Alloy Digest (1979) 28 (6): Cu-374.
Published: 01 June 1979
... AMPCO A-1 is a cast copper-base alloy well suited for use up to 750 F. It is characterized by fairly high hardness and strength, good resistance to fatigue and wear, and excellent corrosion resistance. Among its many applications are acid-resisting pumps, pickling equipment, gears, marine hardware...
Journal Articles
Alloy Digest (1983) 32 (10): Cu-464.
Published: 01 October 1983
... Copper Alloy No. C93800 is a cast copper-tin-lead alloy (bronze). It is characterized by low strength, good machinability and good resistance to corrosion. Commercial names formerly used (not recommended) are (1) Anti-Acid Metal, (2) Ingot No. 319, (3) High-Leaded Tin Bronze and (4) 78-7-15. Its...
Journal Articles
Alloy Digest (1980) 29 (12): Cu-408.
Published: 01 December 1980
... AMPCOLOY 521 is a cast copper-nickel alloy with excellent resistance to many highly active corrosives, particularly saline waters and sulfuric and phosphoric acids. It has high strength and good ductility and can be welded readily. Its many applications include valves, pump bodies, steam fittings...
Journal Articles
Alloy Digest (1996) 45 (6): Ni-19.
Published: 01 June 1996
... used in engineered equipment, such as pumps and valves, made by the alloy’s manufacturer. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-12.
Published: 01 May 1996
... CHLORIMET 2 is a nickel-base alloy that provides good resistance to corrosive conditions not normally handled by other types of commercially available alloys. CHLORIMET 2 is a refined equivalent of HASTELLOY B and is most commonly used in engineered equipment, such as pumps and valves, made...
Journal Articles
Alloy Digest (1969) 18 (5): Ni-145.
Published: 01 May 1969
... Deloro alloy C is a nickel base alloy designed primarily for high corrosion resistance for the chemical industry. It is used for pumps, valves, and hard facing electrodes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1953) 2 (10): CI-3.
Published: 01 October 1953
... Chamctdsticu CORROSIRON is a highiy comxion misting high- carbon high-silicon alloy especidy suitabie for acid andsanicarydninsItishard,brittleandmnrhimhle with d&&y. It resists abrasion and scouting. Since ttlisauoycatulotbethreaded~cations ofuslallna- chine design are required co avoid such type of con...
Journal Articles
Alloy Digest (1969) 18 (2): Ni-142.
Published: 01 February 1969
... BRUSII Alloy 200C is a beryllium-nickel casting alloy having high resistance to wear, corrosion, thermal shock and oxidation. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1973) 22 (9): SS-109.
Published: 01 September 1973
... in the production of fertilizer. The reaction takes place during constant agitation of an acid-rock slurry. Equipment used to handle the acids and slurry, such as qitator paddles and shafts, slurry pumps, filtration units. etc., are exposed to severe abrasive, erosive and corrosive attack by the mix. DOI: 10.31399...
Journal Articles
Alloy Digest (1985) 34 (4): Ni-312.
Published: 01 April 1985
... NICORROS 400 is a nickel-copper, solid-solution alloy having excellent corrosion resistance in a wide range of marine and chemical environments and good mechanical properties from sub-zero temperatures to about 900 F. Among its uses are pump parts, heat exchangers, petroleum production...
Journal Articles
Alloy Digest (1977) 26 (12): Cu-345.
Published: 01 December 1977
... Copper Alloy No. 903 is a cast copper-tin-zinc alloy known also as G Bronze or 88-8-0-4 alloy. It has a good combination of strength and corrosion resistance and is often used in castings subject to liquid or gas pressures. Among its many uses are valves, pumps, bushings and gears. This datasheet...
Journal Articles
Alloy Digest (1981) 30 (1): Cu-410.
Published: 01 January 1981
... Copper Alloy No. C96600 is a cast copper-tin-lead-zinc alloy also known as 87-10-1-2 alloy. It is characterized by a good combination of strength, machinability and resistance to corrosion. This alloy is often used to make castings for valves and pumps which are subject to liquid and gas pressure...
Journal Articles
Alloy Digest (1968) 17 (9): Ni-138.
Published: 01 September 1968
... Brush Alloy 260-C is a beryllium nickel casting alloy having high strength, hardness and good corrosion resistance. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (8): Ni-146.
Published: 01 August 1969
... ILLIUM B was developed as a bearing alloy for maximum wear and galling resistance in high concentrations of hot sulfuric acid. The alloy is capable of being age hardened. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1992) 41 (11): Fe-5.
Published: 01 November 1992
... be accurately produced. Weldability: Welding is readily accomplished by theoxyacetylene ff ame. with careful preheating and after cooling of the parts welded. The weld is as acid-resistant as the rest of the casting. Molten Duriron is quite fluid, and the torch must be handled somewhat more rapidly than...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-463.
Published: 01 September 1994
... Carlson Alloy C400 is a general purpose nickel-copper alloy having an excellent combination of high strength, ductility, weldability and corrosion resistance. It is widely used for handling sulfuric acid under reducing conditions, but also has good resistance to hydrofluoric acid, alkaline...
Journal Articles
Alloy Digest (1984) 33 (10): Ni-304.
Published: 01 October 1984
... NICLOY 400 is a nickel-copper, solid-solution alloy which is utilized in numerous applications because of its good mechanical strength and overall excellent resistance to corrosion. Among its many uses are pump parts, marine fixtures, oil production and refining equipment, heat exchangers...
Journal Articles
Alloy Digest (1978) 27 (6): Cu-355.
Published: 01 June 1978
... Copper Alloy No. 923 is a cast copper-tin-zinc-lead alloy known also as Leaded G Bronze or 87-8-1-4 alloy. This alloy possesses a good combination of strength, resistance to corrosion and machinability. It is a good alloy to withstand gas or liquid pressures. Applications include pump impellers...
Journal Articles
Alloy Digest (1982) 31 (2): Cu-432.
Published: 01 February 1982
... International bearings cast bronze castability chemical composition compressive strength Copper alloy no. C90500 corrosion-resistant alloys elasticity fatigue properties fracture toughness gears hardness heat treatability joinability machinability physical properties pumps tensile...
Journal Articles
Alloy Digest (1984) 33 (5): Cu-477.
Published: 01 May 1984
... Copper Alloy No. C92700 is a cast copper-base alloy; it formerly was known as 88-10-2-0 alloy. It is characterized by a good combination of machinability, strength and resistance to corrosion. Among its many uses are bearings, pump impellers, piston rings and valve parts that are subject to liquid...