Alloy Digest (1987) 36 (1): Cu-520.
Published: 01 January 1987
... ZHC COPPER is a high-electrical-conductivity alloy developed to satisfy the requirements of high-power electronic circuits. It has high strength compared to other metals of equivalent conductivity, good bend formability, excellent stress-relaxation resistance and is readily soldered. It also is...
Journal Articles
Alloy Digest (1994) 43 (10): Cu-552.
Published: 01 October 1994
... softening and stress-relax- ation resistance. Specification Equivalents: UNS Cl5100 ZHC Copper ASTM B747 Forms Available: Bar, Foil, Plate, Sheet and Strip Exposure time, s Figure 2 -Softening resistance of lead frame materials at the upper temperature limit, 930°F (500 Applications: Switches, high...
Journal Articles
Alloy Digest (1974) 23 (6): Cu-280.
Published: 01 June 1974
... COPPER Alloy No. 425 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by convectional processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Journal Articles
Alloy Digest (1988) 37 (8): Cu-539.
Published: 01 August 1988
... UNS C42500 is a copper-zinc-tin alloy suitable for electrical switches and springs, fuse and pen clips, and weather stripping. It can be cold worked readily by conventional processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1988) 37 (12): Zn-45.
Published: 01 December 1988
... added copper. It is a relatively ductile (bendable and shapable) die casting alloy. Compositton: (Weight %) Alumimtm 3.5-4.3 ~Cadrnium 0.004 max. Copper 0.25 max. Iron 0.100 max. Magnesium 0.02-0.05 0.005 max.. Tin 0.003 max. ZhC Remainder Physical Constants: Density, Ib/cu in. Specific gravity Melting...
Journal Articles
Alloy Digest (1957) 6 (3): Cu-48.
Published: 01 March 1957
... SCOBRONZE, also known as Scovill No. 381 Alloy, is a copper-zinc alloy containing tin for increased strength and fatigue characteristics and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1988) 37 (12): Al-293.
Published: 01 December 1988
... Copper 3.040 specific gravity 2.71 ZhC 3.0 max. Melting range, F (Approximate) 1000-1100 2.0 max. Specific heat, Btu/lb/ F (At 212°F) 0.230 Mw!m= 0.50 max. Thermal coef. expansion/OF (68-212OF) 10.7 x 106 Nickel 0.50 max. (as-392T) 12.2 x 1w Tin 0.35 max. Thermal conductivity, Btu/ftW/hrrPF (At 77°F...
Journal Articles
Alloy Digest (1959) 8 (9): Al-82.
Published: 01 September 1959
... recommended for applications where good high-tempera cure strength, low co fkient of thermal expansion, and good resistance to weat are required. Composition: SilkOIl copper Magnesium Nickel IrOll Maw== ZhC Titanium Other elements, total Aluminum 8.5 - 10.5 2.0 - 4.0 0.5 - 1.5 0.5 - 1.5 1.2 max. 0.5 msx. 0.5...
Journal Articles
Alloy Digest (1962) 11 (3): Al-112.
Published: 01 March 1962
... combination of mechanical proper- ties, corrosion resistance and machinability. Composition: Physical Constants: (Solution Annealed) Magnesium Copper Iron Silicon Manganese ZhC Other elements, total Aluminum 9.5-10.6 0.20 max. 0.30 max. 0.20 max. 0.10 max. 0.10 max. 0.15 max. Remainder Specific gravity...
Journal Articles
Alloy Digest (1972) 21 (7): Al-204.
Published: 01 July 1972
...-hardening heat treatment. It has good strength, weldability aud corrosion resistance.. Composition: Silicon Iron Copper Manganese Magnesium ZhC Titanium Others: Each Others: Total 8.6-9.4 0.20 max 1.6-2.0 0.10 max 0.4 O-O.6 0.10 mw 0.20 max 0.05 max 0.15 max Remainder Physical Constants: (Green sand cast...
Journal Articles
Alloy Digest (1973) 22 (6): Al-207.
Published: 01 June 1973
... the manufacture of porcelain enameled housewares. Competition: Silicon Iron Copper Manganese Magnesium Chromium ZhC Titanium Others, each others. total AlUminUlll 0.50 max. 0.50 max. 2.2-3.0 0.10-0.40 0.30-0.60 0.10 max. 0.25 max. 0.15 max. 0.05 max. 0.15 max. Remain&I Physical Constants: (Approx. 1...