Alloy Digest (2020) 69 (8): SS-1326.
Published: 01 August 2020
... Zapp Ergste 1.4028YN is a medium-carbon, 13% Cr, martensitic stainless steel that is designed for medical applications requiring high strength and hardness along with good corrosion resistance in moderately corrosive environments. This datasheet provides information on composition, physical...