Alloy Digest (1962) 11 (11): Zn-9.
Published: 01 November 1962
... Zilloy 20 is a wrought zinc-base alloy having good stability and creep resistance. It is recommended for architectural applications, and for formed articles requiring maximum creep resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1959) 8 (1): Zn-6.
Published: 01 January 1959
... Zilloy 15 is a zinc-base alloy strip recommended for drawn or mildly formed parts requiring maximum stiffness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion...
Journal Articles
Alloy Digest (1957) 6 (12): Zn-5.
Published: 01 December 1957
... ZILLOY 40 is a sheet and strip zinc-base alloy recommended for drawn or mildly formed parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well...