Alloy Digest (1982) 31 (7): Zr-8.
Published: 01 July 1982
... ZIRCADYNE 705 is a zirconium-niobium (columbium) alloy which contains 2-3% niobium. Because of its excellent resistance to many corrosive media and its good mechanical and heat transfer properties, Zircadyne 705 has found widespread use in many chemical process applications. This datasheet...
Journal Articles
Alloy Digest (1983) 32 (5): Zr-10.
Published: 01 May 1983
... ZIRCADYNE 706 is a zirconium-niobium (columbium) alloy containing 2-3% niobium. It is similar in chemical compositions (except for slightly lower oxygen) to Zircadyne 705 (Alloy Digest Zr-8, July 1982). Zircadyne 706 was developed specifically for severe forming applications such as panel-type...
Journal Articles
Alloy Digest (1982) 31 (12): Zr-9.
Published: 01 December 1982
...- ature, high-pressure water and steam. The tensile strength of Zir- cadyne 704 is intermediate between Zircadynes 702 and 705. Forms Available: Ingot. biiet, sheet. strip, plate, bar, rod, wire, tube and pipe. Applications: Applications involving high-temperature, high-pressure water and steam, chemical...