Alloy Digest (1982) 31 (12): Zr-9.
Published: 01 December 1982
... ZIRCADYNE 704 is a zirconium-tin-iron-chromium alloy. Zircadyne 704 can contain up to 4.5% hafnium which is naturally present in the zirconium ore. The hafnium is very similar to zirconium metallurgically and chemically and is not detrimental to the corrosion resistance of Zircadyne 704...