1004.
Published: 01 December 2007
... Crucible 422 has a structure of tempered martensite to give the alloy high strength. It is useful in the aerospace industry for structurals with high strength/weight ratios. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2008) 57 (5): Al-413.
Published: 01 May 2008
... temper are shown in Table 1. Product Forms Available: Sheet coil and plate, typically supplied in 1.5 6.0 in. plate. Applications: Aerospace structural components Producer: Tennalum A Division of Kaiser Aluminum Jackson, TN 38301 (800) USE-2011 (731) 427-6499 (fax) www.kaiseraluminum.com DATA...
Journal Articles
Alloy Digest (2012) 61 (9): Al-439.
Published: 01 September 2012
... structures. ALCOA ALLOY 2099-T83 and T8E67 (Reduced-Density, High-Strength Aerospace Alloy) ALCOA ALLOY 2099-T83 and T8E67 Chemical Composition, wt (Range) Silicon 0.05 max Iron 0.07 max Copper 2.4 3.0 Manganese 0.10 0.50 Magnesium 0.10 0.50 Chromium 0.05 Zinc 0.4 1.0 Lithium 1.6 2.0 Zirconium 0.05 0.12...
Journal Articles
Alloy Digest (1969) 18 (9): Ni-147.
Published: 01 September 1969
... IN-102 is a nickel-chromium-iron alloy designed for long service at temperatures up to 1300 F. It combines high strength and high ductility at the elevated temperatures with a high degree of structural stability. It is used for aerospace, power and steam turbine components. This datasheet provides...
Journal Articles
Alloy Digest (1970) 19 (5): SA-251.
Published: 01 May 1970
... VascoMax 350 CVM is an ultra-high-strength steel responding to a maraging heat treatment. It has superior notch toughness and ductility at the high yield strength level of 340,000 psi and above. It is recommended for aerospace and rocket equipment and structures. This datasheet provides...
Journal Articles
Alloy Digest (1970) 19 (12): Ta-1.
Published: 01 December 1970
... WC Ta-10W is a tantalum-base alloy having a combination of low-temperature ductility and fabricability in both the recrystalilzed and wrought conditions, as well as excellent weld ductility. Developed originally for structural applications at elevated temperatures, it is now available...
Journal Articles
Alloy Digest (1983) 32 (5): SA-390.
Published: 01 May 1983
... LESCALLOY 4335+V VAC-ARC is a low-alloy steel with high hardenability and good strength and toughness. It is produced by the vacuum consumable electrode melting process to provide optimum cleanliness and preferred ingot structure. Its uses include aircraft and aerospace components, gears, shafting...
Journal Articles
Alloy Digest (1997) 46 (6): Co-103.
Published: 01 June 1997
... Conicro 5010W has a face-centered cubic structure and is a cobalt-base alloy containing chromium, tungsten, and nickel. The alloy is used in aerospace applications and in the heat-treatment industry. This datasheet provides information on composition, physical properties, and elasticity. It also...
Journal Articles
Alloy Digest (1988) 37 (7): Al-282.
Published: 01 July 1988
... Alcoa Aluminum Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy. It is available in five tempers. It is crossing many market areas of applications in aerospace, defense, automotive and general structural use. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (2017) 66 (3): Al-455.
Published: 01 March 2017
... is 19.0 38.1 mm (0.75 1.5 in Applications: Alloy 2624 plate was developed to replace alloy 2024 and 2324 in applications requiring moderate or high strength and the highest levels of damage tolerance, such as lower wing panels and other tension-dominated aerospace structures. The machining and fabrication...