Alloy Digest (1963) 12 (5): Ni-82.
Published: 01 May 1963
... CORRONEL 220 is a high molybdenum nickel-base alloy having high strength and high acid resistance. It is a vanadium stabilised variant of the alloy formerly known as CORRONEL B. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1966) 15 (9): SS-186.
Published: 01 September 1966
... Uranus-50T is a chromium-nickel austenitic stainless steel having high resistance to acids and freedom from intergranular corrosion. It is recommended for the chemical, food and marine industries. This datasheet provides information on composition, physical properties, microstructure, hardness...
Journal Articles
Alloy Digest (1966) 15 (5): Ni-113.
Published: 01 May 1966
... HASTELLOY Alloy G is a nickel-base alloy recommended for tough environmental applications. It resists hot sulfuric and phosphoric acid service, and is also resistant to stress-corrosion cracking. This alloy is covered by U.S. Pat. No. 2,777,766. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1966) 15 (6): SS-182.
Published: 01 June 1966
... Carpenter Stainless 20Cb-3 is an austenitic stainless steel designed for improved resistance to sulfuric acid. It finds wide use in all phases of the chemical industry. It has good mechanical properties and comparative ease of fabrication. Columbium stabilizes the alloy to minimize carbide...
Journal Articles
Alloy Digest (1952) 1 (3): Ni-1.
Published: 01 November 1952
...~ Workobilityz IUipm G is too brittle and too hard for forming. I.UumRcanbcfonned,thcpra&callimitofcoid rcductiont20pctccnt Corrosion Resistance: M ofacidcorrosion %L4 ill which both acidic and - galvironmalkucalcountued. Aisoruists &$ tanpuaturu and high temperature oxidation such as that encomtercd...
Journal Articles
Alloy Digest (1955) 4 (1): SS-24.
Published: 01 January 1955
... WORTHITE is a high nickel-chromium acid-resisting steel for the chemical and process industries. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as casting, forming, heat...
Journal Articles
Alloy Digest (1956) 5 (10): SS-48.
Published: 01 October 1956
... ALLEGHENY LUDLUM 316 and 316L are acid resistant, molybdenum type 18-8 stainless steels. Type 316L is the low carbon grade of Type 316 offering decreased carbide precipitation. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity...
Journal Articles
Alloy Digest (1957) 6 (11): SS-63.
Published: 01 November 1957
... CARPENTER STAINLESS No. 20 and No. 20-Cb are wrought low carbon austenitic alloy steels of high nickel and chromium content. They are highly resistant to hot and cold strong acids. No. 20-Cb contains columbium for carbide stabilization and retention of its corrosion resistance in the as-welded...
Journal Articles
Alloy Digest (1996) 45 (3): SS-5.
Published: 01 March 1996
... DURIMET 20 is a special austenitic stainless steel alloy of nickel, chromium, molybdenum, and copper. It is highly resistant to hot and cold strong acids and is supplied in the form of castings to the grade CN7M. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1992) 41 (10): SS-535.
Published: 01 October 1992
... CARLSON C20 PLUS alloy is an austenitic stainless steel designed for improved resistance to reducing acids, particularly sulfuric acid. It finds wide use in all phases of the chemical industry and has good strength and fabricability for case in making process equipment and piping. This datasheet...
Journal Articles
Alloy Digest (1979) 28 (6): Cu-374.
Published: 01 June 1979
... AMPCO A-1 is a cast copper-base alloy well suited for use up to 750 F. It is characterized by fairly high hardness and strength, good resistance to fatigue and wear, and excellent corrosion resistance. Among its many applications are acid-resisting pumps, pickling equipment, gears, marine hardware...
Journal Articles
Alloy Digest (1996) 45 (2): SS-636.
Published: 01 February 1996
... Sandvik 3R60 is an acid resistant austenitic stainless steel. It has a low carbon content to offer decreased carbide precipitation and increased intergranular corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1962) 11 (3): Cu-55.
Published: 01 March 1962
... NI-VEE Type D is a precipitation hardening leaded-nickel bearing bronze suitable for bearings and acid-resisting castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion and wear...
Journal Articles
Alloy Digest (1956) 5 (11): Cu-44.
Published: 01 November 1956
... NI-VEE TYPE E is a precipitation hardening leaded-nickel bearing bronze suitable for bearings and acid-resisting castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as deformation. It also...
Journal Articles
Alloy Digest (1978) 27 (5): SS-350.
Published: 01 May 1978
... UDDEHOLM Stainless 24 and 24L are essentially similar except for the extra-low carbon content of 24L for use where forming and welding result in relatively long heating within the range 930-1650 F (500-900 C). They are acid-resistant, non-hardenable and nonmagnetic steels. Their wide usage...
Journal Articles
Alloy Digest (2019) 68 (10): SS-1310.
Published: 01 October 2019
... NSSMC Advanced 347AP is an austenitic stainless steel with excellent polythionic acid resistance and good high-temperature strength. This datasheet provides information on composition as well as creep. It also includes information on high temperature performance. Filing Code: SS-1310. Producer...
Journal Articles
Alloy Digest (1973) 22 (7): SS-287.
Published: 01 July 1973
... UHB Stainless 904L is an extra-low-carbon, non-stabilized austenitic stainless steel with excellent corrosion resistance in severe acids and acidic solutions. It is particularly suitable for structural applications in the chemical industry and other process industries. This datasheet provides...
Journal Articles
Alloy Digest (1988) 37 (10): Cu-542.
Published: 01 October 1988
... CONTINUOUS-CAST ALUMINUM BRONZE has good metal-to-metal wear and abrasion resistance. It has excellent resistance to acid corrosion. Popular aluminum bronze alloys known up to a few years ago only by their trade name specifications are now covered by standard specifications (see Specification...
Journal Articles
Alloy Digest (1984) 33 (6): SS-446.
Published: 01 June 1984
... the problem of corrosion under these circumstances. NICROFER 3127 LC shows good resistance to sulfuric and nitric acids and to organic acids such as acetic and formic and rruxIures of the latter acids. Resistance is shown to hydrochloric. hydrofluoric and hydrofluorosiliclc acids and the alloy may be used...
Journal Articles
Alloy Digest (1955) 4 (4): Fe-7.
Published: 01 April 1955
... DURICHLOR is a high silicon iron for corrosive services, especially in the handling of hydrochloric acid in all concentrations. It is also very resistant to moist chlorine gas and many destructive chloride-containing solutions. This datasheet provides information on composition, physical...